Abstract Deep undercooling for Ni-base alloy, i.e., (Ni_(0.53)Fe_(0.33)Co_(0.14))_(73)B_(17)Si_8Nb_2, wasobtained by technique of auto-separating denucleation of molten glass. The solidification ofthe undercooled Ni-base alloy is observed to be in a mode of twin growth. Mechanism on theformation and growth of twins was approached by studies of composition, structure andmorphology of the alloy, together with the solidificatiion of deep undercooling alloy melt. Theundercooling, crystal lattice and composition of the alloy seem to be the most important fac-tors in the formation and growth of twins.
|
Received: 18 September 1993
|
1 Ghadwick G A. Metallography of Phase Transformations. London: Butterworths, 1972 2 Jones B. L, Rarde. In: John T, Burke J J eds., Solidification Technology, Portsmouth, New Hampshire, 1972: 407 3 Morris L R, Carruthers J R, Plumtrec A, Winegard W C. Trans Metall Soc AIME 1966; 236: 1286 4 中尾善信.轻金属,1968;18:410 5 闵乃本.第6届学部委员会论文集,1991:87 6 周根树,杨根仓,周尧和,郭振琪.材料科学进展,待发表 7 Piccone T J, Flemings M C. Metall Trans, 1987; 18: 925 8 周尧和,杨根仓.西北工业大学学报,1985;3:227 |
No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|