TWIN GROWTH IN DEEPLY UNDERCOOLED (NiFeCo)-B-Si-Nb ALLOY
ZHOU Genshu;YANG Gencang;ZHOU Yaohe Northwestern Polytechnical University; Xi'an
Cite this article: 

ZHOU Genshu;YANG Gencang;ZHOU Yaohe Northwestern Polytechnical University; Xi'an. TWIN GROWTH IN DEEPLY UNDERCOOLED (NiFeCo)-B-Si-Nb ALLOY. Acta Metall Sin, 1993, 29(9): 31-34.

Download:  PDF(807KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Deep undercooling for Ni-base alloy, i.e., (Ni_(0.53)Fe_(0.33)Co_(0.14))_(73)B_(17)Si_8Nb_2, wasobtained by technique of auto-separating denucleation of molten glass. The solidification ofthe undercooled Ni-base alloy is observed to be in a mode of twin growth. Mechanism on theformation and growth of twins was approached by studies of composition, structure andmorphology of the alloy, together with the solidificatiion of deep undercooling alloy melt. Theundercooling, crystal lattice and composition of the alloy seem to be the most important fac-tors in the formation and growth of twins.
Key words:  auto-separating denucleation      undercooling      twin growth      Ni-base alloy     
Received:  18 September 1993     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1993/V29/I9/31

1 Ghadwick G A. Metallography of Phase Transformations. London: Butterworths, 1972
2 Jones B. L, Rarde. In: John T, Burke J J eds., Solidification Technology, Portsmouth, New Hampshire, 1972: 407
3 Morris L R, Carruthers J R, Plumtrec A, Winegard W C. Trans Metall Soc AIME 1966; 236: 1286
4 中尾善信.轻金属,1968;18:410
5 闵乃本.第6届学部委员会论文集,1991:87
6 周根树,杨根仓,周尧和,郭振琪.材料科学进展,待发表
7 Piccone T J, Flemings M C. Metall Trans, 1987; 18: 925
8 周尧和,杨根仓.西北工业大学学报,1985;3:227
[1] XU Junfeng, ZHANG Baodong, Peter K Galenko. Model of Eutectic Transformation Involving Intermetallic Compound[J]. 金属学报, 2021, 57(10): 1320-1332.
[2] Kuanhui HU, Xinping MAO, Guifeng ZHOU, Jing LIU, Zhifen WANG. Effect of Si and Mn Contents on the Microstructure and Mechanical Properties of Ultra-High Strength Press Hardening Steel[J]. 金属学报, 2018, 54(8): 1105-1112.
[3] Yun LI, Lianjie LIU, Xinming LI, Jinfu LI. Solidification of Undercooled Co75B25 Alloy[J]. 金属学报, 2018, 54(8): 1165-1170.
[4] Dandan FAN, Junfeng XU, Yanan ZHONG, Zengyun JIAN. Effect of Superheated Temperature and Cooling Rate on the Solidification of Undercooled Ti Melt[J]. 金属学报, 2018, 54(6): 844-850.
[5] Zengyun JIAN, Tao XU, Junfeng XU, Man ZHU, Fang'e CHANG. Development of Solid-Liquid Interfacial Energyof Melt-Crystal[J]. 金属学报, 2018, 54(5): 766-772.
[6] Jinfu LI, Yaohe ZHOU. Remelting of Primary Solid in Rapid Solidification of Deeply Undercooled Alloy Melts[J]. 金属学报, 2018, 54(5): 627-636.
[7] Bin ZHAI, Kai ZHOU, Peng Lü, Haipeng WANG. Rapid Solidification of Ti-6Al-4V Alloy Micro-Droplets Under Free Fall Condition[J]. 金属学报, 2018, 54(5): 824-830.
[8] Jianglei ZHU, Qing WANG, Haipeng WANG. Thermophysical Properties and Atomic Distribution of Undercooled Liquid Cu[J]. 金属学报, 2017, 53(8): 1018-1024.
[9] Junhui YAN,Zengyun JIAN,Man ZHU,Fang'e CHANG,Junfeng XU. SOLIDIFICATION CHARACTERISTICS AND MICRO-STRUCTURE OF HIGH UNDERCOOLED Al-70%Si ALLOY[J]. 金属学报, 2016, 52(8): 931-937.
[10] CHEN Zheng, YANG Yanan, CHEN Qiang, XU Junfeng, TANG Yueyue, LIU Feng. RECALESCENCE EFFECT SIMULATION AND MICROSTRUCTURE EVOLUTION OF UNDERCOOLED Fe82B17Si1 ALLOY[J]. 金属学报, 2014, 50(7): 795-801.
[11] WEN Qiang, JIAN Zengyun, ZHU Man, CHANG Fang'e, DANG Bo. EFFECTS OF RE ON THE SOLIDIFICAIION CHARACTERISTICS OF Al-80%Si ALLOY[J]. 金属学报, 2014, 50(5): 610-618.
[12] GUO Xiong, LIN Xin, WANG Zhitai, CAO Yongqing, PENG Dongjian, HUANG Weidong. FORMATION MECHANISM OF ANOMALOUS EUTECTIC AND MICROSTRUCTURE EVOLUTION IN HIGHLY UNDERCOOLED SOLIDIFICATION OF Ni-30%Sn ALLOY[J]. 金属学报, 2013, 29(4): 475-482.
[13] HU Rui, LIU Yi, ZHANG Tiebang, KOU Hongchao, LI Jinshan. PHASE SELECTION AND THE SOLIDIFICATION CHARACTERISTICS OF TiAl BASE ALLOYS IN THE NONEQUILIBRIUM SOLIDIFICATION[J]. 金属学报, 2013, 49(11): 1295-1302.
[14] CHANG Fang'e ZHAO Zhiwei ZHU Man LI Na FANG Wen DONG Guangzhi JIAN Zengyun. SOLIDIFICATION BEHAVIORS OF HIGHLY UNDERCOOLED Ni-21.4%Si EUTECTIC ALLOY[J]. 金属学报, 2012, 48(7): 875-881.
[15] MU Danning YANG Changlin WEI Xiaowei LIU Feng. RESEARCH ON GRAIN REFINEMENT IN BULK UNDERCOOLED Fe–Co BASE ALLOYS[J]. 金属学报, 2012, 48(12): 1409-1414.
No Suggested Reading articles found!