| DISTRIBUTION OF Si AND B BETWEEN SLAGS AND IRON |
| ZHAI Yuchun;TIAN Yanwen;CHE Yinchang;WANG Baofian;SHAO Zhongbao(Northeasten University; Shenyang) |
|
Cite this article:
ZHAI Yuchun;TIAN Yanwen;CHE Yinchang;WANG Baofian;SHAO Zhongbao(Northeasten University; Shenyang). DISTRIBUTION OF Si AND B BETWEEN SLAGS AND IRON. Acta Metall Sin, 1994, 30(22): 435-438.
|
|
|
Abstract The distribution of Si and B between MgO-SiO_2-B_2O_3 slag and carbon-sat urated iron was determined with the method of chemical equilibrium at 1500℃.The results are as follows
|
|
|
| 1张显鹏.辽宁冶金,1992:(4):362张显鹏.辽宁冶金,1987;(5):573梁英教,车荫昌.无机物热力学数据手册.沈阳:东北大学出版社,1993 |