WETTABILITY AND CRITICAL CURRENT DENSITY OF LITHIUM SALT-CONTAINING CARBON ANODE
QIU Zliuxian;YAO Guangchun;YU Yaxin;ZHANG Zhonglin(Northeastern University; Shenyang)
Cite this article: 

QIU Zliuxian;YAO Guangchun;YU Yaxin;ZHANG Zhonglin(Northeastern University; Shenyang). WETTABILITY AND CRITICAL CURRENT DENSITY OF LITHIUM SALT-CONTAINING CARBON ANODE. Acta Metall Sin, 1994, 30(22): 439-443.

Download:  PDF(300KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The lithium salt-containing carbon anode is with better wettability and higher critical current density than the ordinary carbon anode.The occurrence of anode effect in aluminium electrolysis may be decreased by using this type of carbon anode in industrial cells.The mechanism of inhibiting anode effect is explained.
Key words:  lithium salt-containing carbon anode      wettability      critical current density     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1994/V30/I22/439

QiuZhuxian,WeiQingbin,YaoKwantsung,Aluminium,1983;9:6702HarkerH.ProceedingsoftheFourthConferenceonCarbon.England,1960:1253FrankWB,HaupinWE,DawlessRK.Ullmann'sEncyclopediaofIndustrialChemistry,1985;Al:4594PiontelliR.J ElectrochemSoc,1956;103:7055WatanebeN,ChongYB,AritsukaM,ProceedingsoftheFourthJapan-ChinaBilateralConferenceonMoltenSalts,Japan,1992:1116TojoT,HiraiwaJ,WatanabeN.ProceedingsofthefouthJapan-ChinaBilateralConferenceonMoltenSalts,Japan,1992:1157LiuYexiang,XiaoHM,ChenXG.LightMetals,1991:48
[1] Yantao YAO, Liqing CHEN, Wenguang WANG. Damping Capacities of (B4C+Ti) Hybrid Reinforced Mg and AZ91D Composites Processed by In Situ Reactive Infiltration Technique[J]. 金属学报, 2019, 55(1): 141-148.
[2] Lei SUN,Minghe CHEN,Liang ZHANG,Fan YANG. Microstructures Evolution and Properties of Sn-Ag-Cu Solder Joints[J]. 金属学报, 2017, 53(5): 615-621.
[3] Xiaoyan CHEN,Zhe JIN,Xuefeng BAI,Yizhou ZHOU,Tao JIN,Xiaofeng SUN. EFFECT OF C ON THE INTERFACIAL REACTION AND WETTABILITY BETWEEN A Ni-BASED SUPERALLOY AND CERAMIC MOULD[J]. 金属学报, 2015, 51(7): 853-858.
[4] CHEN Xiaoyan, ZHOU Yizhou, ZHANG Chaowei, JIN Tao, SUN Xiaofeng. EFFECT OF Hf ON THE INTERFACIAL REACTION BETWEEN A NICKEL BASE SUPERALLOY AND A CERAMIC MATERIAL[J]. 金属学报, 2014, 50(8): 1019-1024.
[5] MA Guofeng, HE Chunlin, LI Zhengkun, ZHANG Bo, LI Hong, ZHANG Haifeng, HU Zhuangqi. EFFECTS OF THE ADDITION OF Ti OR Al ON THE WETTING BEHAVIORS AND INTERFACIALCHARACTERISTICS OF Zr50Cu50 BULK METALLIC GLASS/W SUBSTRATE[J]. 金属学报, 2013, 29(4): 495-500.
[6] ZHOU Jian; SUN Yangshan; XUE Feng. Microstructures and Properties of Sn-Zn-Bi Solder Alloys[J]. 金属学报, 2005, 41(7): 743-749 .
[7] WU Yichu;CHANG Xiangrong;TIAN Zhongzhuo;XIAO Jimei University of Science and Technology Beijing. HYDROGEN DAMAGE IN HIGH PURITY IRON[J]. 金属学报, 1992, 28(2): 43-46.
[8] LIU Yaohui;YU Sirong;HE Zhenming Jilin University of Technology; Changchun; LI Qingchun Harbin Institute of Technology. EFFECT OF Ce ON WETTABILITY AT INTERFACEBETWEEN Al_2O_3/MEDIUM MANGANESE STEEL[J]. 金属学报, 1991, 27(1): 126-129.
[9] ZHANG Oiyun;HAN Wanshu;LIU Junkang Peking University; Beijing ZHANG Qiyun; professor; Department of Chemistry; Peking University 100871. INTERACTION BETWEEN Cu AND LIQUID Sn——Also on Physical Meaning of Wetting Curve[J]. 金属学报, 1989, 25(6): 85-90.
No Suggested Reading articles found!