CAI Xun; ZHOU Pingnan; (Shanghai Jiaotong University ; Shanghai 200030)Bangert H (Technical University of Vienna; Auslria)(Manuscript received 94-07-18)
Cite this article:
CAI Xun; ZHOU Pingnan; (Shanghai Jiaotong University ; Shanghai 200030)Bangert H (Technical University of Vienna; Auslria)(Manuscript received 94-07-18). SIMULATION OF INDENTATION MICROHARDNESS TESTING. Acta Metall Sin, 1995, 31(13): 44-5.
Abstract In order to explain many of the phenomena observed in microindentation test.for example, the substrate effect on the microhardness measurements of coating-substrate systems, the determining of the critical load and the apparent microhardness increase with decreasing load etc, the finite element method is applied to simulate the microindentation process on bulk materials and coating-substrate systems. Correspondent. CAI Xun. professor. Department of Materials Science, Shanghai Jiaotong University,Shanghai, 200030