Please wait a minute...
Acta Metall Sin  1995, Vol. 31 Issue (18): 266-268    DOI:
Current Issue | Archive | Adv Search |
INFLUENCE OF DENUCLEATION ON THERMAL STABILITY OF AMORPHOUS ALLOY
ZHOU Genshu(Xi'an Jiaotong University; Hi'an 710049); YANG Gencang; ZHOUYaohe(Northwestern Polytechnical University; Hi'an 710072)
Cite this article: 

ZHOU Genshu(Xi'an Jiaotong University; Hi'an 710049); YANG Gencang; ZHOUYaohe(Northwestern Polytechnical University; Hi'an 710072). INFLUENCE OF DENUCLEATION ON THERMAL STABILITY OF AMORPHOUS ALLOY. Acta Metall Sin, 1995, 31(18): 266-268.

Download:  PDF(207KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  DSC result indicated that the thermal stability of amorphous (Ni0.53,Fe0.33,Co0.14)73B17Si8Nb2 alloy could be increased further with the pre-denucleation of the melts. Denucleation enables the thicker amorphous stripes to possess higher degree of thermal stability. The rapidly quenching of the denucleated melts is effective for preparing bulk amorphous alloy and improving its property of application.
Key words:  denucleation      thermal stability      amorphous alloy     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1995/V31/I18/266

1王一禾,杨膺善,非晶态合金,北京:冶金工业出版社,1989:1102LuborskyFE.MaterSciEng,1987;28:1393周根树,马宝钢,金志浩,杨根仓,周尧和.94'秋季中国材料研讨会论文集,19944GaptaA,JayarajME.JNon-CrystSolids,1992;149:2755周根树,杨根仓,周尧和.材料科学进展,1993;7:156InoueA,YamamotoH.MasumotoT.MaterTransJIM,1989:30:6777KissingerHE,AnalChem,1957;29:17208LuborskyFE著.杨成,施与湛,罗阳,何开元译.非晶态金属合金.北京:冶金工业出版社,1989:192
[1] YUAN Jianghuai, WANG Zhenyu, MA Guanshui, ZHOU Guangxue, CHENG Xiaoying, WANG Aiying. Effect of Phase-Structure Evolution on Mechanical Properties of Cr2AlC Coating[J]. 金属学报, 2023, 59(7): 961-968.
[2] FENG Aihan, CHEN Qiang, WANG Jian, WANG Hao, QU Shoujiang, CHEN Daolun. Thermal Stability of Microstructures in Low-Density Ti2AlNb-Based Alloy Hot Rolled Plate[J]. 金属学报, 2023, 59(6): 777-786.
[3] LIU Shuaishuai, HOU Chaonan, WANG Engang, JIA Peng. Plastic Rheological Behaviors of Zr61Cu25Al12Ti2 and Zr52.5Cu17.9Ni14.6Al10Ti5 Amorphous Alloys in the Supercooled Liquid Region[J]. 金属学报, 2022, 58(6): 807-815.
[4] LI Jinfu, LI Wei. Structure and Glass-Forming Ability of Al-Based Amorphous Alloys[J]. 金属学报, 2022, 58(4): 457-472.
[5] ZHANG Jinyong, ZHAO Congcong, WU Yijin, CHEN Changjiu, CHEN Zheng, SHEN Baolong. Structural Characteristic and Crystallization Behavior of the (Fe0.33Co0.33Ni0.33)84 -x Cr8Mn8B x High-Entropy-Amorphous Alloy Ribbons[J]. 金属学报, 2022, 58(2): 215-224.
[6] NIE Jinfeng, WU Yuli, XIE Kewei, LIU Xiangfa. Microstructure and Thermal Stability of Heterostructured Al-AlN Nanocomposite[J]. 金属学报, 2022, 58(11): 1497-1508.
[7] HAN Luhui, KE Haibo, ZHANG Pei, SANG Ge, HUANG Huogen. Kinetic Crystallization Behavior of Amorphous U60Fe27.5Al12.5 Alloy[J]. 金属学报, 2022, 58(10): 1316-1324.
[8] LIU Riping, MA Mingzhen, ZHANG Xinyu. New Development of Research on Casting of Bulk Amorphous Alloys[J]. 金属学报, 2021, 57(4): 515-528.
[9] HU Xiang, GE Jiacheng, LIU Sinan, FU Shu, WU Zhenduo, FENG Tao, LIU Dong, WANG Xunli, LAN Si. Combustion Mechanism of Fe-Nb-B-Y Amorphous Alloys with an Anomalous Exothermic Phenomenon[J]. 金属学报, 2021, 57(4): 542-552.
[10] WANG Yihan, YUAN Yuan, YU Jiabin, WU Honghui, WU Yuan, JIANG Suihe, LIU Xiongjun, WANG Hui, LU Zhaoping. Design for Thermal Stability of Nanocrystalline Alloys Based on High-Entropy Effects[J]. 金属学报, 2021, 57(4): 403-412.
[11] WANG Xiaobo, WANG Yongzhe, CHENG Xudong, JIANG Rong. Thermal Stability of AlCrON-Based Solar Selective Absorbing Coating in Air[J]. 金属学报, 2021, 57(3): 327-339.
[12] ZHU Min, OUYANG Liuzhang. Kinetics Tuning and Electrochemical Performance of Mg-Based Hydrogen Storage Alloys[J]. 金属学报, 2021, 57(11): 1416-1428.
[13] PENG Yanyan, YU Liming, LIU Yongchang, MA Zongqing, LIU Chenxi, LI Chong, LI Huijun. Effect of Ageing Treatment at 650 ℃ on Microstructure and Properties of 9Cr-ODS Steel[J]. 金属学报, 2020, 56(8): 1075-1083.
[14] HUANG Huogen, ZHANG Pengguo, ZHANG Pei, WANG Qinguo. Comparison of Glass Forming Ability Between U-Co and U-Fe Base Systems[J]. 金属学报, 2020, 56(6): 849-854.
[15] GENG Yaoxiang, WANG Yingmin. Local Structure-Property Correlation of Fe-Based Amorphous Alloys: Based on Minor Alloying Research[J]. 金属学报, 2020, 56(11): 1558-1568.
No Suggested Reading articles found!