| LATTICE EXPANSION IN NANOCRYSTALLINE PURE Ni |
| LU Ke; LIU Xuedong;ZHANG Haoyue; HU Zhuangqi(State Key Laboratory forRSA; Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110015)(Manuscript received 94-05-10) |
|
Cite this article:
LU Ke; LIU Xuedong;ZHANG Haoyue; HU Zhuangqi(State Key Laboratory forRSA; Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110015)(Manuscript received 94-05-10). LATTICE EXPANSION IN NANOCRYSTALLINE PURE Ni. Acta Metall Sin, 1995, 31(2): 74-78.
|
|
|
Abstract The lattice structure of nanocrystalline pure Ni. prepared by high-frequency sputtering, has been investigated. The lattice parameter of nanocrystalline Ni samples with grain sizes ranging from 6 to 15 nm was measured accurately by X-ray diffraction. It was found that the lattice parameter(a) for the nanocrystallie samples is larger than that for the perfect Ni single crystal(ao), and the value of a increases significantly with the decrease of grain size. According to the thermodynamic theory, the lattice expansion in the nanocrystalline sample was explained.Corespondent:LU Ke,professor,Institute of Metal Research. Chinese Academy of Sciences, Shenyang 110015
|
|
Received: 18 February 1995
|
| 1GleiterH.ProgMaterSci,1989;33:2232LuK.SuiML,JMaterSciTechnol,1993:9:4193LuK,SuiML,LuckR,NanostrMater,1994;4:4654SuiML,LuK,MaterSciEng,1994;A179//A180:5415 LiuXD,LuK,DingBZ,HuZQ.Nanostr Mater,1993;2:5816ShewmonPG.TransformationinMetals.NewYork:McGraw-Hill.1969:30047MutscheleT,KirchheimR.SerMetall,1987;21:1358LuK,LuckR,PredelB.SerMetallMater,1993:28:13879TerwilligerCD,ChiangYM.MaterResSolSympProc,1993;289:15 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|