Please wait a minute...
Acta Metall Sin  1995, Vol. 31 Issue (22): 473-476    DOI:
Current Issue | Archive | Adv Search |
SYNTHESIS OF NANOMETER SILICON CARBIDE WHISKERS BY MICROWAVE HEATING
DAI Changhong; (Department of Non-ferrous Metallurgy; Northeastern University; Shenyang 110006) ZHANG Jinsong; YANG Yongjin; CAO Lihua; ZHANGXianpeng; XIA Fei (Northeastern University; Shenyang 110006) (Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110015)
Cite this article: 

DAI Changhong; (Department of Non-ferrous Metallurgy; Northeastern University; Shenyang 110006) ZHANG Jinsong; YANG Yongjin; CAO Lihua; ZHANGXianpeng; XIA Fei (Northeastern University; Shenyang 110006) (Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110015). SYNTHESIS OF NANOMETER SILICON CARBIDE WHISKERS BY MICROWAVE HEATING. Acta Metall Sin, 1995, 31(22): 473-476.

Download:  PDF(310KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  A method for synthesizing silicon carbide whiskers by microwave heating is described in this paper. Silicon carbide whiskers with diameter in the range of nanometer have been obtaind by the reduction of SiO2 with C in an atmosphere of nitrogen. Ultrafine SiO2 powder, phenol formaldehyde resin and carbon black are used as starting materials. The structures of the whiskers are determined by means of XRD, TEM. The effects of temperature and carbon type on the production of SiC whiskers are discussed.
Key words:  SiC      whisker      microwave heating     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1995/V31/I22/473

1NuttSR.JAmCeramSoc,1988;71:1492MilewskiJV,GacFD,PetrovicJJ,SkaggsSR.JMaterSci,1985;20:11603张劲松,曹丽华,杨永进,沈学逊,沈志翔,夏非.材料导报,1994;2:344宋慎泰,柳光祖,硅酸盐学报,1993;21:15ChrysanthouA,GrievesonP,JhaA.JMaterSci,1991;26:34636JhaA.JMaterSci,1993;28:3069
[1] ZHOU Xiaobin, ZHAO Zhanshan, WANG Wanxing, XU Jianguo, YUE Qiang. Physical and Mathematical Simulation on the Bubble Entrainment Behavior at Slag-Metal Interface[J]. 金属学报, 2023, 59(11): 1523-1532.
[2] SHEN Yingying, ZHANG Guoxing, JIA Qing, WANG Yumin, CUI Yuyou, YANG Rui. Interfacial Reaction and Thermal Stability of the SiCf/TiAl Composites[J]. 金属学报, 2022, 58(9): 1150-1158.
[3] FENG Di, ZHU Tian, ZANG Qianhao, LEE Yunsoo, FAN Xi, ZHANG Hao. Solution Behavior of Spray-Formed Hypereutectic AlSiCuMg Alloy[J]. 金属学报, 2022, 58(9): 1129-1140.
[4] GU Ruicheng, ZHANG Jian, ZHANG Mingyang, LIU Yanyan, WANG Shaogang, JIAO Da, LIU Zengqian, ZHANG Zhefeng. Fabrication of Mg-Based Composites Reinforced by SiC Whisker Scaffolds with Three-Dimensional Interpenetrating-Phase Architecture and Their Mechanical Properties[J]. 金属学报, 2022, 58(7): 857-867.
[5] WU Caihong, FENG Di, ZANG Qianhao, FAN Shichun, ZHANG Hao, LEE Yunsoo. Microstructure Evolution and Recrystallization Behavior During Hot Deformation of Spray Formed AlSiCuMg Alloy[J]. 金属学报, 2022, 58(7): 932-942.
[6] TIAN Zhihua, ZHANG Peigen, LIU Yushuang, LU Chengjie, DING Jianxiang, SUN Zhengming. Research Progress and Outlook of Metal Whisker Spontaneous Growth on MAX Phase Substrates[J]. 金属学报, 2022, 58(3): 295-310.
[7] WANG Di, HUANG Jinhui, TAN Chaolin, YANG Yongqiang. Review on Effects of Cyclic Thermal Input on Microstructure and Property of Materials in Laser Additive Manufacturing[J]. 金属学报, 2022, 58(10): 1221-1235.
[8] PI Huilong, SHI Xiaolei, XU Xingxiang. Effect of SiC-ZrC Coating Prepared by SiZr Liquid Phase Sintering on the Oxidation Resistance of C/SiC Composites[J]. 金属学报, 2021, 57(6): 791-796.
[9] WU Yucheng, GAO Zhiqiang, XU Guangqing, LIU Jiaqin, XUAN Haicheng, LIU Youhao, YI Xiaofei, CHEN Jingwu, HAN Peide. Current Status and Challenges in Corrosion and Protection Strategies for Sintered NdFeB Magnets[J]. 金属学报, 2021, 57(2): 171-181.
[10] WANG Chao, ZHANG Xu, WANG Yumin, YANG Qing, YANG Lina, ZHANG Guoxing, WU Ying, KONG Xu, YANG Rui. Mechanisms of Interfacial Reaction and Matrix Phase Transition in SiCf /Ti65 Composites[J]. 金属学报, 2020, 56(9): 1275-1285.
[11] WU Yupeng, ZHANG Bo, LI Jingming, ZHANG Shuangnan, WU Ying, WANG Yumin, CAI Guixi. Ultrasonic Detection for Fiber Broken in Aero-Engine Integral Bladed Ring[J]. 金属学报, 2020, 56(8): 1175-1184.
[12] CHEN Yongjun, BAI Yan, DONG Chuang, XIE Zhiwen, YAN Feng, WU Di. Passivation Behavior on the Surface of Stainless Steel Reinforced by Quasicrystal-Abrasive via Finite Element Simulation[J]. 金属学报, 2020, 56(6): 909-918.
[13] WANG Bo,SHEN Shiyi,RUAN Yanwei,CHENG Shuyong,PENG Wangjun,ZHANG Jieyu. Simulation of Gas-Liquid Two-Phase Flow in Metallurgical Process[J]. 金属学报, 2020, 56(4): 619-632.
[14] Yucheng WU. The Routes and Mechanism of Plasma Facing Tungsten Materials to Improve Ductility[J]. 金属学报, 2019, 55(2): 171-180.
[15] Jianqiang REN, Shuhua LIANG, Yihui JIANG, Xiang DU. Research on the Microstructure and Properties of In Situ (TiB2-TiB)/Cu Composites[J]. 金属学报, 2019, 55(1): 126-132.
No Suggested Reading articles found!