| SYNTHESIS OF NANOMETER SILICON CARBIDE WHISKERS BY MICROWAVE HEATING |
| DAI Changhong; (Department of Non-ferrous Metallurgy; Northeastern University; Shenyang 110006) ZHANG Jinsong; YANG Yongjin; CAO Lihua; ZHANGXianpeng; XIA Fei (Northeastern University; Shenyang 110006) (Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110015) |
|
Cite this article:
DAI Changhong; (Department of Non-ferrous Metallurgy; Northeastern University; Shenyang 110006) ZHANG Jinsong; YANG Yongjin; CAO Lihua; ZHANGXianpeng; XIA Fei (Northeastern University; Shenyang 110006) (Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110015). SYNTHESIS OF NANOMETER SILICON CARBIDE WHISKERS BY MICROWAVE HEATING. Acta Metall Sin, 1995, 31(22): 473-476.
|
|
|
Abstract A method for synthesizing silicon carbide whiskers by microwave heating is described in this paper. Silicon carbide whiskers with diameter in the range of nanometer have been obtaind by the reduction of SiO2 with C in an atmosphere of nitrogen. Ultrafine SiO2 powder, phenol formaldehyde resin and carbon black are used as starting materials. The structures of the whiskers are determined by means of XRD, TEM. The effects of temperature and carbon type on the production of SiC whiskers are discussed.
|
|
|
| 1NuttSR.JAmCeramSoc,1988;71:1492MilewskiJV,GacFD,PetrovicJJ,SkaggsSR.JMaterSci,1985;20:11603张劲松,曹丽华,杨永进,沈学逊,沈志翔,夏非.材料导报,1994;2:344宋慎泰,柳光祖,硅酸盐学报,1993;21:15ChrysanthouA,GrievesonP,JhaA.JMaterSci,1991;26:34636JhaA.JMaterSci,1993;28:3069 |
| No Suggested Reading articles found! |
|
|