Solution Behavior of Spray-Formed Hypereutectic AlSiCuMg Alloy
FENG Di1(), ZHU Tian1, ZANG Qianhao1, LEE Yunsoo2,3, FAN Xi4, ZHANG Hao4
1.School of Materials Science and Engineering, Jiangsu University of Science and Technology, Zhenjiang 212003, China 2.Metallic Materials Division, Korea Institute of Materials Science, Changwon 51508, Korea 3.Department of Materials Science and Engineering, Inha University, Incheon 22212, Korea 4.Jiangsu Haoran Spray Forming Alloy Co., Ltd., Zhenjiang 212009, China
Cite this article:
FENG Di, ZHU Tian, ZANG Qianhao, LEE Yunsoo, FAN Xi, ZHANG Hao. Solution Behavior of Spray-Formed Hypereutectic AlSiCuMg Alloy. Acta Metall Sin, 2022, 58(9): 1129-1140.
Al-Si multicomponent alloys are commonly used in automotive and aerospace fields owing to their excellent castability, good wear resistance, and low coefficient of thermal expansion. After adding Cu and Mg followed by appropriate heating, Al2Cu, AlCuSiMg, or Mg2Si phases precipitate in an α-Al matrix. Hypereutectic AlSiCuMg alloys have been used in wear-resistant products, such as engine cylinders, pistons, and air-conditioning rotors, owing to the hardening effect of Si particles and the solid solution strengthening and precipitation strengthening effects of Cu and Mg. The evolution behaviors of secondary phases and the grains of the spray-formed Al25Si4Cu1Mg (mass fraction, %) alloy were examined via OM, XRD, SEM + EBSD, TEM, hardness tests, and phase diagram calculations. The results showed that the hot extrusion microstructure of spray-formed hypereutectic AlSi alloys comprises equiaxed α-Al, proeutectic Si, eutectic Si, eutectic AlCuSiMg, a eutectic Al2Cu phase, and a low volume fraction Fe-bearing phase at the micron level but without a lamellar morphology. α-Al contained both micro-nano and nano-sized Al2Cu phases precipitates. Over the temperature range of 475-495oC, the precipitated Al2Cu phase and some of the eutectic Al2Cu phase redissolved, and the residual Al2Cu phase concentrated to a Fe-bearing phase and coarsened. The volume fraction and size of the AlCuSiMg phase increased. However, when solution-treated at less than 515oC, the volume fraction of the AlCuSiMg phase began to decrease, and no overburning structure was observed. When the solution temperature exceeded 515oC, the incipient melting of the nonequilibrium eutectic phase increased with increasing solution temperature. The main characteristics of the overburning structure were the network eutectic and grain boundary broadening. The hardness of the spray-formed Al25Si4Cu1Mg alloy was dependent on five factors: the solid solubility of solute atoms, the volume fraction of the residual second phase, the grain size of α-Al, the scale of the Si phase, and the incipient melting of the nonequilibrium eutectic phase.
Fund: National Natural Science Foundation of China(51801082);Undergraduate Innovation and Entrepreneurship Training Program of Jiangsu Province(202010289019Z)
About author: FENG Di, associate professor, Tel: (0511)84401188, E-mail: difeng1984@just.edu.cn
Fig.1 DSC curves of spray-formed Al25Si4Cu1Mg alloy after hot extrusion (a) and partial enlarged drawing of Fig.1a (b)
Fig.2 XRD spectra of Al25Si4Cu1Mg alloy
Fig.3 SEM images of spray-formed Al25Si4Cu1Mg alloy (a-c) as-sprayed (Fig.3c is the detail of the box in Fig.3b) (d-f) as-extruded
Fig.4 OM images of microstructures of spray-formed Al25Si4Cu1Mg alloy treated by different solution temperatures (solution time is 2 h) (a) 475oC (b) 495oC (c) 515oC (d) 535oC (e) 555oC
Fig.5 SEM images of microstructures of spray-formed Al25Si4Cu1Mg alloy treated by different solution temperatures (solution time is 2 h) (a) 495oC (b) 515oC (c, e) 535oC (d, f) 555oC
Fig.6 The hardness comparison between different solution treatments (a) hardness of different solution temperatures (solution time is 2 h) (b) hardness of different solution time (solution temperature is 515℃)
Fig.7 Local misoritations (a, c, e) and secondary electron images (b, d, f) of microstructures under different solution temperatures (The grain boundary colored by black indicate the misorientation larger than 15°. The grain boundary colored by red indicate the misorientation is in the range of 2°~15°. Solution time is 2 h) (a, b) 475oC (c, d) 515oC (e, f) 535oC
Fig.8 The vertical section of Al25Si4Cu1Mg phase diagram based on FactSage software (Normal to the cross sectional surface)
1
Vandersluis E, Ravindran C. Effects of solution heat treatment time on the as-quenched microstructure, hardness and electrical conductivity of B319 aluminum alloy [J]. J. Alloys Compd., 2020, 838: 155577
doi: 10.1016/j.jallcom.2020.155577
2
Sadeghi I, Wells M A, Esmaeili S. Effect of particle shape and size distribution on the dissolution behavior of Al2Cu particles during homogenization in aluminum casting alloy Al-Si-Cu-Mg [J]. J. Mater. Process. Technol., 2018, 251: 232
doi: 10.1016/j.jmatprotec.2017.08.042
3
Vieira A C, Pinto A M, Rocha L A, et al. Effect of Al2Cu precipitates size and mass transport on the polarisation behaviour of age-hardened Al-Si-Cu-Mg alloys in 0.05 M NaCl [J]. Electrochim. Acta, 2011, 56: 3821
doi: 10.1016/j.electacta.2011.02.044
4
Wang Y J, Liao H C, Wu Y N, et al. Effect of Si content on microstructure and mechanical properties of Al-Si-Mg alloys [J]. Mater. Des., 2014, 53: 634
doi: 10.1016/j.matdes.2013.07.067
5
Wu Y N, Liao H C, Zhou K X. Effect of minor addition of vanadium on mechanical properties and microstructures of as-extruded near eutectic Al-Si-Mg alloy [J]. Mater. Sci. Eng., 2014, A602: 41
6
Liao H C, Wu Y N, Ding K. Hardening response and precipitation behavior of Al-7%Si-0.3%Mg alloy in a pre-aging process [J]. Mater. Sci. Eng., 2013, A560: 811
7
Giovanni M T D, Mørtsell E A, Saito T, et al. Influence of Cu addition on the heat treatment response of A356 foundry alloy [J]. Mater. Today Commun., 2019, 19: 342
doi: 10.1016/j.mtcomm.2019.02.013
8
Hwang J Y, Banerjee R, Doty H W, et al. The effect of Mg on the structure and properties of Type 319 aluminum casting alloys [J]. Acta Mater., 2009, 57: 1308
doi: 10.1016/j.actamat.2008.11.021
9
Han Y, Samuel A M, Doty H W, et al. Optimizing the tensile properties of Al-Si-Cu-Mg 319-type alloys: Role of solution heat treatment [J]. Mater. Des., 2014, 58: 426
doi: 10.1016/j.matdes.2014.01.060
10
Zhang J Y, Zuo L J, Feng J, et al. Effect of thermal exposure on microstructure and mechanical properties of Al-Si-Cu-Ni-Mg alloy produced by different casting technologies [J]. Trans. Nonferrous Met. Soc. China, 2020, 30: 1717
doi: 10.1016/S1003-6326(20)65333-X
11
Lasa L, Rodriguez-Ibabe J M. Evolution of the main intermetallic phases in Al-Si-Cu-Mg casting alloys during solution treatment [J]. J. Mater. Sci., 2004, 39: 1343
doi: 10.1023/B:JMSC.0000013895.72084.c9
12
Mohamed A M A, Samuel F H, Al kahtani S. Influence of Mg and solution heat treatment on the occurrence of incipient melting in Al-Si-Cu-Mg cast alloys [J]. Mater. Sci. Eng., 2012, A543: 22
13
Lombardi A, Ravindran C, MacKay R. Optimization of the solution heat treatment process to improve mechanical properties of 319 Al alloy engine blocks using the billet casting method [J]. Mater. Sci. Eng., 2015, A633: 125
14
Toda H, Nishimura T, Uesugi K, et al. Influence of high-temperature solution treatments on mechanical properties of an Al-Si-Cu aluminum alloy [J]. Acta Mater., 2010, 58: 2014
doi: 10.1016/j.actamat.2009.11.044
15
Luna I A, Molinar H M, Román M J C, et al. Improvement of the tensile properties of an Al-Si-Cu-Mg aluminum industrial alloy by using multi stage solution heat treatments [J]. Mater. Sci. Eng., 2013, A561: 1
16
Lin G Y, Tan X, Feng D, et al. Effects of conform continuous extrusion and heat treatment on the microstructure and mechanical properties of Al-13Si-7.5Cu-1Mg alloy [J]. Int. J. Min., Met., Mater., 2019, 26: 1013
17
Zhang J Y, Zuo L J, Feng J, et al. Effect of thermal exposure on microstructure and mechanical properties of Al-Si-Cu-Ni-Mg alloy produced by different casting technologies [J]. Trans. Nonferrous Met. Soc. China, 2020, 30: 1717
doi: 10.1016/S1003-6326(20)65333-X
18
Feng D, Han Z J, Li J C, et al. Evolution behavior of primary phase during pre-heat treatment before deformation for spray formed 7055 aluminum alloy [J]. Rare Met. Mater. Eng., 2020, 49: 4253
Hu Y S, Feng D, Zhou, J D, et al. Constitutive equation and thermal processing map of spray formed AlSi25Cu4Mg wear resistant alloy [J]. Mater. Rep., 2020, 34: 10120
Zang Q H, Feng Di, Lee Y S, et al. Microstructure and mechanical properties of Al-7.9Zn-2.7Mg-2.0Cu (wt%) alloy strip fabricated by twin roll casting and hot rolling [J]. J. Alloys Compd., 2020, 847: 156481
doi: 10.1016/j.jallcom.2020.156481
21
Zhang J S, Xiong B Q, Cui H. Spray Forming Rapid Solidification Technology: Principles and Applications [M]. Beijing: Science Press, 2008: 1
Samuel A M, Gauthier J, Samuel F H. Microstructural aspects of the dissolution and melting of Al2Cu phase in Al-Si alloys during solution heat treatment [J]. Metall. Mater. Trans., 1996, 27A: 1785
23
Han Y M, Samuel A M, Samuel F H, et al. Effect of solution heat treatment type on the dissolution of copper phases in Al-Si-Cu-Mg type alloys [J]. AFS Trans., 2008, 116: 79
24
Han Y M, Samuel A M, Samuel F H, et al. Dissolution of Al2Cu phase in non-modified and Sr modified 319 type alloys [J]. Int. J. Cast Met. Res., 2008, 21: 387
doi: 10.1179/136404608X347662
25
Vandersluis E, Andilab B, Ravindran C, et al. In-situ characterization of the solution heat treatment of B319 aluminum alloy using X-ray diffraction and electron microscopy [J]. Mater. Charact., 2020, 167: 110499
doi: 10.1016/j.matchar.2020.110499
26
Wang F, Gu Y L, Duan X J, et al. The study of spray deposited hyper-eutectic Al-Si alloy [J]. Acta Metall. Sin., 1999, 35: 121
Samuel A M, Doty H W, Valtierra S, et al. Relationship between tensile and impact properties in Al-Si-Cu-Mg cast alloys and their fracture mechanisms [J]. Mater. Des., 2014, 53: 938
doi: 10.1016/j.matdes.2013.07.021
28
Feng D, Wang G Y, Chen H M, et al. Effect of grain size inhomogeneity of ingot on dynamic softening behavior and processing map of Al-8Zn-2Mg-2Cu alloy [J]. Met. Mater. Int., 2018, 24: 195
doi: 10.1007/s12540-017-7324-2
29
Feng D, Zhang X M, Liu S D, et al. Effect of grain size on hot deformation behavior of a new high strength aluminum alloy [J]. Rare Met. Mater. Eng., 2016, 45: 2104
Zang Q H, Yu H S, Lee Y S, et al. Hot deformation behavior and microstructure evolution of annealed Al-7.9Zn-2.7Mg-2.0Cu (wt%) alloy [J]. J. Alloys Compd., 2018, 763: 25
doi: 10.1016/j.jallcom.2018.05.307
31
Wu Y N, Liao H C, Yang J, et al. Effect of Si content on dynamic recrystallization of Al-Si-Mg alloys during hot extrusion [J]. J. Mater. Sci. Technol., 2014, 30: 1271
doi: 10.1016/j.jmst.2014.07.011