Acta Metall Sin  2020, Vol. 56 Issue (4): 549-557    DOI: 10.11900/0412.1961.2019.00453
Current Issue | Archive | Adv Search |
Research and Application Progress in Ultra-HighStrength Stainless Steel
LIU Zhenbao(),LIANG Jianxiong,SU Jie,WANG Xiaohui,SUN Yongqing,WANG Changjun,YANG Zhiyong
Division of Special Steels, Central Iron and Steel Research Institute, Beijing 100081, China
Cite this article: 

LIU Zhenbao,LIANG Jianxiong,SU Jie,WANG Xiaohui,SUN Yongqing,WANG Changjun,YANG Zhiyong. Research and Application Progress in Ultra-HighStrength Stainless Steel. Acta Metall Sin, 2020, 56(4): 549-557.

Download:  HTML  PDF(1599KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  

In the present work, the development and research on ultra-high strength stainless steels (UHSSS) have been systematically reviewed. Specifically, the focus was primarily placed on the precipitation hardening and austenite phase toughening mechanisms. And, the hydrogen-induced stress corrosion cracking (SCC) and hydrogen embrittlement (HE) behaviors of high-strength stainless steels were also retrospected. It is suggested that the future development of UHSSS is on the basis of computer-aided alloy designing system, strengthening via multiple high-coherency precipitates and toughening by filmy high-stability austenite phase. Besides, verification of the SCC and HE underlying mechanisms is vital to further optimizing the performance of UHSSS.

Key words:  ultra-high strength stainless steel      strengthening and toughening mechanism      hydrogen embrittlement      stress corrosion      precipitate      reverted austenite     
Received:  27 December 2019     
ZTFLH:  TG142.71  
Fund: National Key Research and Development Program of China(2016YFB0300104)

URL: 

https://www.ams.org.cn/EN/10.11900/0412.1961.2019.00453     OR     https://www.ams.org.cn/EN/Y2020/V56/I4/549

SteelCCrNiTiMoAlCuCoMnWFe
17-4PH0.0716.04.0---4.0-≤1.0-Bal.
15-5PH0.0415.04.7---3.0-≤1.0-Bal.
Custom4500.0414.98.5---1.5---Bal.
PH13-80.0312.67.9-1.71.0----Bal.
Ultrafort4010.0212.08.20.82.0--5.3--Bal.
Ultrafort4030.0211.07.70.44.4--9.0--Bal.
1RK910.0112.29.00.874.00.331.95-0.320.15Bal.
Custom4650.0211.611.01.51.0-----Bal.
USS122G0.0912.03.0-5.0--14.0-1.0Bal.
Ferrium?S530.219.04.80.021.5--13.0-1.0Bal.
Table 1  Chemical compositions of typical high strength stainless steels[13,14,15,16,17,18,19,20,21]
SteelRp0.2 / MPaRm / MPaKIC / (MPa·m1/2)AKU / JStrengthening phase
17-4PH12621365-21Cu
15-5PH12131289-79Cu
Custom45012691289-55Cu
PH13-814481551-41NiAl
Ultrafort4011565166910356Ni3Ti
Ultrafort403166916896034Ni3Ti
1RK91150017005827Cu/Ni3Ti
Custom4651703177971-Ni3Ti
USS122G1550194090-Laves/α'
Ferrium?S531551198677-M2C
Table 2  Mechanical properties of typical high strength stainless steels[13,14,15,16,17,18,19,20,21]
Fig.1  Atom probe tomography (APT) map within a selected cube (box size is 70 nm×70 nm×240 nm) of a newly developed ultra-high strength steel aged specimenColor online
[1] Zhao B, Xu G X, He F, et al. Present status and prospect of ultra high strength steel applied to aircraft landing gear [J]. J. Aeronaut. Mater., 2017, 36(6): 1
[1] 赵 博, 许广兴, 贺 飞等. 飞机起落架用超高强度钢应用现状及展望 [J]. 航空材料学报, 2017, 36(6): 1
[2] Yang Z Y, Liu Z B, Liang J X, et al. Development of maraging stainless steel [J]. Trans. Mater. Heat Treat., 2008, 29(4): 1
[2] 杨志勇, 刘振宝, 梁剑雄等. 马氏体时效不锈钢的发展 [J]. 材料热处理学报, 2008, 29(4): 1
[3] Yang K, Niu M C, Tian J L, et al. Research and development of maraging stainless steel used for new generation landing gear [J]. Acta Metall. Sin., 2018, 54: 1567
[3] 杨 柯, 牛梦超, 田家龙等. 新一代飞机起落架用马氏体时效不锈钢的研究 [J]. 金属学报, 2018, 54: 1567
[4] Wang J, Zou H, Li C, et al. The effect of microstructural evolution on hardening behavior of type 17-4PH stainless steel in long-term aging at 350 ℃ [J]. Mater. Charact., 2006, 57: 274
[5] Zhang T P, Zhan D P, Qi X W, et al. Austenite and precipitation in secondary-hardening ultra-high-strength stainless steel [J]. Mater. Charact., 2018, 144: 393
[6] Anil K V, Karthikeyan M K, Gupta R K, et al. Aging behavior in 15-5 PH precipitation hardening martensitic stainless steel [J]. Mater. Sci. Forum, 2012, 710: 483
[7] Palanisamy D, Senthil P, Senthilkumar V. The effect of aging on machinability of 15Cr-5Ni precipitation hardened stainless steel [J]. Arch. Civil Mech. Eng., 2016, 16: 53
[8] Martin J W, Kosa T, Dulmaine B A. High-strength, notch-ductile precipitation-hardening stainless steel alloy [P]. US, 5681528, 1997
[9] Martin J W, Kosa T. Ultra-high-strength precipitation-hardenable stainless steel and strip made therefrom [P]. US, 6630103, 2003
[10] Olson G B, Kuehmann C J. Materials genomics: From CALPHAD to flight [J]. Scr. Mater., 2014, 70: 25
[11] Lu S Y, Zhang T K. Stainless Steel [M]. Beijing: Atomic Energy Press, 1995: 19
[11] 陆世英, 张廷凯. 不锈钢 [M]. 北京: 原子能出版社, 1995: 19
[12] Liu Z B, Yang Z Y, Yong Q L, et al. A 1900 MPa grade ultra-high strength stainless steel [J]. Mater. Mech. Eng., 2008, 32(3): 48
[12] 刘振宝, 杨志勇, 雍歧龙等. 1900 MPa级超高强度不锈钢的研制 [J]. 机械工程材料, 2008, 32(3): 48
[13] Bajguirani H R H. The effect of ageing upon the microstructure and mechanical properties of type 15-5 PH stainless steel [J]. Mater. Sci. Eng., 2002, A338: 142
[14] Bratukhin A G. Ways to increase the reliability of welded joints of high-strength steels in a new generation of aircraft [J]. Met. Sci. Heat Treat., 1997, 39: 123
[15] Voznesenskaya N M, Kablov E N, Petrakov A F, et al. High-strength corrosion-resistant steels of the austenitic-martensitic class [J]. Met. Sci. Heat Treat., 2002, 44: 300
[16] Kostina M V, Bannykh O A, Blinov V M. Effect of plastic deformation and heat treatment on the structure and hardening of nitrogen-bearing steel 0Kh16AN4B [J]. Met. Sci. Heat Treat., 2001, 43: 259
[17] Il'ina V P. Effect of heat treatment mode on the microstructure and fracture behavior of maraging steels 03Kh11N10M2T-VD and 03Kh11N10M2T2-VD [J]. Met. Sci. Heat Treat., 2002, 44: 116
[18] Rundkvist N A, Grachev S V. Effect of alloying and of the austenizing temperature on the phase composition and properties of corrosion-resistant maraging steels [J]. Met. Sci. Heat Treat., 1989, 31: 244
[19] Bel'tyukov A A, Stepanov V P, Shein A S. Effect of carbon on the properties of corrosion-resistat maraging steels without titanium [J]. Met. Sci. Heat Treat., 1989, 31: 830
[20] Liu P, Stigenberg A H, Nilsson J O. Quasicrystalline and crystalline precipitation during isothermal tempering in a 12Cr-9Ni-4Mo maraging stainless steel [J]. Acta Metall. Mater., 1995, 43: 2881
[21] Webster D. Optimization of strength and toughness in two high-strength stainless steels [J]. Metall. Trans., 1971, 2: 1857
[22] Habibi-Bajguirani H R H. The effect of ageing upon the microstructure and mechanical properties of type 15-5 PH stainless steel [J]. Mater. Sci. Eng., 2002, A338: 142
[23] Habibi-Bajguirani H R, Jenkins M L. High-resolution electron microscopy analysis of the structure of copper precipitates in a martensitic stainless steel of type PH 15-5 [J]. Philos. Mag. Lett., 1996, 73: 155
[24] Guo Z, Sha W, Vaumousse D. Microstructural evolution in a PH13-8 stainless steel after ageing [J]. Acta Mater., 2003, 51: 101
[25] Liang J X, Liu Z B, Yang Z Y. Development and application of high strength stainless steel [J]. Aerosp. Mater. Technol., 2013, 43(3): 1
[25] 梁剑雄, 刘振宝, 杨志勇. 高强不锈钢的发展与应用技术 [J]. 宇航材料工艺, 2013, 43(3): 1
[26] Schober M, Schnitzer R, Leitner H. Precipitation evolution in a Ti-free and Ti-containing stainless maraging steel [J]. Ultramicroscopy, 2009, 109: 553
[27] Li Y C, Yan W, Cotton J D, et al. A new 1.9 GPa maraging stainless steel strengthened by multiple precipitating species [J]. Mater. Des., 2015, 82: 56
[28] Lu Q, Xu W, Van Der Zwaag S. A strain-based computational design of creep-resistant steels [J]. Acta Mater., 2014, 64: 133
[29] Xu W, Rivera-Díaz-del-Castillo P E J, Yan W, et al. A new ultrahigh-strength stainless steel strengthened by various coexisting nanoprecipitates [J]. Acta Mater., 2010, 58: 4067
[30] Lu Q, Xu W, Van Der Zwaag S. The design of a compositionally robust martensitic creep-resistant steel with an optimized combination of precipitation hardening and solid-solution strengthening for high-temperature use [J]. Acta Mater., 2014, 77: 310
[31] P?rn J, Rarey M. Incorporating QSPR in the enumeration of fragment space [J]. Chem. Cent. J., 2009, 3: 18
[32] Matsuda S, Okamura Y. Reverse transformation of low-carbon low alloy steels [J]. Tetsu Hagané, 1974, 60: 226
[32] 松田 昭一, 岡村 義弘. 低炭素低合金鋼の逆変態 [J]. 鐵と鋼, 1974, 60: 226
[33] Watanabe S, Ohtani H, Kunitake T. The influence of hot rolling and heat treatments on the distribution of boron in steel [J]. Tetsu-Hagané, 1976, 62: 1842
[33] 渡辺 征一, 大谷 泰夫, 邦武 立郎. 鋼中Bの分布状態におよぼす熱間圧延および熱処理の影響 [J]. 鉄と鋼, 1976, 62: 1842
[34] Song Y, Li X, Rong L, et al. The influence of tempering temperature on the reversed austenite formation and tensile properties in Fe-13%Cr-4%Ni-Mo low carbon martensite stainless steels [J]. Mater. Sci. Eng., 2011, A528: 4075
[35] Nakada N, Tsuchiyama T, Takaki S, et al. Variant selection of reversed austenite in lath martensite [J]. ISIJ Int., 2007, 47: 1527
[36] Schnitzer R, Radis R, N?hrer M, et al. Reverted austenite in PH13-8Mo maraging steels [J]. Mater. Chem. Phys., 2010, 122: 138
[37] Liu Z B, Yang Z Y, Liang J X, et al. Growth behavior and precipitation of reverted austenite in ultra-high strength marageing stainless steel [J]. Heat Treat. Met., 2010, 35(2): 11
[37] 刘振宝, 杨志勇, 梁剑雄等. 超高强度马氏体时效不锈钢中逆转变奥氏体的析出与长大行为 [J]. 金属热处理, 2010, 35(2): 11
[38] Viswanathan U K, Dey G K, Sethumadhavan V. Effects of austenite reversion during overageing on the mechanical properties of 18Ni(350) maraging steel [J]. Mater. Sci. Eng., 2005, A398: 367
[39] Johnson W H. II. On some remarkable changes produced in iron and steel by the action of hydrogen and acids [J]. Proc. R. Soc. London, 1875, 23: 168
[40] Frohmberg R P, Barnett W J, Troiano A R. Delayed failure and hydrogen embrittlement in steel [J]. Tech. Rep., 1954, DOI: 10.21236/ad0038142
[41] Nie Y H, Kimura Y, Inoue T, et al. Hydrogen embrittlement of a 1500-MPa tensile strength level steel with an ultrafine elongated grain structure [J]. Metall. Mater. Trans., 2012, 43A: 1670
[42] Nagao A, Hayashi K, Oi K, et al. Effect of uniform distribution of fine cementite on hydrogen embrittlement of low carbon martensitic steel plates [J]. ISIJ Int., 2012, 52: 213
[43] Asahi H, Hirakami D, Yamasaki S. Hydrogen trapping behavior in vanadium-added steel [J]. ISIJ Int., 2003, 43: 527
[44] Wei F G, Hara T, Tsuzaki K. Precise determination of the activation energy for desorption of hydrogen in two Ti-added steels by a single thermal-desorption spectrum [J]. Metall. Mater. Trans., 2004, 35B: 587
[45] Wei F G, Hara T, Tsuzaki K. Hydrogen trapping character of nano-sized NbC precipitates in tempered martensite [A]. Proceedings of the 2008 International Hydrogen Conference-Effects of Hydrogen on Materials [C]. Materials Park, OH: ASM International, 2009: 448
[46] Wei F G, Tsuzaki K. Quantitative analysis on hydrogen trapping of TiC particles in steel [J]. Metall. Mater. Trans., 2006, 37A: 331
[47] Takahashi J, Kawakami K, Kobayashi Y, et al. The first direct observation of hydrogen trapping sites in TiC precipitation-hardening steel through atom probe tomography [J]. Scr. Mater., 2010, 63: 261
[48] Takahashi J, Kawakami K, Tarui T. Direct observation of hydrogen-trapping sites in vanadium carbide precipitation steel by atom probe tomography [J]. Scr. Mater., 2012, 67: 213
[49] Kawakami K, Matsumiya T. Numerical analysis of hydrogen trap state by TiC and V4C3 in bcc-Fe [J]. ISIJ Int., 2012, 52: 1693
[50] Li X F, Zhang J, Fu Q Q, et al. Hydrogen embrittlement of high strength steam turbine last stage blade steels: Comparison between PH17-4 steel and PH13-8Mo steel [J]. Mater. Sci. Eng., 2019, A742: 353
[51] Tsay L W, Chen H H, Chiang M F, et al. The influence of aging treatments on sulfide stress corrosion cracking of PH 13-8 Mo steel welds [J]. Corros. Sci., 2007, 49: 2461
[52] Wei F G, Tsuzaki K. Hydrogen absorption of incoherent TiC particles in iron from environment at high temperatures [J]. Metall. Mater. Trans., 2004, 35A: 3155
[53] Depover T, Escobar D P, Wallaert E, et al. Effect of hydrogen charging on the mechanical properties of advanced high strength steels [J]. Int. J. Hydrogen Energy, 2014, 39: 4647
[54] Olden V, Thaulow C, Johnsen R. Modelling of hydrogen diffusion and hydrogen induced cracking in supermartensitic and duplex stainless steels [J]. Mater. Des., 2008, 29: 1934
[55] Oriani R A. Hydrogen embrittlement of steels [J]. Annu. Rev. Mater. Sci., 1978, 8: 327
[56] Liu Q L, Venezuela J, Zhang M X, et al. Hydrogen trapping in some advanced high strength steels [J]. Corros. Sci., 2016, 111: 770
[57] Li X F, Zhang J, Chen J, et al. Effect of aging treatment on hydrogen embrittlement of PH 13-8 Mo martensite stainless steel [J]. Mater. Sci. Eng., 2016, A651: 474
[58] Yang J L, Huang F, Guo Z H, et al. Effect of retained austenite on the hydrogen embrittlement of a medium carbon quenching and partitioning steel with refined microstructure [J]. Mater. Sci. Eng., 2016, A665: 76
[59] Zhu X, Li W, Zhao H S, et al. Hydrogen trapping sites and hydrogen-induced cracking in high strength quenching & partitioning (Q&P) treated steel [J]. Int. J. Hydrogen Energy, 2014, 39: 13031
[60] Fan Y H, Zhang B, Yi H L, et al. The role of reversed austenite in hydrogen embrittlement fracture of S41500 martensitic stainless steel [J]. Acta Mater., 2017, 139: 188
[61] Yang Y, Zhang H M, Wu Z H, et al. Analysis and protection of stress corrosion of 300M ultra-high strength steel for landing gear [J]. Equip. Environ. Eng., 2016, 13(1): 68
[61] 杨 永, 张宏明, 吴朝华等. 起落架用300M超高强度钢应力腐蚀分析与防护 [J]. 装备环境工程, 2016, 13(1): 68
[62] Luo H, Yu Q, Dong C F, et al. Influence of the aging time on the microstructure and electrochemical behaviour of a 15-5PH ultra-high strength stainless steel [J]. Corros. Sci., 2018, 139: 185
[63] Yu Q. Evolution mechanism of nanphase and its influence on corrosion of high strength stinless steel [D]. Beijing: University of Science and Technology Beijing, 2017
[63] 余 强. 高强度不锈钢中纳米析出相演变规律及其对腐蚀的影响 [D]. 北京: 北京科技大学, 2017
[64] Pardo A, Merino M C, Coy A E, et al. Influence of Ti, C and N concentration on the intergranular corrosion behaviour of AISI 316Ti and 321 stainless steels [J]. Acta Mater., 2007, 55: 2239
[1] LU Yuhua, WANG Haizhou, LI Dongling, FU Rui, LI Fulin, SHI Hui. A Quantitative and Statistical Method of γ' Precipitates in Superalloy Based on the High-Throughput Field Emission Scanning Eelectron Microscope[J]. 金属学报, 2023, 59(7): 841-854.
[2] WANG Bin, NIU Mengchao, WANG Wei, JIANG Tao, LUAN Junhua, YANG Ke. Microstructure and Strength-Toughness of a Cu-Contained Maraging Stainless Steel[J]. 金属学报, 2023, 59(5): 636-646.
[3] HAN En-Hou, WANG Jianqiu. Effect of Surface State on Corrosion and Stress Corrosion for Nuclear Materials[J]. 金属学报, 2023, 59(4): 513-522.
[4] CHANG Litao. Corrosion and Stress Corrosion Crack Initiation in the Machined Surfaces of Austenitic Stainless Steels in Pressurized Water Reactor Primary Water: Research Progress and Perspective[J]. 金属学报, 2023, 59(2): 191-204.
[5] RUI Xiang, LI Yanfen, ZHANG Jiarong, WANG Qitao, YAN Wei, SHAN Yiyin. Microstructure and Mechanical Properties of a Novel Designed 9Cr-ODS Steel Synergically Strengthened by Nano Precipitates[J]. 金属学报, 2023, 59(12): 1590-1602.
[6] CHEN Kaixuan, LI Zongxuan, WANG Zidong, Demange Gilles, CHEN Xiaohua, ZHANG Jiawei, WU Xuehua, Zapolsky Helena. Morphological Evolution of Fe-Rich Precipitates in a Cu-2.0Fe Alloy During Isothermal Treatment[J]. 金属学报, 2023, 59(12): 1665-1674.
[7] MA Guonan, ZHU Shize, WANG Dong, XIAO Bolv, MA Zongyi. Aging Behaviors and Mechanical Properties of SiC/Al-Zn-Mg-Cu Composites[J]. 金属学报, 2023, 59(12): 1655-1664.
[8] MA Zhimin, DENG Yunlai, LIU Jia, LIU Shengdan, LIU Honglei. Effect of Quenching Rate on Stress Corrosion Cracking Susceptibility of 7136 Aluminum Alloy[J]. 金属学报, 2022, 58(9): 1118-1128.
[9] LI Xiaolin, LIU Linxi, LI Yating, YANG Jiawei, DENG Xiangtao, WANG Haifeng. Mechanical Properties and Creep Behavior of MX-Type Precipitates Strengthened Heat Resistant Martensite Steel[J]. 金属学报, 2022, 58(9): 1199-1207.
[10] LIU Xuxi, LIU Wenbo, LI Boyan, HE Xinfu, YANG Zhaoxi, YUN Di. Calculation of Critical Nucleus Size and Minimum Energy Path of Cu-Riched Precipitates During Radiation in Fe-Cu Alloy Using String Method[J]. 金属学报, 2022, 58(7): 943-955.
[11] WANG Shuo, WANG Junsheng. Structural Evolution and Stability of the δ′/θ′/δ′ Composite Precipitate in Al-Li Alloys: A First-Principles Study[J]. 金属学报, 2022, 58(10): 1325-1333.
[12] XIAO Na, HUI Weijun, ZHANG Yongjian, ZHAO Xiaoli. Hydrogen Embrittlement Behavior of a Vacuum-Carburized Gear Steel[J]. 金属学报, 2021, 57(8): 977-988.
[13] LI Xueda, LI Chunyu, CAO Ning, LIN Xueqiang, SUN Jianbo. Crystallography of Reverted Austenite in the Intercritically Reheated Coarse-Grained Heat-Affected Zone of High Strength Pipeline Steel[J]. 金属学报, 2021, 57(8): 967-976.
[14] LAN Liangyun, KONG Xiangwei, QIU Chunlin, DU Linxiu. A Review of Recent Advance on Hydrogen Embrittlement Phenomenon Based on Multiscale Mechanical Experiments[J]. 金属学报, 2021, 57(7): 845-859.
[15] ZHU Wenting, CUI Junjun, CHEN Zhenye, FENG Yang, ZHAO Yang, CHEN Liqing. Design and Performance of 690 MPa Grade Low-Carbon Microalloyed Construction Structural Steel with High Strength and Toughness[J]. 金属学报, 2021, 57(3): 340-352.
No Suggested Reading articles found!