Baojun ZHAO,Yuhong ZHAO,Yuanyang SUN,Wenkui YANG,Hua HOU. Effect of Mn Composition on the Nanometer Cu-Rich Phase of Fe-Cu-Mn Alloy by Phase Field Method. Acta Metall Sin, 2019, 55(5): 593-600.
The precipitation of nanometer Cu-rich phase can be observed in Fe-Cu alloy systems during isothermal ageing. The existence of Cu-rich phase is one of the reasons for the embrittlement of reactor pressure vessel (RPV) steel. The phase-field method applies a set of field variables defined by functions of space and time to describe the temporal evolution of composition and structural parameter, characterizing microstructure evolution during phase transformation. This work uses phase-field model to simulate the three-dimensional morphology, the volume fraction, number density and average particle radius of Cu-rich phase in Fe-Cu-Mn alloy at 823 K. The chemical free energy is derived from the thermodynamic database of the calculated phase diagram (CALPHAD), so the microstructure evolution of precipitation changes are directly corresponded to phase diagram of the real alloy system. The simulation results show that nanometer Cu-rich phase are formed by the spinodal decomposition mechanism in the early stage of phase separation. Meanwhile, Mn atoms segregate to the center of the Cu-rich phase. During the process of Ostwald coarsening, Mn atoms migrate from core to the interface of Cu-rich phase, finally forming Mn-rich ring distributed in the exterior of Cu-rich phase. Its existence can decrease the rates of diffusion growth and coarsening of Cu-rich phase. The Cu-rich phase is bcc structure and disperses in the matrix with spherical shape in the early stage of ageing. As the Cu-rich phase continues to grow, it will transform into fcc structure with ellipsoid or rod shapes. Meanwhile, increasing Mn content of Fe-Cu-Mn alloy accelerates the precipitation of Cu-rich phase and facilitates the growth and coarsening of Cu-rich phase.
Fund: National Natural Science Foundation of China(U1610123);National Natural Science Foundation of China(51674226);National Natural Science Foundation of China(51574206);National Natural Science Foundation of China(51774254);National Natural Science Foundation of China(51701187);Science and Technology Major Project of Shanxi Province(MC2016-06)
Table 1 The parameters used in the phase field model[31]
Fig.1 Morphology evolutions of Cu precipitates in Fe-Cu-Mn alloys with 1% (a1~d1), 3% (a2~d2) and 5% (a3~d3) Mn aged at 823 K and ageing time of t*=3000 (a1~a3), t*=3500 (b1~b3), t*=5000 (c1~c3) and t*=7500 (d1~d3)Color online
Fig.2 Concentration distribution curves of Cu and Mn at defined horizontal line in Fe-Cu-Mn alloys with 1% (a), 3% (b) and 5% (c) Mn aged for t*=3000 at 823 K
Fig.3 Concentration distribution curves of Cu precipitates at defined horizontal line in Fe-Cu-Mn alloys with 1% (a) and 5% (b) Mn aged at 823 K for different time
Fig.4 Structure order parameter of Cu precipitates at defined horizontal line in Fe-Cu-Mn alloys with 1% (a), 3% (b) and 5% (c) Mn aged at 823 K for different time
Fig.5 Variation of volume fraction of Cu-rich phase in Fe-Cu-Mn alloys with 1%, 3% and 5% Mn aged at 823 K as a function of ageing time
Fig.6 The particle number density of the Cu-rich phase in Fe-Cu-Mn alloys with 1%, 3% and 5% Mn aged at 823 K as a function of ageing time
Fig.7 The particle number density of the Cu-rich phase in Fe-Cu-Mn alloys with 1%, 3% and 5% Mn aged at 823 K as a function of ageing time
[1]
MillerM K, RussellK F. Embrittlement of RPV steels: An atom probe tomography perspective[J]. J. Nucl. Mater., 2010, 371: 145
[2]
LuZ. Radiator-induced embrittlement and life evaluation of reactor pressure vessels[J].Acta Metall. Sin., 2011, 47: 777
ZhangZ W, LiuC T, WangX L, et al. Effects of proton irradiation on nanocluster precipitation in ferritic steel containing fcc alloying additions[J]. Acta Mater., 2012, 60: 3034
[4]
StymanP D, HydeJ M, WilfordK, et al. Precipitation in long term thermally aged high copper, high nickel model RPV steel welds[J]. Prog. Nucl. Energy, 2012, 57: 86
[5]
LambrechtM, MeslinE, MalerbaL, et al. On the correlation between irradiation-induced microstructural features and the hardening of reactor pressure vessel steels[J]. J. Nucl. Mater., 2010, 406: 84
[6]
RadiguetB, PareigeP, BarbuA. Irradiation induced clustering in low copper or copper free ferritic model alloys[J]. Nucl. Instrum. Methods Phys. Res., 2009, 267B: 1496
[7]
LiB Y, ZhangL, LiC L, et al. Finding non-classical critical nuclei and minimum energy path of Cu precipitates in Fe-Cu alloys[J]. Modell. Simul. Mater. Sci. Eng., 2017, 25: 085006
[8]
DeschampsA, MilitzerM, PooleW J. Precipitation kinetics and strengthening of a Fe-0.8wt%Cu alloy[J]. ISIJ Int., 2001, 41: 196
[9]
LiuZ C, LiW X, WangY F, et al. Precipitation of Cu in Fe-1.12Cu alloys[J].Heat Treat. Met., 2005, 30(6): 40
XuG, ChuD F, CaiL L, et al. Investigation on the precipitation and structural evolution of Cu-rich nanophase in RPV model steel[J].Acta Metall. Sin., 2001, 47: 905
LiuF, ZhouB X, PengJ C, et al. Characterization of a complex crystal structure within Cu-rich precipitates in RPV model steel[J]. J.Mater. Eng., 2015, 43(7): 80
[12]
LeeT H, KimY O, KimS J. Crystallographic model for bcc-to-9R martensitic transformation of Cu precipitates in ferritic steel[J]. Philos. Mag., 2007, 87: 209
[13]
BlackstockJ J, AcklandG J. Phase transitions of copper precipitates in Fe-Cu alloys[J]. Philos. Mag., 2001, 81A: 2127
[14]
MonzenR, IguchiM, JenkinsM L. Structural changes of 9R copper precipitates in an aged Fe-Cu alloy[J]. Philos. Mag. Lett., 2000, 80: 137
[15]
WenY R, HirataA, ZhangZ W, et al. Microstructure characterization of Cu-rich nanoprecipitates in a Fe-2.5Cu-1.5Mn-4.0Ni-1.0Al multicomponent ferritic alloy[J]. Acta Mater., 2013, 61: 2133
[16]
ShenQ, XiongX Y, LiT, et al. Effects of co-addition of Ni and Al on precipitation evolution and mechanical properties of Fe-Cu alloy[J]. Mater. Sci. Eng., 2018, A723: 279
[17]
MillerM K, WirthB D, OdetteG R. Precipitation in neutron-irradiated Fe-Cu and Fe-Cu-Mn model alloys: A comparison of APT and SANS data[J]. Mater. Sci. Eng., 2003, A353: 133
[18]
GladeS C, WirthB D, OdetteG R, et al. Positron annihilation spectroscopy and small-angle neutron scattering characterization of the effect of Mn on the nanostructural features formed in irradiated Fe-Cu-Mn alloys[J]. Philos. Mag., 2005, 85: 629
[19]
WangX J. Mechanism research of nanaoscale composite precipitates in Fe-Cu-Ni-Al-Mn steel[D]. Shanghai: Shanghai University, 2016
MaQ S, JinY C, ZhaoY H, et al. Microscopic phase-field simulation for the influence of interatomic potential on the precipitation process of Ni75Al14Mo11 alloy[J]. Acta Metall. Sin. (Engl. Lett.), 2016, 29: 975
[21]
WangK, ZhaoY H, YangD R, et al. Microscopic phase-field simulation for formation of pre-precipitation for Ni75Al14 Mo11[J]. Rare Met. Mater. Eng., 2015, 44: 939
[22]
ZhaoY H. Simulation for the Materials Microstructure Evolution in Phase Transformation Process[M]. Beijing: National Defend Industry Press, 2010: 12
[22]
(赵宇宏. 材料相变过程微观组织模拟 [M]. 北京: 国防工业出版社, 2010: 12)
[23]
ZhaoY H, HouH. Simulation of dendritic crystal growth of pure Ni using the phase-field model[J]. Rev. Adv. Mater. Sci., 2013, 33: 246
[24]
ZhaoY H. Atomic-Scale computer simulation for alloy during early precipitation process[D]. Xi'an: Northwestern Polytechnical University, 2003
[24]
(赵宇宏. 合金早期沉淀过程的原子尺度计算机模拟 [D]. 西安: 西北工业大学, 2003)
[25]
CahnJ W. On Spinodal decomposition[J]. Acta Metall., 1961, 9: 795
[26]
CahnJ W, HilliardJ E. Free energy of a nonuniform system. I. Iinterfacial free energy[J]. J. Chem. Phys., 1958, 28: 258
[27]
CahnJ W, AllenS M. A microscopic theory for domain wall motion and its experimental verification in Fe-Al alloy domain growth kinetics[J]. J. Phys., 1977, 38: S51
[28]
AllenS M, CahnJ W. A microscopic theory for antiphase boundary motion and its application to antiphase domain coarsening[J]. Acta Metall., 1979, 27: 1085
[29]
KoyamaT, HashimotoK, OnoderaH. Phase-field simulation of phase transformation in Fe-Cu-Mn-Ni quaternary alloy[J]. J. Mater. Trans., 2006, 47: 2765
[30]
KoyamaT, OnoderaH. Phase-field modeling of the microstructure evolutions in Fe-Cu base alloys[J]. Mater. Sci. Forum, 2007, 539-543: 2383
[31]
BuergerM J. A handbook of lattice spacings and structures of metals and alloys[J]. Z. Kristallogr., 1961, 115: 319
[32]
DinsdaleA T. SGTE data for pure elements[J]. Calphad, 1991, 15: 317
[33]
WuX C. Precipitation kinetics in Ni-Al alloys using phase field simulation[D]. Nanjing: Nanjing University of Science & Technology, 2016
[33]
(吴兴超. Ni-Al合金沉淀动力学的相场法研究 [D]. 南京: 南京理工大学, 2016)
[34]
MiettinenJ. Thermodynamic description of the Cu-Mn-Ni system at the Cu-Ni side[J]. Calphad, 2003, 27: 147
YIN Zhongda; LI Hiaodong;LI Haibin; LAI Zhonghong(Harbin Instilute of Technology; Harbin 150001)(Manuscript received 94-01-13; in revised form 94-06-06). AGING MECHANISM OF 18Ni MARAGING STEEL[J]. 金属学报, 1995, 31(1): 7-13.