| EFFECT OF ELECTROMAGNETIC MELT TREATMENT NEAR LIQUIDUS ON THE FORMATION OF NON-DENDRITE MICROSTRUCTURE OF SUPERALLOY |
GAO Zhongtang, HU Rui( ), WANG Jun, YANG Jieren, LI Jinshan |
| State Key Laboratory of Solidification Processing, Northwestern Polytechnical University, Xi'an 710072 |
|
Cite this article:
GAO Zhongtang, HU Rui, WANG Jun, YANG Jieren, LI Jinshan. EFFECT OF ELECTROMAGNETIC MELT TREATMENT NEAR LIQUIDUS ON THE FORMATION OF NON-DENDRITE MICROSTRUCTURE OF SUPERALLOY. Acta Metall Sin, 2014, 50(12): 1471-1477.
|
|
|
Abstract The effects of electromagnetic field and melt treatment near liquidus on the grain refinement of the Ni-20Cr-18W (mass fraction, %) superalloy have been studied. The average grain size of 60 kg ingot can be refined to 127 μm and the grains are both ?ne and globular. Based on the effect of electromagnetic field on atomic cluster, interface stability and transformation from dendritic grain to globular grain, the mechanism of grain refinement has been studied from the aspect of nucleation thermodynamics by OM, SEM, EBSD. The results show that electromagnetic melt treatment near liquidus results in signi?cant re?nement. The grain refinement can be attributed to the mechanism that atomic clusters and globular structures can become the nucleus when the initial undercooling reaches certain level. Electromagnetic field not only improves homogeneity of the macroscopic temperature field, but also plays a positive role in interface stability and dendritic to globular transformation, which increases the nucleation rate.
|
|
|
|
|
| Fund: Supported by National Basic Research Program of China (No.2011CB610404), Program of Introducing Talents of Discipline to Universities (No.B08040) and Research Found of the State Key Laboratory of Solidification Processing China (No.62-TP-2011) |
| [1] |
Kotadia H R, Zhang H, Fan Z. Mater Lett, 2010; 64: 671
|
| [2] |
Haghayehi R, Nastac L. Mater Lett, 2011; 65: 3230
|
| [3] |
Xiong Y H, Li P J, Yang A M, Yan W D, Zeng D B, Liu L. Acta Metall Sin, 2002; 38: 529
|
|
(熊玉华, 李培杰, 杨爱民, 严卫东, 曾大本, 刘 林. 金属学报, 2002; 38: 529)
|
| [4] |
Zhou Y H. Solidification Technology. Beijing: Mechanical Industry Press, 1998: 55
|
|
(周尧和. 凝固技术. 北京: 机械出版社, 1998: 55)
|
| [5] |
Xia K, Tausing G. Mater Sci Eng, 1998; A246: 1
|
| [6] |
Li X F, Zhang F, Zu F Q, Lv X, Zhao Z X, Yang D D. J Alloys Compd, 2010; 505: 472
|
| [7] |
Wang Y Q, Wu Y Q, Liu J T, Bian X F. Chin Phy Lett, 2006; 23: 2513
|
| [8] |
Men H, Jiang B, Fan Z. Acta Mater, 2010; 58: 6526
|
| [9] |
Alirezar K, Miwa K J, Toshiyuki K S. Trans Nonferrous Met Soc China, 1998; 29: 1477
|
| [10] |
Du Y Y, Lu Y P, Wang T M, Li T J, Zhang G L. Proc Eng, 2012; 27: 1129
|
| [11] |
Wang J S, Xue Q G, Chang G W, Tang Y, Wang J Z, Cang D Q. J Univ Sci Technol Beijing, 2004; 11: 123
|
| [12] |
Haghayeghi R, Nastac L. Mater Lett, 2011; 65: 3230
|
| [13] |
Zhang X L, Li T J, Teng H T, Me S S, Jin J Z. Mater Sci Eng, 2007; A475: 194
|
| [14] |
Wannasin J, Canyook R, Wisutmethangoon S, Flemings M C. Acta Mater, 2013; 61: 3897
|
| [15] |
Li Q S, Song C J, Li H B, Zhai Q J. Mater Sci Eng, 2007; A466: 101
|
| [16] |
Zi B T, Ba Q X, Cui J Z, Xu G M. Scr Mater, 2000; 43: 377
|
| [17] |
He S X, Wang J, Zhou Y H. Acta Metall Sin, 2002; 38: 379
|
|
(何树先, 王 俊, 周尧和. 金属学报, 2002; 38: 379)
|
| [18] |
Liu Y, Hu R, Li J S. Mater Sci Eng, 2009; A508: 141
|
| [19] |
Yue J T, Voltmer W. J Cryst Growth, 1975; 29: 32
|
| [20] |
Li M J, Takuya T, Naoki O, Kenji M W. J Alloys Compd, 2009; 487: 187
|
| [21] |
Shibayan R, Satyam S, Tamirisa K. Acta Mater, 2011; 59: 5494
|
| [22] |
Zuo Y B, Cui J Z, Zhao H T. J Mater Sci, 2012; 47: 5501
|
| [23] |
Wang B, Yang Y S, Zhou J X, Tong W H. Rare Met Mater Eng, 2009; 38: 519
|
|
(汪 彬, 杨院生, 周吉学, 童文辉. 稀有金属材料与工程, 2009; 38: 519)
|
| [24] |
Jia P, Wang E G, Lu L, He J C. Acta Metall Sin, 2013; 49: 1573
|
|
(贾 鹏, 王恩刚, 鲁 辉, 赫冀成. 金属学报, 2013; 49: 1573)
|
| [25] |
Fan Z, Wang Y, Xia M, Arumuganathar S. Acta Mater, 2009; 57: 4891
|
| [26] |
Li T, Lin X, Huang W D. Acta Mater, 2006; 54: 4815
|
| [27] |
Lin X, Tong L L, Zhao L N, Wanng L L, Wang M, Huang W D. Trans Nonferrous Met Soc China, 2010; 20: S826
|
| [28] |
Dong J, Lu G M, Ren Q F, Cui J Z. Acta Metall Sin, 2002; 38: 203
|
|
(董 杰, 路贵民, 任栖峰, 崔建中. 金属学报, 2002; 38: 203)
|
| [29] |
Flemings M C. Solidification Processing. New York: McGraw Hill Book Company, 1974: 42
|
| [30] |
Huang Y, Liu S, Lu D Y, Zhou Y H, Cheng G S, Zhang F S. Chin Space Sci Technol, 1989; 9(1): 7
|
|
(黄 焰, 刘 山, 鲁德洋, 周尧和, 程功善, 张福生. 中国空间科学技术, 1989; 9(1): 7)
|
| [31] |
Shu D, Sun B D, Mi J, Gran P S. Acta Mater, 2011; 59: 2
|
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|