| CRYSTALLIZATION PROCESS AND NON–ISOTHERMAL CRYSTALLIZATION KINETICS OF MELT–SPUN Nd–Fe–B AMORPHOUS THICK RIBBONS |
| WANG Dapeng; BAO Xiaoqian; ZHANG Maocai; ZHU Jie |
| State Key Laboratory of Advanced Metals and Materials; University of Science and Technology Beijing; Beijing 100083 |
|
Cite this article:
WANG Dapeng; BAO Xiaoqian; ZHANG Maocai; ZHU Jie. CRYSTALLIZATION PROCESS AND NON–ISOTHERMAL CRYSTALLIZATION KINETICS OF MELT–SPUN Nd–Fe–B AMORPHOUS THICK RIBBONS. Acta Metall Sin, 2009, 45(2): 237-242.
|
|
|
Abstract Crystallization processes and non–isothermal crystallization kinetics of Nd6Fe72B22 and Nd6Fe68Ti4B17C5 amorphous thick ribbons rapidly quenched at a roller running rate of 12 m/s were investigated by means of DSC, XRD, Kempen model and Kissinger equation, respectively.
Two thick ribbons show different crystallization processes and kinetic mechanisms. The crystallization processes of Nd6Fe72B22 and Nd6Fe68Ti4B17C5 alloys can be discribed as: amorphous phase (AP)→ Nd2Fe23B3→Nd2Fe14B+ α--Fe +Fe3B→Nd2Fe14B+α--Fe+Fe3B+NdFe4B4, and AP→Nd2(Fe, Ti)14(B, C)+α--Fe + Fe3B, respectively. Different from polymorphic crystallization controlled by interface for Nd6Fe72B22 alloy, the crystallization of Nd6Fe68Ti4B17C5 is eutectoidic and the nucleus growth is controlled by diffusion.
|
|
Received: 10 July 2008
|
| [1] Croat J J, Herbst J F, Lee R W, Pinkerton F E. J Appl Phys, 1984; 55: 2078
[2] Skomski R. J Appl Phys, 1994; 76: 7059
[3] Biswas K, Ram S, Schultz L, Eckert J. J Alloys Compd, 2005; 397: 104
[4] Li F S, Zhang T, Guan S K, Shen N F. Trans Nonferrous Met Soc China, 2004; 14: 840
[5] Guschl P C, Kim H S, Otaigbe J U. J Appl Polym Sci, 2001; 83: 1091
[6] Horiguchi T, Sekizawa H, Murata M, Kondo H, Kawagoe T, Iguchi Y, Kohn K, Mizoguchi T. Key Eng Mater, 1990; 40: 87
[7] Gao Y Q, Wang W. J Non–Cryst Solids, 1986; 81: 129
[8] Kempen A TW, Sommer F, Mittemeijer E J. J Mater Sci, 2002; 37: 1321
[9] Kissinger H E. Anal Chem, 1957; 29: 1702
[10] Lu K. Mater Sci Eng, 1996; R16: 161
[11] Trujillo M P, Orozco A, Casas–Ruiz M, Ligero R A, Jimenez–Garay R. Mater Lett, 1995; 24: 287
[12] Cahn J W. Acta Metall, 1956; 4: 572
[13] Yinnon H, Uhlmann D R. J Non–Cryst Solids, 1983; 54: 253
[14] Gao Y Q,WangW, Zheng F Q, Liu X. J Non–Cryst Solids, 1986; 81: 135
[15] Jain R, Saxena N S, Bhandari D, Sharma S K, Rao K V R. Phys B (Amsterdam, Neth), 2001; 301B: 341
[16] Liu X J, Hui X D, Chen G L. Mater Sci Forum, 2005; 475: 3385
[17] Soliman A A, Al–Heniti S, Al–Hajry A, Al–Assiri M, Al–Barakati G. Therm Acta, 2004; 413: 57
[18] Christian J W. Theory of Transformation in Metals and Alloys. 2nd ed., Oxford: Pergamon Press; 1975: 487
[19] Takeuchi A, Inoue A. Mater Trans, 2005; 46: 2817
[20] Wang Y H, Yang Y S. Amorphous Alloys. Beijing: Metallurgical Industry Press; 1989: 96
(王一禾, 杨膺善. 非晶态合金. 北京: 冶金工业出版社; 1989:96) |