MULTISCALE SIMULATION OF NANOINDENTATION ON Al THIN FILM
LI Junwan1;  NI Yushan1;  LIN Yihan1;  LUO Cheng1; JIANG Wugui2
1.Department of Mechanics and Engineering Science; Fudan University; Shanghai 200433
2.Faculty of Built Environment and Engineering; Queensland University of Technology; Brisbane QLD4001; Australia
Cite this article: 

LI Junwan NI Yushan LIN Yihan LUO Cheng JIANG Wugui. MULTISCALE SIMULATION OF NANOINDENTATION ON Al THIN FILM. Acta Metall Sin, 2009, 45(2): 129-136.

Download:  PDF(4305KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  

In order to study the early stages of plastic deformation with initial defect under the action of an indenter, the nanoindentation processes of the single crystal aluminum thin film were simulated using the quasicontinuum method. The load vs displacement response curves and strain energy vs displacement curves of the single crystal aluminum thin film with initial defect and defect--free were presented, respectively. The nanoindentation processes under influences of the initial defect were investigated about dislocation nucleation, dislocation emission, Peierls stress and load necessary for dislocation emission. The results demonstrate that the load vs displacement response curves experience many times abrupt drops with the emission of dislocations beneath the indenter. The initial defect is found to be insignificant on nucleation and emission of the 1st and 3rd dislocation dipoles, but has a distinct effect on the 2nd dislocation dipole. The nucleation and emission of the 2nd dislocation dipole is postponed obviously because of the effect of initial defect, and then crack propagation is accompanied. The strain energy of single crystal aluminum thin film and Peierls stress of dislocation dipole beneath the indenter increase with deformation processes due to the severe lattice distortion in the thin film. Before the cleavage occurs, the load necessary for the 2nd dislocation dipole nucleation and emission increases in nanoindentation with initial defect, on the contrary, it decreases after the cleavage occurred. The nanohardness and Peierls stress in this simulation show a good agreement with relevant theoretical and experimental results.

Key words:  Al film      nanoindentation      multiscale      quasicontinuum method      initial defect     
Received:  20 July 2008     
ZTFLH: 

TB383

 
Fund: 

National Natural Science Foundation of China (No. 10576010)

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2009/V45/I2/129

[1] Oliver W C, Pharr G M. J Mater Res, 1992; 7: 1564
[2] Li X D, Bhushan B. Mater Charact, 2002; 48: 11
[3] Bamber M J, Cooke K E, Mann A B, Derby B. Thin Solid Films, 2001; 399: 299
[4] Bhushan B, Koinkar V N. Appl Phys Lett, 1994; 64: 1653
[5] Chen J, Bull S J. Thin Solid Films, 2006; 494: 1
[6] Sangwal K, Gorostiza P, Sanz F. Surf Sci, 2000; 446: 314
[7] Zimmerman J A, Kelchner C L, Klein P A, Hamilton J C, Foiles S M. Phys Rev Lett, 2001; 87: 165507
[8] Shankar R M. Appl Phys Lett, 2007; 90: 171924
[9] Kiely J D, Hwang R Q, Houston J E. Phys Rev Lett, 1998;81: 4424
[10] Yang B, Vehoff H. Acta Mater, 2007; 55: 849
[11] Soifer Y M, Verdyan A, Kazakevich M, Rabkin E. Scr Mater, 2002; 47: 799
[12] Liu Y, Varghese S, Ma J, Yoshino M, Lu H, Komanduri R. Int J Plast, 2008; 24: 1990
[13] Kiely J D, Houston J E. Phys Rev, 1998; 19B: 12588
[14] Phillips R, Rodney D, Shenoy V, Tadmor E, Ortiz M. Modell Simul Mater Sci Eng, 1999; 7: 769
[15] Shenoy V B, Phillips R, Tadmor E B. J Mech Phys Solids,2000; 48: 649
[16] Ni Y S, Wang H T. Chin Q Mech, 2005; 26: 366
(倪玉山, 王华滔.力学季刊, 2005; 26: 366)
[17] Tadmor E B, Miller R, Phillips R. J Mater Res, 1999; 14:2233
[18] Shan D, Yuan L, Guo B. Mater Sci Eng, 2005; A412: 264
[19] Iglesias R A, Leiva E P. Acta Mater, 2006; 54: 2655
[20] Li J W, Jiang W G. Acta Metall Sin, 2007; 43: 851
(黎军顽, 江五贵.金属学报, 2007; 43: 851)
[21] Jiang W G, Li J W, Su J J, Tang J L. Acta Mech Solida Sin, 2007; 28: 375
(江五贵, 黎军顽, 苏建君, 汤井伦.固体力学学报, 2007; 28:375)
[22] Ni Y S, Wang H T. Chin J Mech Eng, 2007; 43: 101
(倪玉山, 王华滔.机械工程学报, 2007; 43: 101)
[23] Tadmor E B, Hai S. J Mech Phys Solids, 2003; 51: 765
[24] Miller R, Ortiz M, Phillips R, Shenoy V, Tadmor E B. Eng Fract Mech, 1998; 61: 427
[25] Gannepalli A, Mallapragada S K. Phys Rev, 2002; 66B:104103
[26] Jarausch K F, Kiely J D, Houston J E, Russell P E. J Mater Res, 2000; 15: 1693
[27] Smith R, Christopher D, Kenny S D, Richter A, Wolf B. Phys Rev, 2003; 67B: 245405
[28] Van Vliet K J, Li J, Zhu T, Choi Y J, Yip S, Suresh S. Solid Mech Its Appl, 2004; 115: 203
[29] Kelchner C L, Plimpton S J, Hamilton J C. Phys Rev, 1998; 58B: 11085
[30] Tadmor E B. PhD Thesis, Brown University, Providence, Rhode Island, 1996
[31] Tadmor E B, Ortiz M, Phillips R. Philos Mag, 1996; 73A: 1529
[32] Tadmor E B, Phillips R, Ortiz M. Langmuir, 1996; 12: 4529
[33] Shenoy V B, Miller R, Tadmor E B, Rodney D, Phillips R, Ortiz M. J Mech Phys Solids, 1999; 47: 611
[34] Ercolessi F, Adams J B. Europhys Lett, 1994; 28: 538
[35] Minor A M, Lilleodden E T, Stach E A, Morris J W. J Mater Res, 2004; 19: 176
[36] Hirth J P, Lothe J. Theory of Dislocations. New York: John Wiley and Sons, 1982: 757
[37] Kosugi T, Kino T. Mater Sci Eng, 1993; A164: 368

[1] LI Shilei, LI Yang, WANG Youkang, WANG Shengjie, HE Lunhua, SUN Guang'ai, XIAO Tiqiao, WANG Yandong. Multiscale Residual Stress Evaluation of Engineering Materials/Components Based on Neutron and Synchrotron Radiation Technology[J]. 金属学报, 2023, 59(8): 1001-1014.
[2] ZHU Bin, YANG Lan, LIU Yong, ZHANG Yisheng. Micromechanical Properties of Duplex Microstructure of Martensite/Bainite in Hot Stamping via the Reverse Algorithms in Instrumented Sharp Indentation[J]. 金属学报, 2022, 58(2): 155-164.
[3] LIU Zhongqiu, LI Baokuan, XIAO Lijun, GAN Yong. Modeling Progress of High-Temperature Melt Multiphase Flow in Continuous Casting Mold[J]. 金属学报, 2022, 58(10): 1236-1252.
[4] LAN Liangyun, KONG Xiangwei, QIU Chunlin, DU Linxiu. A Review of Recent Advance on Hydrogen Embrittlement Phenomenon Based on Multiscale Mechanical Experiments[J]. 金属学报, 2021, 57(7): 845-859.
[5] SUN Xiaojun, HE Jie, CHEN Bin, ZHAO Jiuzhou, JIANG Hongxiang, ZHANG Lili, HAO Hongri. Effect of Fe Content on the Microstructure, Electrical Resistivity, and Nanoindentation Behavior of Zr60Cu40-xFex Phase-Separated Metallic Glasses[J]. 金属学报, 2021, 57(5): 675-683.
[6] LIU Jizhao, HUANG Hefei, ZHU Zhenbo, LIU Awen, LI Yan. Numerical Simulation of Nanohardness in Hastelloy N Alloy After Xenon Ion Irradiation[J]. 金属学报, 2020, 56(5): 753-759.
[7] LI Changji,ZOU Minjie,ZHANG Lei,WANG Yuanming,WANG Sucheng. High-Resolution X-Ray Diffraction Analysis of Epitaxial Films[J]. 金属学报, 2020, 56(1): 99-111.
[8] Sensen HUANG,Yingjie MA,Shilin ZHANG,Min QI,Jiafeng LEI,Yaping ZONG,Rui YANG. Influence of Alloying Elements Partitioning Behaviors on the Microstructure and Mechanical Propertiesin α+β Titanium Alloy[J]. 金属学报, 2019, 55(6): 741-750.
[9] Pengyue ZHAO, Yongbo GUO, Qingshun BAI, Feihu ZHANG. Research of Surface Defects of Polycrystalline Copper Nanoindentation Based on Microstructures[J]. 金属学报, 2018, 54(7): 1051-1058.
[10] Guangping ZHANG, Honglei CHEN, Xuemei LUO, Bin ZHANG. Progress in Thermal Fatigue of Micro/Nano-ScaleMetal Conductors[J]. 金属学报, 2018, 54(3): 357-366.
[11] Hongyang XU,Haibo KE,Huogen HUANG,Pei ZHANG,Pengguo ZHANG,Tianwei LIU. Nanoindentation Creep Behavior of U65Fe30Al5 Amorphous Alloy[J]. 金属学报, 2017, 53(7): 817-823.
[12] Jihou LIU,Hongyun ZHAO,Zhuolin LI,Xiaoguo SONG,Hongjie DONG,Yixuan ZHAO,Jicai FENG. Microstructures and Mechanical Properties of Cu/Sn/Cu Structure Ultrasonic-TLP Joint[J]. 金属学报, 2017, 53(2): 227-232.
[13] Yuqiu CHEN, Yapei ZU, Jun GONG, Cao SUN, Chen WANG. Effect of Al Film on the Electromagnetic Properties of Glass Fiber Reinforced Resin Matrix Composite[J]. 金属学报, 2017, 53(11): 1511-1520.
[14] Biao YANG,Bailin ZHENG,Xingjian HU,Pengfei HE,Zhufeng YUE. EFFECT OF VOID ON NANOINDENTATION PROCESS OF Ni-BASED SINGLE CRYSTAL ALLOY[J]. 金属学报, 2016, 52(2): 129-134.
[15] XU Yang, SUN Mingxue, ZHOU Yanlei, LIU Zhenyu. PRECIPITATION BEHAVIOR OF (Nb, Ti)C IN COILING PROCESS AND ITS EFFECT ON MICRO-MECHANICAL CHARACTERISTICS OF FERRITE[J]. 金属学报, 2015, 51(1): 31-39.
No Suggested Reading articles found!