| Superalloy fine powders prepared by a novel spark plasma discharge process |
| Changchun Ge;Jun YU;;;; |
| 北京科技大学材料科学与工程学院 |
|
Cite this article:
Changchun Ge; Jun YU. Superalloy fine powders prepared by a novel spark plasma discharge process. Acta Metall Sin, 2008, 44(7): 892-896 .
|
|
|
Abstract In the past three decades, the P/M superalloy in our country has a great progress. But in general, there is a big gap between domestic and foreign. The powders are the key. So a novel spark plasma discharge process , different from traditional process such as Plasma Rotating Electrode Process and Argon Gas Atomization, is proposed to produce Superalloy fine powders. Fine powders from wrought superalloy plate and a new P/M superalloy bar are studied.
|
|
Received: 06 December 2007
|
|
|
[1]Zhang Y W,Shangguan Y H.Powder Metall Ind,2004; 14(6):30 (张义文,上官永恒.粉末冶金工业,2004;14(6):30) [2]Zou J W,Wang W X.J Aeronaut Mater,2006;26:244 (邹金文,汪武祥.航空材料学报,2006;26:244) [3]Zhang Y,Zhang Y W,Song P S,Zhang F G,Tao Y,Chen X C,Yang S Z.J Iron Steel Res,2003;15:71 (张莹,张义文,宋璞生,张凤戈,陶宇,陈希春,杨仕仲.钢铁研究学报,2003;15:71) [4]Zhang L N,Zhang M C,Li X,Xie X S.Ordnance Mater Sci Eng,2001;24(3):64 (张丽娜,张麦仓,李晓,谢锡善.兵器材料科学与工程,2001;24(3):64) [5]Guo W M,Wu J T,Zhang F G,Zhou B,Zhao M H.Mater Rev,2004;18(11):87 (国为民,吴剑涛,张风戈,周波,赵明汉.材料导报,2004;18(11):87) [6]Zou J W,Wang W X.Powder Metall Technol,2001;19: 7 (邹金文,汪武祥.粉末冶金技术,2001;19:7) [7]Gessinger G H.Powder Met Int,1981;13:93 [8] [9]Chen S Q,Huang B Y.Powder Metall Technol,2004;22: 297 (陈仕奇,黄伯云.粉末冶金技术,2004;22:297) [10]Newell K.Met Powder Rep,1999;54(5):4 [11]Guha S.Met Powder Rep,1997;52(3):12 [12]Guha S.Mater Technol,1995;10(7-8):136 [13]Hu B F,Li H Y,Wu C J,Zhang S H.Acta Metall Sin, 1990;26:334 (胡本芙,李慧英,吴承建,章守华.金属学报,1990;26:334) [14]Chen H M,Hu B F,Li H Y,Yu Q M,Zhang Y W.Acta Metall Sin,2003;39:30 (陈焕铭,胡本芙,李慧英,余泉茂,张义文.金属学报,2003;39:30) [15]Wang X Q.Powder Metall Technol,2001;19:70 (王旭青.粉末冶金技术,2001;19:70) |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|