| Hydrogen evolution reaction on the composite LaNi5/Ni-S alloy film in alkaline medium |
| ;;; |
| 东北大学 |
|
Cite this article:
;. Hydrogen evolution reaction on the composite LaNi5/Ni-S alloy film in alkaline medium. Acta Metall Sin, 2008, 44(7): 887-891 .
|
|
|
Abstract By molten salt electrolysis combined with aquatic electrodeposition, the composite LaNi5/Ni-S film with high stability and HER activity was obtained. The results showed that in the Na3AlF6-La2O3 (92 : 8) molten salt system, although the cathodic potential is much lower than the decomposition potential of lanthanum, the LaNi5 film could be obtained due to the strong depolarization ability of Ni cathode. The composite LaNi5/Ni-S film (η150 = 75 mV, 80oC) could absorb large amount of H atoms, which would be oxidized and avoid the dissolution of the Ni-S film under the state of open-circuit effectively and prolong the lifetime of the cathode.
|
|
Received: 14 December 2007
|
|
|
[1]Norsk H.Netherlands Pat,7801955,1978 [2]Hine F,Yasuda M,Watanabe M.Denki Kagaku,1979;47: 401 (日根富郎,安田正雄,渡边正男.电气化学,1979;47:401) [3]Gonsalez E R,Avaca L A,Tremiliosi-Filho G.Int J Hy- drogen Energy,1994;19:17 [4]Sabela R,Paseka I.J Appl Electrochem,1990;20:500 [5]Paseka I.Electrochim Acta,1993;38:2449 [6]de Giz M J,Ferreira M,Gonzalez E R.J Appl Electrochem, 1993;23:641 [7]Vandenborre H,Vermeiren Ph,Leysen R.Electrochim Acta,1984;29:297 [8]Wen T C,Lin S M,Tsai J M.J Appl Electrochem,1994; 24:233 [9]Valand T,Burchardt T,Grontoft T.Int J Hydrogen En- ergy,2002;27:39 [10]Xu Y H,He G R,Wang X L.Int J Hydrogen Energy,2003; 28:961 [11]Kitamura T,Iwakura C,Tamura H.Chem Left,1981:965 [12]Kitamura T,Iwakura C,Tamura H.Chem Left,1981:1755 [13]Hu W K.Int J Hydrogen Energy,2000;25:111 [14]Bocutti R,Saeki M J,Florentino A O.Int J Hydrogen Energy,2000;25:1051 [15]Han Q,Liu K R,Chen J S.Int J Hydrogen Energy,2003; 28:1207 [16]Bard A J,Fauikner L R.Electrochemical Methods Fun- damentals and Applications.2nd Ed.,New York:John Wiley & Sons,INC,2003:135 [17]Carvalho J D,Tremiliosi-Filho G,Avaca L A.In:Srini- vasan S,Wagner S,Wroblowa H,eds.,Electrode Materials and Processes .for Energy Conversion and Storage.Pen- nington:The Electrochem Soc Inc,1987:356 [18]Vandenborre H,Vermeiren P,Leysen R.Electrochim Acta, 1984;29:297 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|