Abstract In this research the PLE(Partition Local Equilibrium)/NPLE(Negligible Partition Local Equilibrium) model has been introduced into the deformed system to describe the γ→α transformation of Fe-C-Xi alloy(Xi represents for one or several substitutional elements such as Mn, Si, Cr, etc). Based on a calculate method in static system which has been reported, a thermodynamic equation which suits the plastic deformed system is established under the orthoequilibrium model, to calculate the PLE-NPLE critical temperature. Isothermal γ→α transformation experiments have been conducted to a Fe-C0.073-Mn2.17-Si0.80-Cr0.88(wt%) steel under different temperatures after a process of hot deformation at 820℃and the critical temperature of PLE-NPLE is roughly mensurated. The experimental results correspond well with the calculated results and both of them reveal that deformation does heighten the critical temperature of PLE-NPLE, as for the tested steel in this paper, after a 40% nominal deformation at 820℃ by deformed rate of 0.5s-1, the critical temperature of PLE-NPLE in isothermal γ→α transformation has been heighten by nearly 10℃.
|
|
Received: 26 October 2007
|
|
|
[1]Purdy G R,Weihert D H,Kirkaldy J S.Trans TMS- AIME,1964;230:1025 [2]Coates D E.Metall Trans,1973;4A:2313 [3]Coates D E.Metall Trans,1972;3A:1203 [4]Coates D E.Metall Trans,1973;4A:1077 [5]Bowman F E.Trans ASM,1946;36:61 [6]Enomoto M.Trans ISIJ,1988;28:826 [7]Sheng G,Yang Z G.Acta Metall Sin,2007;43:349 (盛广,杨志刚.金属学报,2007;43:349) [8]Gllmour J B,Purdy G R,Kirkaldy J S.Metall Trans, 1972;3A:3213 [9]Umemoto M,Tamura I,Otsuka H.Tetsu Hagan■,1982; 68(Suppl.):1384 (梅本实,田村今男,大冢秀幸.铁钢,1982;68(增刊):1384) [10]Mecking H,Kocks U F.Acta Metall,1981;29:1865 [11]Yu Y N.Metallic Theory.Beijing:Metallurgial Industry Press,2000:295 (余永宁.金属学原理.北京:冶金工业出版社,2000:295) [12]Xu Z Y.Heat Treat,2005;19(2):1 (徐祖耀.热处理,2005;19(2):1) [13]Wang Q C,Yang Z G,Li Z D.Acta Metall Sin,2007;43: 344 (王启超,杨志刚,李昭东.金属学报.2007;43:344) [14]Luo H W,Sietsma J,Van der Zwaag S.Metall Mater Trans,2004;35A:2789 [15]Lan Y J,Huang C J,Li D Z,Li Y Y.Acta Metall Sin, 2003;39:242 (兰勇军,黄成江,李■中,李依依.金属学报,2003;39:242) |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|