Abstract A mathematical model was developed to describe the inclusion dynamic growth process in the continuous casting mold. This model includes Eulerian method to predict turbulent flow and inclusion distribution in the continuous casting mold, and Lagrangian method to trace single inclusion in the inclusion concentration field and to study its collision and aggregation. Numerical results show that fluid flow is the key factor to affect inclusion’s distribution. In the continuous caster, the liquid steel and the inclusions have the upper and lower recirculation, and have “W” distribution at the exit. For the single inclusion, the seed inclusions can grasp the other inclusions continuously, thus, the bigger inclusions are dendritic with some tips and arms.
|
Received: 05 November 2007
|
|
[1]Zhang L.Steel Res lnt,2005;76:784 [2]Lei H,Zhu M Y,He J C.J Iron Steel Res lnt,2003:10(2): 21 [3]Aboutalebi M R,Hasan M,Guthrie R I L.Metall Mater Trans,1995;26B:731 [4]Miki Y,Shimada Y,Thomas B G,Denissov A.Iron Steel- maker,1997;24(8):31 [5]Zhang B W,Deng K,Lci Z S,Ren Z M.Acta Metall Sin, 2004;40:623 (张邦文,邓康,雷作胜,任忠鸣.金属学报,2004:40:623) [6]Zhang L,Taniguchi S,Cai K.Metall Mater Trans,2000; 31B:253 [7]Nakanishi K,Szekely J.Trans ISIJ,1975;15:522 [8]Javurek M,Gittlcr P,Rossler R,Kaufmann B,Prcblinger H.Steel Res lnt,2005;76:64 [9]Sinha A K,Sahai Y.ISIJ lnt,1993;33:556 [10]Wang L T,Peng S H,Zhang Q Y,Li Z B.Steel Res Int, 2006;77:25 [11]Zhao L G,Liu K.J Res Iron Steel,2002:14(6):19 (赵连刚,刘坤.钢铁研究学报,2002;14(6):19) [12]Lei H,Wang L,Wu Z,Fan J.ISIJ lnt,2002;42:717 [13]Launder B E,Spalding D B.Comput Meth Appl Meeh En9,1974;15:269 [14]O′Rourke P J.PhD Thesis,Princeton University,New.Jer- sey,USA,1981 [15]Taniguchi S,Kikuchi A,Ise T,Shoji N.ISIJ Int.1996;36 (Suppl.):117 [16]Thomas B G,Mika L J,Najjar F M.Metall Trans,1990; 21B:387 [17]Thomas B G,Huang X,Sussman R C.Metall Mater Trans,1994;25B:527 [18]Bouris D,Bergeles G.Metall Mater Trans,1998;29B:641 [19]Lei H,Jin Y,Zhu M,He J.J Mater Sei Technol,2002;18: 403 [20]Lu L F,Lu S P,Zhou S Q,Ren Q,Li D,Kang R M,Wu W D.J Chongqing Univ,2006;29(2):72 (刘林飞,刘守平,周土祺,任勤,李丁,康人木,吴文东.重庆大学学报,2006;29(2):72) [21]Yin H,Shibata H,Emi T,Suzuki M.ISIJ lnt,1997;37: 936 [22]Kimura S,Nabeshima Y,Nakajima K,Mizoguchi S.Metall Mater Trans,2000;31B:1013 |
No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|