| FABRICATION OF Zr41.25Ti13.75Ni10Cu12.5Be22.5 BULK METALLIC GLASS FOAM |
| QIU K Q |
| 沈阳工业大学材料科学与工程学院 |
|
Cite this article:
QIU K Q. FABRICATION OF Zr41.25Ti13.75Ni10Cu12.5Be22.5 BULK METALLIC GLASS FOAM. Acta Metall Sin, 2006, 42(4): 379-382 .
|
|
|
Abstract A bulk metallic glass foam with a diameter of 8.1 mm and a length of 70 mm was fabricated by infiltrating Zr-based liquid metal into NaCl powder as a pattern in a few seconds and water quenching the pattern. Both the powders and the prealloyed charges were sealed in a U-turn quartz tube as a crucible and heated in two different temperature regions respectively in the electric resistance furnace. The sample fabricated is the largest in diameter up to now according to the literature. The X-ray diffraction and the scanning electron microscopy were used to check the amorphous nature and structure of the porous samples. The results show that the samples are consisted of amorphous phase and have good connectivity among the cells in the foam. The sizes of struts and the holes are largely smaller than 1mm. The density and porosity of the open-cellular bulk metallic glass are 3.63g/cm3 and 40.5% respectively. Porous bulk metallic glass is the most potential materials that will be used as biologic-transplant materials.
|
|
Received: 21 July 2005
|
|
|
[1] Pan M X, Wang W H. Physics, 2002; 31: 453 (潘明祥,汪卫华.物理,2002;31:453) [2] http://www.liquidmetal.com/applications/ [3] Qiu K Q, Wang A M, Zhang H F, Ding B Z, Hu Z Q. Intermetallica, 2002; 10: 1283 [4] Qiu K Q, Wu X F, Wang A M, Zhang H F, Hu Z Q. Metall Mater Trans, 2003; 34A: 1147 [5] Schroers J, Veazey C, Johnson W L. Appl Phys Lett, 2003; 82: 370 [6] Brothers A H, Dunand D C. Appl Phys Lett, 2004; 84: 1108 [7] Apfel R E, Qiu N. J Mater Res, 1996; 11: 2916 [8] Wada T, Inoue A. Mater Trans, 2004; 45: 2761 [9] Wada T, Inoue A. Mater Trans, 2003; 44: 2228 [10] Brothers A H, Scheunemann R, DeFouw J D, Dunand D C. Scr Mater, 2005; 52: 33 [11] Peker A, Johnson W L. Appl Phys Lett, 1993; 63: 2342 [12] Conner R D, Johnson W L, Paton N E, Nix W D. J Appl Phys, 2003; 94: 904 [13] Liu P S. Introduction to Cellular Materials. Beijing: Tsinghua University Press, 2004: 300 (刘培生.多孔材料引论.北京:清华大学出版社,2004:300) [14] Conner R D, Dandliker R B, Johnson W L. Acta Mater, 1998; 46: 6089 [15] Marchi S C, Brothers A H, Dunand D C. Mater Res Soc Symp Proc, 2003; 754: CC1.8.1 [16] Qiu K Q. PhD Dissertation, Institute of Metal Research, The Chinese Academy of Sciences, Shenyang, 2002 (邱克强.中国科学院金属研究所博士学位论文,沈阳,2002) [17] Dandliker R B, Conner R D, Johnson W L, J Mater Res, 1998; 13: 2896 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|