| Research Progress in Precipitation Crystallography models |
| Dong Qiu;Wenzheng Zhang |
| 清华大学材料系 |
|
Cite this article:
Dong Qiu; Wenzheng Zhang. Research Progress in Precipitation Crystallography models. Acta Metall Sin, 2006, 42(4): 341-349 .
|
|
|
Abstract In-depth understanding of precipitation crystallography is very essential to the control of microstructure in many multi-phases materials. The present paper reviews the recent development of various crystallographic models. Each model was reviewed in terms of its hypothesis, applicable scope, basic idea, and especially its limitation. According to the comparison and contrast between different models, it is proposed that combining the O-line model and Near Coincidence Sites model may provide a more powerful tool to interpret the precipitation crystallography and morphology.
|
|
Received: 10 August 2005
|
|
|
[1] Potter D A, Easterling K E. Phase Transformations in Metals and Alloys. 2nd edition, London: Chapman and Hall, 1992: 305 [2] Bollmann W. Crystal Defects and Crystalline Interfaces. Berlin: Springer, 1970: 55 [3] Bonnet R, Durnad F. In: Proc Conf on In situ Composite, Lakeville, USA: NMAB 308-1, 1973: 209 [4] Dahmen U. Scr Metall, 1981; 15: 77 [5] Dahmen U. Acta Metall, 1982; 30: 63 [6] Ameyama K, Weatherly G C, Aust K T. Acta Metall Mater, 1992; 40: 1835 [7] Dahmen U, Ferguson P, Westmacott K H. Acta Metall, 1984; 32: 803 [8] Fujii T, Mori T, Kato M. Acta Metall Mater, 1992; 40: 3413 [9] Weatherly G C, Humble P, Borland D. Acta Metall, 1979; 27: 1815 [10] Luo C P, Dahmen U, Westmacott K H. Acta Metall Mater, 1994; 42: 1923 [11] Luo C P, Weatherly G C. Philos Mag, 1988; 58A: 445 [12] Lang J M, Dahmen U, Wstmacott K H. Phys State Soc, 1983; 75: 409 [13] Viswanadham R K, Wert C A. J Less-Common Met, 1976; 18: 135 [14] Diercks D R, Wert C A. Metall Trans, 1972; 3: 1699 [15] Jack K H. Iron Steel Inst, 1951; 169: 26 [16] Kato M. Mater Sci Eng, 1991; A146: 205 [17] Xiao S Q, Howe J M. Acta Mater, 2000; 48: 3253 [18] Luo C P, Weatherly G C. Acta Metall, 1987; 35: 1963 [19] Howell P R, Southwick P D, Honeycombe R W K. J Mi- crosc, 1979; 116: 151 [20] Hall M G, Aaronson H I. Acta Metall, 1986; 34: 1409 [21] Zhang W Z, Purely G R. Acta Metall Mater, 1993; 41: 543 [22] Zhang W Z, Purely G R. Philos Mag, 1993; 68A: 279 [23] Zhang W Z, Purely G R. Philos Mag, 1993, 68A: 291 [24] Smith D A, Hazzledine P M. Scr Metall, 1981; 15: 393 [25] Qiu D, Zhang W Z. Philos Mag, 2003; 83: 3093 [26] Weatherly G C, Zhang W Z. Metall Mater Trans, 1994; 25A: 1865 [27] Ye F, Zhang W Z, Qiu D. Acta Mater, 2004; 52: 2249 [28] Knowles K M, Smith D A. Acta Crystallogr, 1982; A38: 34 [29] Bilby B A, Bullough R, de Grinberg D K. Discuss Faraday Soc, 1964; 38: 61 [30] Bollmann W, Nissen H U. Acta Crystallogr, 1968; A24: 546 [31] Ecob R C, Ralph B. Acta Metall, 1981; 29: 1037 [32] Hall M G, Aaronson H I, Kinsma K R. Surf Sci, 1972; 31: 257 [33] Rigsbee J M, Aaronson H I. Acta Metall, 1979; 27: 351 [34] Russell K C, Hall M G, Kinsma K R, Aaronson H I. Metall Trans, 1974; 5: 1503 [35] Furuhara T, Aaronson H I. Acta Metall Mater, 1991; 39: 2857-2872 [36] Liang Q, Reynolds W T Jr. Metall Mater Trans, 1998; 29A: 2059 [37] Miyano N, Ameyama K, Weatherly G C. IS1J Int, 2000; 40: S199 [38] Hall M G, Furuhara T, Aaronson H I, Hirth J P. Acta Mater, 2001; 49: 3487 [39] Miyano N, Ameyama K, Weatherly G C. Mater Sci Eng, 2002; A333: 85 [40] Miyano N, Ameyama K, Weatherly G C. Mater Trans, 2002; 43: 1547 [41] Reynolds W T Jr, Nie J F, Zhang W Z, Howe J M, Aaronson H I, Purdy G R. Scr Mater, 2003; 49: 405 [42] Frank F C. Acta Metall, 1953; 1: 15 [43] Fecht H J. Acta Metall Mater, 1992; 40: S39 [44] Shiflet G J, van der Merwe J H. Metall Mater Trans, 1994; 25A: 1895 [45] Howe J M. Interfaces in Materials. New York: John Wiley and Sons, 1997: 299 [46] Howe J M. Mater Trans JIM, 1998; 39: 3 [47] Kelly P M, Zhang M X. Mater Forum, 1999; 23: 41 [48] Zhang M X, Kelly P M. Acta Mater, 2005; 53: 1073 [49] Zhang M X, Kelly P M. Acta Mater, 2005; 53: 1085 [50] Savva G C, Kirkaldy J S, Weatherly G C. Philos Mag, 1997; 75A: 315 [51] Pond R C. In: Nabarro F R N ed., Dislocations in Solids, Amsterdam: North-Holland, 1989: 38 [52] Pond R C, Celotto S, Hirth J P. Acta Mater, 2003; 51: 5385 [53] Ye F. Ph.D Thesis. Beijing: Tsinghua University, 2004 (叶 飞.清华大学博士学位论文,北京, 2004)% |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|