| EFFECT OF REINFORCEMENT PARTICLE ON GROWTH OF MICROARC OXIDATION FILM ON ALUMINUM MATRIX COMPOSITE |
| WenBin Xue |
| 北京师范大学低能核物理研究所射线束材料改性开放实验室 |
|
Cite this article:
WenBin Xue. EFFECT OF REINFORCEMENT PARTICLE ON GROWTH OF MICROARC OXIDATION FILM ON ALUMINUM MATRIX COMPOSITE. Acta Metall Sin, 2006, 42(4): 350-354 .
|
|
|
Abstract A thick ceramic film on SiC/2024 aluminum matrix composite was fabricated by plasma microarc discharge method. The growing curve of film was determined, and the morphology and phase composition of film were analyzed by scanning electron microscopy and X-ray diffraction. The morphology and distribution of reinforcement particles were emphatically observed, and then a growth model of microarc oxidation film on metal matrix composites was proposed. Under microarc discharge sintering, most SiC reinforcement particles have been oxidized, but only a few residual SiC particles still remain in the film close to the composite/film interface. Although the SiC particles hinder the film growth, the continuity of film has not been disrupted. That is completely different from conventional anodizing on metal matrix composites.
|
|
Received: 26 July 2005
|
|
|
[1] Yue T M, Wu Y X, Man H C. Surf Coat Technol, 1999; 114: 13 [2] Greene H J, Mansfeld F. Corrosion, 1997; 53: 920 [3] Yu X W, Cao C N, Lin H C, Zhou Y H, Zhou D R, Yin Z D. Acta Phys-Chem Sin, 2000; 16: 547 (于兴文,曹楚南,林海潮,周育红,周德瑞,尹钟大.物理化 学学报,2000;16:547) [4] Belevantsev V I, Terleeva O P, Markov G A, Shulepko E K, Slonova A I, Utkin V V. Prot Met, 1998; 34: 416 [5] Xue W B, Deng Z W, Lai Y C, Chen R Y. J Am Ceram Soc, 1998; 81: 1365 [6] Yao Z P, Jiang Z H, Sun X T, Xin S G, Li Y P. Thin Solid Films, 2004; 468: 120 [7] Xue W B, Wang C, Chen R Y, Deng Z W. Mater Lett, 2002; 52: 435 [8] Jiang B L, Zhang X-F, Zhu J. Heat Treat Met, 2004; 29: 23 (蒋百灵,张先锋,朱 静.金属热处理, 2004;29:23) [9] Nie X, Meletis E I, Jiang J C, Leyland A, Yerokhin A L, Matthews A. Surf Coat Technol, 2002; 149: 245 [10] Xue W B, Deng Z W, Chen R Y, Zhang T H. Ada Metall Sin, 1999; 35: 638 (薛文斌,邓志威,陈如意,张通和.金属学报,1999;35:638) [11] Wang Y K, Xiong R Z, Sheng L, Li B S. Ordnance Mater Sci Eng, 1998; 21(4): 25 (王永康,熊仁章,盛磊,李炳生.兵器材料科学与工程,1998; 21(4):25) [12] Jin L, Yang Z, Li G H, Ma Y H, Li J P. Ordnance Mater Sci Eng, 2003; 26(3): 31 (金 玲,扬 忠,李高宏,马玉韩,李建平.兵器材料科学与 工程,2003;26(3):31) [13] Xue W B, Wang C, Li Y, Chen R Y, Zhang T H. ISIJ Int, 2002; 42: 1273 [14] Xue W B, Deng Z W, Chen R Y, Zhang T H. Thin Solid Films, 2000, 372: 114 [15] Shahid M. J Mater Sci, 1997; 32: 3775 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|