| Hot deformation and processing map of GH2674 superalloy |
| Quan Ju;; |
| 北京科技大学材料科学与工程学院 |
|
Cite this article:
Quan Ju. Hot deformation and processing map of GH2674 superalloy. Acta Metall Sin, 2006, 42(2): 218-224 .
|
|
|
Abstract The hot deformation behavior of GH2674 has been studied in the temperature range 950-1200℃ and strain rate range 0.001-10 s-1, using hot compressing testing on a Gleeble-1500 simulator. A processing map is developed on the basis of these data and using the principles of dynamic material modeling. The map exhibits two domains: one at 1050℃ and 0.01 s-1, with a peak efficiency of power dissipation of 38%, the second at 1150℃ and 10s-1, with a peak efficiency of 40%. On the basis of optical microscopic observations, these they are interpreted to represent two dynamic recrystallization(DRX) domains, of which the mechanisms are different. The map also exhibits a long concave band in the temperature range 1075-1100℃,which may be related to the solutionizing of M3B2 phase. At temperatures lower than 1000℃ and strain rates higher than 0.1s-1, the material may be subjected to potential instabilities, while at temperatures higher than 1050℃ and strain rates lower than 0.01s-1 , the material exhibits significant grain coarsening, furthermore, the wedge cracking would appear at 1200℃ and 0.001s-1. On the basis of the constitutive behavior of GH2674 alloy as revealed in the processing map, the hot working schedules have been designed primarily
|
|
Received: 24 May 2005
|
|
|
[1] The Editorial Committee of China Aeronautical Materials Handbook. China Aeronautical Materials Handbook. Beijing: Standards Press of China, 2002: 93 (《中国航空材料手册》编辑委员会.中国航空材料手册.北京:中国标准出版社,2002:93) [2] Rao K P, Doraivelu S M, Roshan H M, Prasad Y V R K.Metall Trans, 1983; 14A: 1671 [3] Prasad Y V R K, Gegel H L, Doraivelu S M, Malas J C,Morgan K A, Barker D R. Metall Trans, 1984; 15A: 1883 [4] Prasad Y V R K, Sasidhara S. Hot Working Guide: A Compendium of Processing Maps. Materials Park, OH:ASM International, 1997: 1 [5] Wang L Y, Fan Y G, Huang G J, Huang G S. Chin J Nonferrous Met, 2004; 14: 1068 (汪凌云,范永革,黄光杰,黄光胜.中国有色金属学报,2004;14: 1068) [6] Gao S. PhD Thesis, Northeaster University, Shenyang,1997 (高珊.东北大学博士学位论文,沈阳, 1997) [7] Prasad Y V R K, Seshacharyulu T. Int Mater Rev, 1998;43: 243 [8] Prasad Y V R K.J Mater Eng Perfor, 2003; 12: 638 [9] Ziegler H. In: Sneddon I N, Hill R, eds., Progress in Solid Mechanics, Amsterdam: North-Holland Publishing, 1965: 91 [10] Somani M C, Muraleedaran K, Prasad Y V R K, Singh V. Mater Sci Eng, 1998; A245: 88 [11] Superalloy Division of University of Science and Technology Beijing. GH132 Alloy. Beijing: National Defence Press, 1980: 150 (北京科技大学高温合金教研室,GH132合金.北京:国防科技出版社,1980:150) [12] Medeiros S C, Prasad Y V R K, Frazier W G, Srinivasan R. Mater Sci Eng, 2000; A293: 198U |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|