| COUPLED NUMBERICAL SIMULATION ON SOLIDIFICATION AND SOLUTE TRANSPORT IN THIN SLAB CONTINUOUS CASTING PROCESS |
| 沈阳 |
|
Cite this article:
. COUPLED NUMBERICAL SIMULATION ON SOLIDIFICATION AND SOLUTE TRANSPORT IN THIN SLAB CONTINUOUS CASTING PROCESS. Acta Metall Sin, 2006, 42(2): 211-217 .
|
|
|
Abstract Based on the control-volume method a 3-D comprehensively coupled model has been developed for binary iron-carbon to describe the turbulent fluid flow, heat transfer, solidification, and solute redistribution in the thin slab continuous casting process. The calculated results show that the turbulent fluid flow dramatically alters the shape of the isotherms and the distribution of the solute in the thin slab. The thickness of solidified shell is uneven along broad face because of the flow jet. The formation mechanism of macrosegregation is investigated and the possible position of the macrosegregation is analyzed.
|
|
Received: 20 November 2005
|
|
|
[1] Tian N Y. Continuous Casting and Hot-roll of Thin Slab. Beijing: Metallurgical Industry Press, 1998: 3 (田乃媛,薄板坯连铸连轧.北京:冶金工业出版社.1998; 3) [2] Asai S, Szekely J. Ironmaking Steelmaking, 1975; 3: 205 [3] Thomas B G, Mika L J, Najjar F M. Metall Trans, 1990;21B: 387 [4] Huang X, Thomas B G, Najjar F M. Metall Trans, 1992;23B: 339 [5] Aboutalebi M R, Hasan M, Guthrie R I L. Metall Mater Trans, 1995; 26B: 731 [6] Flint P J. In: Spalding D B, ed., Proc 73rd Steelmaking Conf, Warrendale, PA: Iron and Steel Society, 1990: 481 [7] Zhu M Y, Sawada I. Ada Metall Sin, 1997; 33: 11 (朱苗勇,迟田郁夫.金属学报,1997; 33: 11) [8] Yang B J, Su J Y. Iron Steel, 1996; 31: 24 (杨秉俭,苏俊义.钢铁,1996; 31: 24) [9] Zhang H W, Wang E G, He J C. Ada Metall Sin, 2002;38: 99 (张红伟,王恩刚,赫冀成.金属学报,2002; 38: 99) [10] Yang H L, Zhao L G, Zhang X Z, Deng K W, Li W C,Gan Y. Metall Mater Trans, 1998; 29B: 1345 [11] Bao Y P, Zhu J Q, Jiang W, Zhang T, Tian N Y, Xu B M. J Univ Sd Technol Beijing, 2000; 24: 409 (包燕平,朱建强,蒋伟,张涛 ,田乃媛,徐宝美.北京科技大学学报,2000;24:409) [12] Yu H X, Zhang J M, Wang W J, Wang X H, Yang Z Y, Yang L X. J Univ Sd Technol Beijing, 2002; 26: 492 (于会香,张炯明,王万军,杨振亚,杨立新.北京科技大学学报,2002; 26:492) [13] Honeyands T, Herbertson J. Steel Res, 1995; 66(7): 287 [14] O'Connor T G, Dantzig J A. Metall Mater Trans, 1994;25B: 443 [15] Nam H, Park H S, Yoon J K. ISIJ Int, 2000; 40: 886 [16] Park H S, Nam H, Yoon J K. ISIJ Int, 2001; 41: 974 [17] Launder B E, Spalding D B. Comp Mater Appl Mech Eng,1974; 3: 269 [18] Carmon P C. Trans Ins Chem Eng, 1937; 15: 150 [19] Bennon W D, Incropera F P. Int J Heat Mass Trans, 1987;30: 2161 [20] Tao W Q. Numerical Heat Transfer. Xi'an: Xi'an Jiaotong University Press, 1988: 349 (陶文铨.数值传热学.西安:西安交通大学, 1988:349) [21] Patankar S V, translated by Zhang Z. Numberial Heat Transfer and Fluid Flow. Beijing: Science Press, 1984:131 (Patankar S V 著,张政译.传热与热体流动的数值计算.北京:科学出版社,1984:131) [22] Offerman C. Scand J Metall, 1981; 10: 25h |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|