PLS Method Applied to Analysis of Binary Laves Phase Structures
JIANG Weiqing; HUANG Cunke; HUANG Dan; JIAN Xiaoling; GUO Jin
College of Physics Science and Technology; Guangxi University; Nanning 530004
Cite this article: 

JIANG Weiqing; HUANG Cunke; HUANG Dan; JIAN Xiaoling; GUO Jin. PLS Method Applied to Analysis of Binary Laves Phase Structures. Acta Metall Sin, 2005, 41(1): 19-.

Download:  PDF(149KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The AB2 type Laves phases with cubic MgCu2 and hexagonal MgZn2 structures are investigated by partial least square (PLS) method and some criteria for classification of the two structures of Laves phases are obtained. It is found that for nontransition-transition and transition-transition alloys the valence electron densities of component elements are significant in influencing their Laves phase structures, and for transition-lanthanide (actinides) alloys the valence electron density of the atom at B position is the most important factor influencing their Laves phase structures. Besides, the effects of both valence charge and atomic radius on Laves phase structures are in opposition to each other in transition-lanthanide (actinides) alloys.
Key words:  Laves phase      partial least square method (PLS)      
Received:  09 February 2004     
ZTFLH:  TG111.5  

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2005/V41/I1/19

[1] Ansara I, Chart T G, Guillermet A F, Hayes F H, KattnerU R. CALPHAD, 1997; 21: 171
[2] Liu C T, Zhu J H, Brady M P, McKamey G G, Pike L M.Intermetallics, 2000; 8:1119
[3] Yoshida M, Ishibashi H, Susa K, Ogura T, Akiba E. JAlloys Compd, 1995; 226: 161
[4] Xu Y H, Chen C P, Wang X L, Lei Y Q, Wang Q D. JAlloys Compd, 2002; 337: 214
[5] Liu B H, Li Z P, Kitani R, Suda S. J Alloys Compd, 2002;330-332: 825
[6] Shu K Y, Zhang S K, Lei Y Q, Lu G L, Wang Q D. JAlloys Compd, 2003; 349: 237
[7] Iwakura C, Kasuga H, Kim I, Inoue H, Matsuoka M. Elec-trochim Acta, 1996; 41:2691
[8] Du Y L, Yang X G, Zhang Q A, Lei Y Q, Zhang M S. IntJ Hydrogen Energy, 2001; 26: 333
[9] Okada M, Kuriiwa T, Kamegawa A, Takamura H. MaterSci Eng, 2002; 329-331A: 305
[10] Stein F, Palm M, Sauthoff G. Intermetallics, 2004; 12:713
[11] Zhu J H, Liu C T, Pike L M, Liaw P K. Intermetallics,2002; 10: 579
[12] Chen N Y, Li C H, Yao S W, Wang X Y. J Alloys Compd,1996; 234: 130
[13] Yao S W, Li C H, Qin P, Chen N Y. Comp Appl Chem,1997; 14(1): 75(姚树文,李重河,钦佩,陈念贻.计算机与应用化学,1997;14(1):75)
[14] Hoskuldsson A. J Chemometrics, 1988; 2: 211_
[1] WEN Donghui, JIANG Beibei, WANG Qing, LI Xiangwei, ZHANG Peng, ZHANG Shuyan. Microstructure Evolution at Elevated Temperature and Mechanical Properties of MoNb-Modified FeCrAl Stainless Steel[J]. 金属学报, 2022, 58(7): 883-894.
[2] CHEN Jianjun, DING Yutian, WANG Kun, YAN Kang, MA Yuanjun, WANG Xingmao, ZHOU Shengming. Effects of Laves Phase on Burst Behavior of GH3625 Superalloy Pipe During Hot Extrusion[J]. 金属学报, 2021, 57(5): 641-650.
[3] WU Yun, LIU Yahui, KANG Maodong, GAO Haiyan, WANG Jun, SUN Baode. Microstructure Evolution of K4169 Alloy During Cyclic Loading[J]. 金属学报, 2020, 56(9): 1185-1194.
[4] Gaowu QIN, Hongbo XIE, Hucheng PAN, Yuping REN. A New Class of Ordered Structure Between Crystals and Quasicrystals[J]. 金属学报, 2018, 54(11): 1490-1502.
[5] Zhenliang LI,Fei LIU,Aiping YUAN,Baoyu DUAN,Xiaowei LI,Yiming LI. EFFECTS OF ROLLING DEFORMATION ON TEXTURE AND LPSO PHASE OF SPRAY-DEPOSITED MAGNESIUM ALLOYS CONTAINING Nd[J]. 金属学报, 2016, 52(8): 938-944.
[6] Kejian LI,Zhipeng CAI,Yifei LI,Jiluan PAN. EVOLUTION BEHAVIOR OF LAVES PHASE IN FB2 MARTENSITIC STAINLESS STEEL DURING WELDING[J]. 金属学报, 2016, 52(6): 641-648.
[7] MA Ping, WU Erdong, LI Wuhui, SUN Kai, CHEN Dongfeng. MICROSTRUCTURES AND HYDROGEN STORAGE PROPERTIES OF Ti0.7Zr0.3(Cr1-xVx)2 ALLOYS[J]. 金属学报, 2014, 50(4): 454-462.
[8] WANG Xue, YU Shumin, REN Yaoyao, LIU Hong, LIU Hongwei, HU Lei. LAVES PHASE EVOLUTION IN P92 STEEL DURING AGEING[J]. 金属学报, 2014, 50(10): 1195-1202.
[9] WANG Xue, LI Yong, REN Yaoyao, LIU Hongwei, LIU Hong, WANG Wei. EFFECT OF LAVES PHASE PRECIPITATION ON REDISTRIBUTION OF ALLOYING ELEMENTS IN P92 STEEL[J]. 金属学报, 2014, 50(10): 1203-1209.
[10] ZHANG Maicang, CAO Guoxin, DONG Jianxin, ZHENG Lei, YAO Zhihao. INVESTIGATIONS ON DISSOLUTION MECHANISM OF LAVES PHASE IN GH4169 ALLOY INGOT BASED ON CLASSICAL DYNAMICAL MODEL[J]. 金属学报, 2013, 49(3): 372-378.
[11] SHENG Liyuan, ZHANG Wei, LAI Chen, GUO Jianting,XI Tingfei, YE Hengqiang. MICROSTRUCTURE AND MECHANICAL PROPERTIES OF LAVES PHASE STRENGTHENING NiAl BASE COMPOSITE FABRICATED BY RAPID SOLIDIFICATION[J]. 金属学报, 2013, 49(11): 1318-1324.
[12] PAN Zhiping, LI Shuangming, XU Lei, FU Hengzhi. THREE-DIMENSIONAL DENDRITIC PATTERN OF PRIMARY LAVES PHASE Cu2Mg IN DIRECTIONAL SOLIDIFICATION OF Cu-10.25 %Mg HYPEREUTECTIC ALLOY[J]. 金属学报, 2013, 49(1): 92-100.
[13] LI Xiaocheng DING Yutian HU Yong. MICROSTRUCTURE AND MAGNETOSTRICTION OF THE Tb0.3Dy0.7Fe1.95-xTix (x=0, 0.03, 0.06, 0.09) ALLOYS[J]. 金属学报, 2012, 48(1): 11-15.
[14] PENG Zhifang CAI Lisheng PENG Fangfang HU Yongping CHEN Fangyu. STUDY ON THE MULTI–SEGMENT FEATURE OF 625 ℃ CREEP–RUPTURE PROPERTY AND THE QUATITATIVE CHANGE OF PHASE PARAMETERS OF M23C6 AND LAVES PHASES IN EACH SEGMENT OF P92 STEEL[J]. 金属学报, 2010, 46(4): 429-434.
[15] WU Erdong GUO Xiumei SUN Kai. NEUTRON DIFFRACTION STUDY OF DEUTERIUM OCCUPANCY OF DEUTERIDE OF LAVES PHASE ALLOY Ti0.68Zr0.32MnCrD3.0[J]. 金属学报, 2009, 45(5): 513-518.
No Suggested Reading articles found!