| STUDY ON THE MULTI–SEGMENT FEATURE OF 625 ℃ CREEP–RUPTURE PROPERTY AND THE QUATITATIVE CHANGE OF PHASE PARAMETERS OF M23C6 AND LAVES PHASES IN EACH SEGMENT OF P92 STEEL |
| PENG Zhifang 1; CAI Lisheng 1; PENG Fangfang 2; HU Yongping 3; CHEN Fangyu 4 |
1. School of Power and Mechanical Engineering; Wuhan University; Wuhan 430072
2. Materials Research Department; Dong Fang Boiler Group Corp. Ltd.; Zigong 643001
3. Special Steels Plant; Inner Mongolia North Heavy Industries Group Corp. Ltd.; Baotou 014033
4. Research Institute of Wuhan Iron and Steel Company Ltd.; Wuhan 430080 |
|
Cite this article:
PENG Zhifang CAI Lisheng PENG Fangfang HU Yongping CHEN Fangyu. STUDY ON THE MULTI–SEGMENT FEATURE OF 625 ℃ CREEP–RUPTURE PROPERTY AND THE QUATITATIVE CHANGE OF PHASE PARAMETERS OF M23C6 AND LAVES PHASES IN EACH SEGMENT OF P92 STEEL. Acta Metall Sin, 2010, 46(4): 429-434.
|
|
|
Abstract In the present study, the multi–segment feature of stress vs rupture–time plot and the corresponding quatitative change of phase parameters of M23C6 and Laves in each segment were investigated for P92 steel samples subjected to 625 ℃ creep–rupture tests. The results indicate that the stress vs rupture–time plot obtained from the test results can be divided into two segments (higher stress level and shorter rupture time segment: 180—150 MPa/30—454 h, and lower stress level and longer rupture time segment: 140—110 MPa/2881—10122 h) respectively, and the microstructural evolution is closely related to the feature of each segment. In the higher stress level and shorter rupture time segment the M23C6 particles are coarsened, while in the lower stress level and longer rupture time segment both M23C6 and Laves phases are coarsened, but the latter is predominantly. The average composition, the amount and the elemental partitioning of each alloy phase called phase parameters can be determined by a multiphase separation method developed.
|
|
Received: 27 September 2009
|
| Fund: Supported by National Natural Science Foundation of China (No.50674072) and Scientific Research Project of Dong Fang Boiler Group Corp. Ltd., 2009 |
| [1] Yang F. In: Chinese Society for Electrical Engineering, ed., Smposium on Sinicization of New Type Steels for 600MW/1000MW Ultra–Supercritical Units, Yang Zhou: China Electric Power Journal Net, 2009: 1
(杨富. 见: 中国电机工程学会主编, 600MW/1000MW超超临界机组新型钢国产化研讨会报告文集, 扬州: 中国电力期刊网, 2009: 1)
[2] Armaki H G, Maruyama K, Yoshizawa M, Igarashi M. Mater Sci Eng, 2008; A490: 66
[3] Maruyama K, Yoshimi K. J Press Vess Technol, 2007; 129:449
[4] Maruyama K, Lee J S, In: Shibli I A, Holdworth S R eds., Creep & Fracture in High Temperature Components–Design & Life Assessment Issues, Lancaster: DEStech Publications, 2005: 372
[5] Lee J S, Armaki H G, Maruyama K, Muraki T, Asahi H. Mater Sci Eng, 2006; A428: 270
[6] Peng Z F, Yang Z G, Yan G Z, Chen S G, Zhou Y G. In: Academic Committee of the Superalloys, CSM ed., High–Temperature Structural Materials for Power and Eergy Resource—Proceedings of 11th Annual Chinese Conference on Sueralloys, Shanghai: Metallurgical Industry Press, 2007: 666
(彭志方, 杨志刚, 阎光宗, 陈盛广, 周元贵. 见: 中国金属学会高温材料分会主编, 动力与能源用高温结构材料---第11届中国高温合金年会论文集, 上海: 冶金工业出版社, 2007: 666)
[7] Peng F F, Peng Z F, Chen F Y. In: Chinese Society for Electrical Engineering ed. Symposium on Sinicization of New Type Steels for 600MW/10MW Ultra–Supercritical Units, Yang Zhou: China Electric Power Journal Net, 2009: 178
(彭芳芳, 彭志方, 陈方玉. 见: 中国电机工程学会主编, 600MW/1000MW超超临界机组新型钢国产化研讨会报告文集, 扬州: 中国电力期刊网, 2009: 178)
[8] Peng Z F, Peng F F, Chen F Y. Electric Power Construction, 2009; 30(12): 1
(彭志方, 彭芳芳, 陈方玉. 电力建设, 2009; 30(12): 1)
[9] Peng Z F, Dang Y Y, Peng F F. Acta Metall Sin, 2010;46: 435
(彭志方, 党莹樱, 彭芳芳. 金属学报, 2010, 46: 435)
[10] Robertson D G. ECCC Data Sheets 2005. http://www.ommi. co. uk/etd/eccc/ advanced creep/index.htm
[11] Kuai C G, Peng Z F. Acta Metall Sin, 2008; 44: 897
(蒯春光, 彭志方. 金属学报, 2008; 44: 897)
[12] Maruyama K, Sawada K, Koike J. ISIJ Int, 2001; 41: 641
[13] Abe F. Sci Technol Adv Mater, 2008; 9: 15 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|