| MARTENSITIC TWINS REORIENTATION AND STRESS-STRAIN BEHAVIOR OF FERROMAGNETIC SHAPE MEMORY ALLOYS Ni-Mn-Ga SINGLE CRYSTALS |
| DENG Lifen; LI Yan; JIANG Chengbao; XU Huibin |
| School of Materials Science and Engineering; Beijing University of Aeronautics and Astronautics; Beijing 100083 |
|
Cite this article:
DENG Lifen; LI Yan; JIANG Chengbao; XU Huibin. MARTENSITIC TWINS REORIENTATION AND STRESS-STRAIN BEHAVIOR OF FERROMAGNETIC SHAPE MEMORY ALLOYS Ni-Mn-Ga SINGLE CRYSTALS. Acta Metall Sin, 2004, 40(12): 1290-1294 .
|
|
|
Abstract Ferromagnetic shape memory alloys Ni53Mn23.5Ga23.5,
Ni54Mn23Ga23 and Ni50Mn27-Ga23 single
crystals were prepared by zone-melting unidirectional solidification.
The orientations of the cut single crystals were determined by X-ray
diffraction method. The Ni-Mn-Ga crystal growth direction is along
[100] with the deviation less than 5 circ. The martensitic twins
reorientation process was detected by the stress-strain curves. The
compression experiments along different directions were performed,
respectively. The results show that the compression improves the
texture of favorable martensitic variants and turns them into a single
martensitic variant by martensite reorientation.
|
|
Received: 08 May 2004
|
|
|
[1] Webster P J, Ziebeck K R A, Town S L, Peak M S. PhilosMag, 1984; 49B: 295 [2] Ullakko K, Huang J K, Kokorin V V, O' Handley R C.Scr Mater, 1997; 36: 1133 [3] Jiang B H, Zhou W M, Liu Y, Qi X. Mater Sci Forum,2003; 426-432: 2285 [4] Gao Z Y, Cai W, Zhao L G, Wu G H, Chen J L, Zhan WS. Trans Nonferrous Met Soc Chin, 2003; 13(1):42 [5] Murray S J, Marioni M, Allen S M, O' Handley R C. ApplPhys Lett, 2000; 77: 886 [6] Sozinov A, Likhachev A A, Lanska N, Ullakko K. ApplPhys Lett, 2002; 80: 1746 [7] Wu G H, Wang W H, Chen J L, Ao L, Liu Z H, Zhan WS. Appl Phys Lett, 2002; 80: 634 [8] O'Handley R C. J Appl Phys, 1998; 83: 3263 [9] Sozinov A, Likhachev A A, Ullakko K. IEEE Trans Magn,2002; 38: 2814 [10] Murray S J, O'Handley R C, Allen S M. J Appl Phys,2001; 89: 1295 [11] Jiang C B, Feng G, Xu H B. Appl Phys Lett, 2002; 80:1619 [12] Liu Z H, Wu G H, Wang W H, Chen J L, Ao L. Acta PhysSin, 2002; 51: 640 (柳祝红,吴光恒,王文洪,陈京兰,敖玲.物理学报,2002: 51:640) [13] Pons J, Chernenko V A, Santamarta R, Cesari E. Acta Mater, 2000; 48: 3027 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|