| Hot Deformation Behavior of 35CrMo Steel |
| ZHANG Bin; ZHANG Hongbing |
| Technology Center; Shanghai No.1 Iron Steel Co.; LTD of Bao Steel Group. Shanghai 200431 |
|
Cite this article:
ZHANG Bin; ZHANG Hongbing. Hot Deformation Behavior of 35CrMo Steel. Acta Metall Sin, 2004, 40(10): 1109-1114 .
|
|
|
Abstract The recrystallization behavior of the steel 35CrMo during hot deformation
was investigated using physical simulation experiments, and the condition
of dynamic recrystallizaiton (DRX) was obtained to be: T>1000℃, A modified DRX kinetic equation is submitted
, from which the DRX fraction calculated
is good agreement with the experiments. An equation describing dynamic
recrystallization grain size can be written . Through the 2-stroke compression
and 1-stroke compression followed by holding temperature experiment, the
activation energy and kinetics equation of static recrystallization (SRX)
of the steel 35CrMo are also obtained.
|
|
Received: 13 November 2003
|
|
|
[1] Sellars C M. Mater Sci Technol, 1990; 6: 1072 [2] Mcqueen H J. J Mater Proc Technol, 1993; 37: 3 [3] Mcqueen H J, Jonas J J. J Appl Metalworking, 1984; 3:233 [4] Wang G D, Liu Z Y. The Control Rolling and ControlCooling of HSLA Steel. Beijing: Metallurgy IndustryPress, 1992: 263(王国栋,刘振宇.高强度低合金钢的控制轧制与控制冷却.北京:冶金工业出版社,1992:263) [5] Weiss I, Sakai T, Jonas J J. Metall Sci, 1984; 2: 77 [6] Laasraoui A, Jonas J J. Metall Trans A, 1991; 22A: 151 [7] Fabregue P. In: Jonas J J ed, Advances in Hot Deformation Texture and Microstructure. New York: The Materials Metals & Materials Society, 1994: 75 [8] Dutta B, Sellars C M. Mater Sci Technol, 1987; 3: 197 [9] Medina S F, Mancilla J E. ISIJ Int, 1996; 36: 1070 |