| Effect of La2O3 on Hardness Distributions of Laser Clad Ferrite--Based |
| ZHAO Gaomin; WANG Kunlin; LIU Jiajun |
| Department of Mechanical Engineering; Tsinghua University; Beijing 100084 |
|
Cite this article:
ZHAO Gaomin; WANG Kunlin; LIU Jiajun. Effect of La2O3 on Hardness Distributions of Laser Clad Ferrite--Based. Acta Metall Sin, 2004, 40(10): 1115-1120 .
|
|
|
Abstract The morphologies of laser clad ferrite--based alloy coatings with
different contents of rare earth (RE) were observed by SEM. The
nanohardness and the elastic modulus of the near the surface
and overlapping area were tested by nanoindentation. The hardness
distribution in the coating was measured by microhardness tester. The
experimental results show that the microstructure of the coatings
with RE was refined, the spacing of second dendrites was reduced, and
spacing the
nanohardness and elastic modulus were
increased. The average hardness (HV) of the coating with RE is about 500,
which is 50 higher than that without RE. The mechanism of the RE
effect was discussed.
|
|
Received: 13 November 2003
|
|
|
[1] Wang Y; Liu J J. Surf Eng, 1993; 9 (2) : 151 [2] Tsai H L, Tsai P C. J Mater Eng Perfor, 1995; 4: 689 [3] Liu Y C, Liu J Y, Yin Y S. J Chin Rare Earths Soc, 2001; 19: 281(刘英才,刘俊友,尹衍生.中国稀土学报,2001;19:281) [4] Xu Y, Ji H, Wei Y D. Chin Rare Earth, 2001; 22(1) : 50(许越,纪红,韦永德.稀土,2001;22(1) :50) [5] Agarwal A, Dahotre N B. Surf Eng, 2001; 17(10) : 66 [6] Hua W S, Wu X F, Lu H, Shen D H. Mater Mech Eng, 2002; 27(3) : 8(华文深,吴杏芳,陆华,沈电洪.机械工程材料,2002;27(3) :8) [7] Hua W S, Wu X F, Shen D H. Appl Surf Sci, 2002; 189:72 [8] Oliver W C, Pharr G M. J Mater Res, 1992; 7: 1564 [9] Hua W S, Wu X F, Lu H. Acta Metall Sin, 2002; 38: 1109(华文深,吴杏芳,陆华.金属学报,2002;38:1109) [10] Zhang L Q, Chen G N. Met Heat Treatment, 2002; 27(11) : 10(张来启,陈光南.金属热处理,2002;27(11) :10) [11] PAN Y J, Xu B F, LI A M. Met Heat Treatment, 2002; 27(8) : 17(潘应君,许伯藩,李安敏.金属热处理,2002;27(8) :17) [12] Caralho N J M, De Hosson J Th M. Surf Eng, 2001; 17(2) :105 [13] Shan J G, Ding J C, Ren J L. J Chin Weld, 2001; 22(4) :1(单际国,丁建春,任家烈.焊接学报,2001;22(4) :1) [14] Wang W. J Chin Rare Earths, 1990; 8: 252(王武.稀土学报,1990;8:252) [15] Shang L J, Yan X M, Li F. J Shenyang Polytechnic Univ, 1995; 17 (2) : 37(尚丽娟,阎秀梅,李峰.沈阳工业大学学报,1995;17(2) :37) [16] Sun W C, Zhang S R, Hou A Q. Rare Earth Behavior in Aluminum Alloy. Beijing: Weapon Industry Press, 1992: 225(孙伟成,张淑荣,候爱芹.稀土在铝合金中的行为.北京:兵器工业出版社,1992:225) [17] Yu D H. Chin Sci Bull, 1981; 4: 206(余端璜.科学通报,1981;4:206) [18] Ji Z S. J Chin Rare Earths Soc, 2000; 18(1) : 27(吉泽升.中国稀土学报,2000;18(1) :27) |