Please wait a minute...
Acta Metall Sin  1998, Vol. 34 Issue (9): 966-970    DOI:
Current Issue | Archive | Adv Search |
IN-SITU IMAGE GRAB AND ANALYSIS FOR PITTING PROCESS OF 304 STAINLESS STEEL
SU Runxi; SONG Shizhe (School of Materials Science and Engineering; Tianjin University; Tianjin 300072)Correspondent. SONG Shizhe; professor; Tel: (022)27405823; Fax: (022)27404724;E-mail: szsong@tju. edu. cn
Cite this article: 

SU Runxi; SONG Shizhe (School of Materials Science and Engineering; Tianjin University; Tianjin 300072)Correspondent. SONG Shizhe; professor; Tel: (022)27405823; Fax: (022)27404724;E-mail: szsong@tju. edu. cn. IN-SITU IMAGE GRAB AND ANALYSIS FOR PITTING PROCESS OF 304 STAINLESS STEEL. Acta Metall Sin, 1998, 34(9): 966-970.

Download:  PDF(1101KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  A method for grabbing and analyzing in-situ images was established to study pitting corrosion in 304 stainless steel. Using a self-developed Visual C++ program, images obtained upon potentiostatic polarization were analyzed. It was found that there was a liner relationship between pitting ratio and reaction electric quantity. Besides, lots of small pits became a larger pit, and grays moved towards smaller values and double peaks were observed on the gray histograms when pitting corrosion happened.
Key words:  image processing      stainless steel      pitting     
Received:  18 September 1998     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1998/V34/I9/966

1 Itzhak D, Dinstein I,Zilberberg T CorrosSci, 1981; 21: 17
2 Costa J M , Sagues F, Vilarrasa M. Corros Sci, 1991;32:665
3 苏润西,宋诗哲第九届全国电化学会议论文摘要集,泰安,1997:425(Su R X,Song S Z Proc 9th CSE National Meeting, Tai'an China, 1997:425)
[1] ZHANG Qiliang, WANG Yuchao, LI Guangda, LI Xianjun, HUANG Yi, XU Yunze. Erosion-Corrosion Performance of EH36 Steel Under Sand Impacts of Different Particle Sizes[J]. 金属学报, 2023, 59(7): 893-904.
[2] HOU Juan, DAI Binbin, MIN Shiling, LIU Hui, JIANG Menglei, YANG Fan. Influence of Size Design on Microstructure and Properties of 304L Stainless Steel by Selective Laser Melting[J]. 金属学报, 2023, 59(5): 623-635.
[3] WANG Bin, NIU Mengchao, WANG Wei, JIANG Tao, LUAN Junhua, YANG Ke. Microstructure and Strength-Toughness of a Cu-Contained Maraging Stainless Steel[J]. 金属学报, 2023, 59(5): 636-646.
[4] WU Xinqiang, RONG Lijian, TAN Jibo, CHEN Shenghu, HU Xiaofeng, ZHANG Yangpeng, ZHANG Ziyu. Research Advance on Liquid Lead-Bismuth Eutectic Corrosion Resistant Si Enhanced Ferritic/Martensitic and Austenitic Stainless Steels[J]. 金属学报, 2023, 59(4): 502-512.
[5] HAN En-Hou, WANG Jianqiu. Effect of Surface State on Corrosion and Stress Corrosion for Nuclear Materials[J]. 金属学报, 2023, 59(4): 513-522.
[6] CHANG Litao. Corrosion and Stress Corrosion Crack Initiation in the Machined Surfaces of Austenitic Stainless Steels in Pressurized Water Reactor Primary Water: Research Progress and Perspective[J]. 金属学报, 2023, 59(2): 191-204.
[7] XIA Dahai, JI Yuanyuan, MAO Yingchang, DENG Chengman, ZHU Yu, HU Wenbin. Localized Corrosion Mechanism of 2024 Aluminum Alloy in a Simulated Dynamic Seawater/Air Interface[J]. 金属学报, 2023, 59(2): 297-308.
[8] WEN Donghui, JIANG Beibei, WANG Qing, LI Xiangwei, ZHANG Peng, ZHANG Shuyan. Microstructure Evolution at Elevated Temperature and Mechanical Properties of MoNb-Modified FeCrAl Stainless Steel[J]. 金属学报, 2022, 58(7): 883-894.
[9] SUN Yangting, LI Yiwei, WU Wenbo, JIANG Yiming, LI Jin. Effect of Inclusions on Pitting Corrosion of C70S6 Non-Quenched and Tempered Steel Doped with Ca and Mg[J]. 金属学报, 2022, 58(7): 895-904.
[10] ZHENG Chun, LIU Jiabin, JIANG Laizhu, YANG Cheng, JIANG Meixue. Effect of Tensile Deformation on Microstructure and Corrosion Resistance of High Nitrogen Austenitic Stainless Steels[J]. 金属学报, 2022, 58(2): 193-205.
[11] YUAN Jiahua, ZHANG Qiuhong, WANG Jinliang, WANG Lingyu, WANG Chenchong, XU Wei. Synergistic Effect of Magnetic Field and Grain Size on Martensite Nucleation and Variant Selection[J]. 金属学报, 2022, 58(12): 1570-1580.
[12] LUO Wenze, HU Long, DENG Dean. Numerical Simulation and Development of Efficient Calculation Method for Residual Stress of SUS316 Saddle Tube-Pipe Joint[J]. 金属学报, 2022, 58(10): 1334-1348.
[13] PAN Qingsong, CUI Fang, TAO Nairong, LU Lei. Strain-Controlled Fatigue Behavior of Nanotwin- Strengthened 304 Austenitic Stainless Steel[J]. 金属学报, 2022, 58(1): 45-53.
[14] CAO Chao, JIANG Chengyang, LU Jintao, CHEN Minghui, GENG Shujiang, WANG Fuhui. Corrosion Behavior of Austenitic Stainless Steel with Different Cr Contents in 700oC Coal Ash/High Sulfur Flue-Gas Environment[J]. 金属学报, 2022, 58(1): 67-74.
[15] AN Xudong, ZHU Te, WANG Qianqian, SONG Yamin, LIU Jinyang, ZHANG Peng, ZHANG Zhaokuan, WAN Mingpan, CAO Xingzhong. Interaction Mechanism of Dislocation and Hydrogen in Austenitic 316 Stainless Steel[J]. 金属学报, 2021, 57(7): 913-920.
No Suggested Reading articles found!