REACTION MECHANISM AND DISTRIBUTION RULE OF SILICON IN MELTING GASIFIER
LU Qing(Department of Metallurgy; Hebei Institute of Technology; Tangshan 063009)
Cite this article: 

LU Qing(Department of Metallurgy; Hebei Institute of Technology; Tangshan 063009). REACTION MECHANISM AND DISTRIBUTION RULE OF SILICON IN MELTING GASIFIER. Acta Metall Sin, 1998, 34(7): 763-768.

Download:  PDF(1260KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Smelting process of melting gasifier is simulated. According to chemical thermodynamics, source of [Si] in furnace, the reaction mechanism, the rule of distribution and factors related to [Si] content were discussed.
Key words:  melting gasifier      Si      reaction      distribution     
Received:  18 July 1998     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1998/V34/I7/763

1 Hotchison S G. Metall Trans, 1988; 19B: 249
2 Ozturk B, Fruehan R J. Metall Trans, 1985; 16B: 121
3 武田斡治,田口整司,福武刚,加藤治雄,池田义俊,才野光男,中井岁一.铁 钢,19862 72:871(Kanji T, Taguchi N, Fukutake K, Kato H, Iketa Y, Saino M, Nafori T Tetsu Hagahe, 1986; 72: S71)
4 Turkdogan E T. Metall Trans, 1978; 9B: 163
5 Tsuchiya N. Tokuda M, Ohtani M. Metall Trans, 1976: 7B: 315
6宋建成.北京科技大学学报,1990;12:313(Song Jiancheng. J Univ Sci Technol Beijing; 1990 12: 313)
7 邓守强,施月循.钢铁,1989;24:5(Deng Shouqiang,Shi Yuexun.Iron Steel,1989; 24:5)
8 吕庆。东北大学博士学位论文,1994(Lu Qing. PhD Thesis, Northeastern University, 1994)
9九岛行正,内藤诚章,柴田清,佐藤裕二,吉田均、铁 钢,1989;75:1286(Kushima K, Narro M, Sibata K, Sato H, Yoshida H. Tetsu Hagane, 1989; 75: 1286)
[1] LU Nannan, GUO Yimo, YANG Shulin, LIANG Jingjing, ZHOU Yizhou, SUN Xiaofeng, LI Jinguo. Formation Mechanisms of Hot Cracks in Laser Additive Repairing Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1243-1252.
[2] FENG Qiang, LU Song, LI Wendao, ZHANG Xiaorui, LI Longfei, ZOU Min, ZHUANG Xiaoli. Recent Progress in Alloy Design and Creep Mechanism of γ'-Strengthened Co-Based Superalloys[J]. 金属学报, 2023, 59(9): 1125-1143.
[3] ZHANG Jian, WANG Li, XIE Guang, WANG Dong, SHEN Jian, LU Yuzhang, HUANG Yaqi, LI Yawei. Recent Progress in Research and Development of Nickel-Based Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1109-1124.
[4] ZHAO Peng, XIE Guang, DUAN Huichao, ZHANG Jian, DU Kui. Recrystallization During Thermo-Mechanical Fatigue of Two High-Generation Ni-Based Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1221-1229.
[5] DU Jinhui, BI Zhongnan, QU Jinglong. Recent Development of Triple Melt GH4169 Alloy[J]. 金属学报, 2023, 59(9): 1159-1172.
[6] LI Jiarong, DONG Jianmin, HAN Mei, LIU Shizhong. Effects of Sand Blasting on Surface Integrity and High Cycle Fatigue Properties of DD6 Single Crystal Superalloy[J]. 金属学报, 2023, 59(9): 1201-1208.
[7] GONG Shengkai, LIU Yuan, GENG Lilun, RU Yi, ZHAO Wenyue, PEI Yanling, LI Shusuo. Advances in the Regulation and Interfacial Behavior of Coatings/Superalloys[J]. 金属学报, 2023, 59(9): 1097-1108.
[8] BI Zhongnan, QIN Hailong, LIU Pei, SHI Songyi, XIE Jinli, ZHANG Ji. Research Progress Regarding Quantitative Characterization and Control Technology of Residual Stress in Superalloy Forgings[J]. 金属学报, 2023, 59(9): 1144-1158.
[9] ZHENG Liang, ZHANG Qiang, LI Zhou, ZHANG Guoqing. Effects of Oxygen Increasing/Decreasing Processes on Surface Characteristics of Superalloy Powders and Properties of Their Bulk Alloy Counterparts: Powders Storage and Degassing[J]. 金属学报, 2023, 59(9): 1265-1278.
[10] JIANG He, NAI Qiliang, XU Chao, ZHAO Xiao, YAO Zhihao, DONG Jianxin. Sensitive Temperature and Reason of Rapid Fatigue Crack Propagation in Nickel-Based Superalloy[J]. 金属学报, 2023, 59(9): 1190-1200.
[11] CHEN Jia, GUO Min, YANG Min, LIU Lin, ZHANG Jun. Effects of W Concentration on Creep Microstructure and Property of Novel Co-Based Superalloys[J]. 金属学报, 2023, 59(9): 1209-1220.
[12] LIU Wei, CHEN Wanqi, MA Menghan, LI Kailun. Review of Irradiation Damage Behavior of Tungsten Exposed to Plasma in Nuclear Fusion[J]. 金属学报, 2023, 59(8): 986-1000.
[13] LIU Xingjun, WEI Zhenbang, LU Yong, HAN Jiajia, SHI Rongpei, WANG Cuiping. Progress on the Diffusion Kinetics of Novel Co-based and Nb-Si-based Superalloys[J]. 金属学报, 2023, 59(8): 969-985.
[14] CHANG Songtao, ZHANG Fang, SHA Yuhui, ZUO Liang. Recrystallization Texture Competition Mediated by Segregation Element in Body-Centered Cubic Metals[J]. 金属学报, 2023, 59(8): 1065-1074.
[15] ZHANG Haifeng, YAN Haile, FANG Feng, JIA Nan. Molecular Dynamic Simulations of Deformation Mechanisms for FeMnCoCrNi High-Entropy Alloy Bicrystal Micropillars[J]. 金属学报, 2023, 59(8): 1051-1064.
No Suggested Reading articles found!