Please wait a minute...
Acta Metall Sin  1998, Vol. 34 Issue (11): 1131-1136    DOI:
论文 Current Issue | Archive | Adv Search |
OXIDATION RESISTANCE OF Fe_3Al INTERMETALLICS AT HIGH TEMPERATURES
SUN Yangshan;YU Xinquan;HUANG Haibo;SUN Guoxiong (Department of Materials Science and Engineering; Southeast University; Nanjing 210096)
Cite this article: 

SUN Yangshan;YU Xinquan;HUANG Haibo;SUN Guoxiong (Department of Materials Science and Engineering; Southeast University; Nanjing 210096). OXIDATION RESISTANCE OF Fe_3Al INTERMETALLICS AT HIGH TEMPERATURES. Acta Metall Sin, 1998, 34(11): 1131-1136.

Download:  PDF(2002KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  

The oxidation resistance of the binary Fe3Al decreases rapidly with the increase of temperature when the temperature is above 1000℃. SEM observations have revealed wisker-shaped oxides on specimen surface oxidized at 1200℃. Cavities and internal oxidation have been observed between the oxidation layer and the matrix of oxidized specimen. Microalloying of Ce increases the oxidation resistance of Fe3Al based alloys significantly. After oxidizing at 1200℃ for a long time (120 h), the specimen surface of the Fe3Al alloy containing cerium is still smooth without spalling and its oxidation resistance is one order of magnitude higher than that of the alloy without cerium addition.

Key words:  Fe_3Al      intermetallics      oxidation      cerium      Fe_3Al      intermetallics      oxidation      cerium     
Received:  18 November 1998     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1998/V34/I11/1131

1Mckamey C G, Devan J H, Tortoreli P T, Sikka V K.J Mater Res; 1991; 6: 1779
2Marcinkowski M J,Taylor M E, Kayser F X.J Mater Sci,1975;10: 4
3 Nishino Y,Kumada C,Asano S.Scr Metall,1997;4:461
4何华英.东南大学硕士学位论文.1998(He H Y.Master Dissertation, Southeast University,1998)
5朱日彰.高温腐蚀及耐高温腐蚀材料上海:上海科技出版社,1995:19(Zhu R Z. High Temperature Corrosion and Corrosion Resistant Materials. Shanghai:Shanghai Sol. &Tech Press; 1995: 19)
6范雄.X射线金属学北京:机械工业出版社,1980:108(Fan X X-ray Analysis of Metals Beijing:Mechanical Industry Press,1980:108)
7 Caplan A D; Hussey R J. Oxid Met, 1980; 14: 279
8 Gibbs G B, Hales R. Corr Sci, 1972; 14: 1021
9 Pint B A. Oxid Met, 1996; 45: 1
10余新泉.东南大学博士学位论文,1998(Yu X Q. Ph D Dissertation Southeast Univ, 1998)
11 Evans H E. Mater High Temp, 1994; 12: 219o

[1] HUANG Ding, QIAO Yanxin, YANG Lanlan, WANG Jinlong, CHEN Minghui, ZHU Shenglong, WANG Fuhui. Effect of Shot Peening of Substrate Surface on Cyclic Oxidation Behavior of Sputtered Nanocrystalline Coating[J]. 金属学报, 2023, 59(5): 668-678.
[2] SHEN Zhao, WANG Zhipeng, HU Bo, LI Dejiang, ZENG Xiaoqin, DING Wenjiang. Research Progress on the Mechanisms Controlling High-Temperature Oxidation Resistance of Mg Alloys[J]. 金属学报, 2023, 59(3): 371-386.
[3] LIU Laidi, DING Biao, REN Weili, ZHONG Yunbo, WANG Hui, WANG Qiuliang. Multilayer Structure of DZ445 Ni-Based Superalloy Formed by Long Time Oxidation at High Temperature[J]. 金属学报, 2023, 59(3): 387-398.
[4] LI Xin, JIANG He, YAO Zhihao, DONG Jianxin. Theoretical Calculation and Analysis of the Effect of Oxygen Atom on the Grain Boundary of Superalloy Matrices Ni, Co and NiCr[J]. 金属学报, 2023, 59(2): 309-318.
[5] XU Wenguo, HAO Wenjiang, LI Yingju, ZHAO Qingbin, LU Bingyu, GUO Heyi, LIU Tianyu, FENG Xiaohui, YANG Yuansheng. Effects of Trace Aluminum and Titanium on High Temper-ature Oxidation Behavior of Inconel 690 Alloy[J]. 金属学报, 2023, 59(12): 1547-1558.
[6] JIN Xinyan, CHU Shuangjie, PENG Jun, HU Guangkui. Effect of Dew Point on Selective Oxidation and Decarburization of 0.2%C-1.5%Si-2.5%Mn High Strength Steel Sheet During Continuous Annealing[J]. 金属学报, 2023, 59(10): 1324-1334.
[7] HU Min, ZHOU Shengyu, GUO Jingyuan, HU Minghao, LI Chong, LI Huijun, WANG Zumin, LIU Yongchang. Oxidation Behavior of Micro-Regions in Multiphase Ni3Al-Based Superalloys[J]. 金属学报, 2023, 59(10): 1346-1354.
[8] CONG Hongda, WANG Jinlong, WANG Cheng, NING Shen, GAO Ruoheng, DU Yao, CHEN Minghui, ZHU Shenglong, WANG Fuhui. A New Design Inorganic Silicate Composite Coating and Its Oxidation Behavior at High Temperature in Steam Atmosphere[J]. 金属学报, 2022, 58(8): 1083-1092.
[9] XIE Leipeng, SUN Wenyao, CHEN Minghui, WANG Jinlong, WANG Fuhui. Effects of Processing on Microstructures and Properties of FGH4097 Superalloy[J]. 金属学报, 2022, 58(8): 992-1002.
[10] ZHAO Xiaofeng, LI Ling, ZHANG Han, LU Jie. Research Progress in High-Entropy Alloy Bond Coat Material for Thermal Barrier Coatings[J]. 金属学报, 2022, 58(4): 503-512.
[11] SU Kaixin, ZHANG Jiwang, ZHANG Yanbin, YAN Tao, LI Hang, JI Dongdong. High-Cycle Fatigue Properties and Residual Stress Relaxation Mechanism of Micro-Arc Oxidation 6082-T6 Aluminum Alloy[J]. 金属学报, 2022, 58(3): 334-344.
[12] PENG Jun, JIN Xinyan, ZHONG Yong, WANG Li. Influence of Substrate Surface Structure on the Galvanizability of Fe-16Mn-0.7C-1.5Al TWIP Steel Sheet[J]. 金属学报, 2022, 58(12): 1600-1610.
[13] CAO Chao, JIANG Chengyang, LU Jintao, CHEN Minghui, GENG Shujiang, WANG Fuhui. Corrosion Behavior of Austenitic Stainless Steel with Different Cr Contents in 700oC Coal Ash/High Sulfur Flue-Gas Environment[J]. 金属学报, 2022, 58(1): 67-74.
[14] CHEN Shenghu, RONG Lijian. Oxide Scale Formation on Ultrafine-Grained Ferritic-Martensitic Steel During Pre-Oxidation and Its Effect on the Corrosion Performance in Stagnant Liquid Pb-Bi Eutectic[J]. 金属学报, 2021, 57(8): 989-999.
[15] PI Huilong, SHI Xiaolei, XU Xingxiang. Effect of SiC-ZrC Coating Prepared by SiZr Liquid Phase Sintering on the Oxidation Resistance of C/SiC Composites[J]. 金属学报, 2021, 57(6): 791-796.
No Suggested Reading articles found!