Please wait a minute...
Acta Metall Sin  1998, Vol. 34 Issue (1): 7-12    DOI:
Current Issue | Archive | Adv Search |
SIMULATION OF SOLIDIFICATION BEHAVIOR IN SPRAY DEPOSITED PREFORMⅠ. Theoretical Analysis
ZHANG Jishan; CUI Hua; DUAN Xianjin; SUN Zuqing; CHEN Guoliang (State Key Laboratory of Advanced Metals and Materials; University of Science and Technology Beijing; Beijing 100083)
Cite this article: 

ZHANG Jishan; CUI Hua; DUAN Xianjin; SUN Zuqing; CHEN Guoliang (State Key Laboratory of Advanced Metals and Materials; University of Science and Technology Beijing; Beijing 100083). SIMULATION OF SOLIDIFICATION BEHAVIOR IN SPRAY DEPOSITED PREFORMⅠ. Theoretical Analysis. Acta Metall Sin, 1998, 34(1): 7-12.

Download:  PDF(363KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Solidification in preform is an important stage during spray forming process, which shows great effect on the final formation of microstructure within the spray deposited preform. It is essential to make a full understanding of the solidification process to optimize the spray forming process and obtain desired preform microstructures. In this study, a concept of"vertual"solidification layer is applied to establish a theoretical model to simulate the solidification process in preform during spray forming, which will provide a theoretical tool for the further analysis of the solidification behavior in spray deposited preform.
Key words:  spray forming      deposition perform      solidification      simulation     
Received:  18 January 1998     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1998/V34/I1/7

1 张济山,段先进.王迪,张卫军,陈国良.金属学报,1995;31(Suppl):638(Zhang Jlshan,Duan Xianjin,Wang Di,Zhang Weijun,Chen Guoliang.Acta Metall Sin,1995;31(Suppl):638)
2 张济山,孙祖庆,陈国良. 96’秋季中国材料研讨会论文集,北京,1996:300(Zhang Jlshan,Sun Zuqing,Chen Guoliang.Proc Chin Mater Res Soc Symp’96 Autumn,Beijing,1996:300)
3 Carcia A, Prates M Metall Trans,1978; 9B: 409
4 Garcia A,Clyne T W, Prates M.Metall Trans;1979; 10B:85
5 Mahur P,Appelian D.Lawley A Acta Metall,1989; 37:42Z
[1] ZHANG Jian, WANG Li, XIE Guang, WANG Dong, SHEN Jian, LU Yuzhang, HUANG Yaqi, LI Yawei. Recent Progress in Research and Development of Nickel-Based Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1109-1124.
[2] MA Dexin, ZHAO Yunxing, XU Weitai, WANG Fu. Effect of Gravity on Directionally Solidified Structure of Superalloys[J]. 金属学报, 2023, 59(9): 1279-1290.
[3] CHEN Jia, GUO Min, YANG Min, LIU Lin, ZHANG Jun. Effects of W Concentration on Creep Microstructure and Property of Novel Co-Based Superalloys[J]. 金属学报, 2023, 59(9): 1209-1220.
[4] BI Zhongnan, QIN Hailong, LIU Pei, SHI Songyi, XIE Jinli, ZHANG Ji. Research Progress Regarding Quantitative Characterization and Control Technology of Residual Stress in Superalloy Forgings[J]. 金属学报, 2023, 59(9): 1144-1158.
[5] ZHANG Haifeng, YAN Haile, FANG Feng, JIA Nan. Molecular Dynamic Simulations of Deformation Mechanisms for FeMnCoCrNi High-Entropy Alloy Bicrystal Micropillars[J]. 金属学报, 2023, 59(8): 1051-1064.
[6] ZHANG Lu, YU Zhiwei, ZHANG Leicheng, JIANG Rong, SONG Yingdong. Thermo-Mechanical Fatigue Cycle Damage Mechanism and Numerical Simulation of GH4169 Superalloy[J]. 金属学报, 2023, 59(7): 871-883.
[7] HOU Juan, DAI Binbin, MIN Shiling, LIU Hui, JIANG Menglei, YANG Fan. Influence of Size Design on Microstructure and Properties of 304L Stainless Steel by Selective Laser Melting[J]. 金属学报, 2023, 59(5): 623-635.
[8] LIU Jihao, ZHOU Jian, WU Huibin, MA Dangshen, XU Huixia, MA Zhijun. Segregation and Solidification Mechanism in Spray-Formed M3 High-Speed Steel[J]. 金属学报, 2023, 59(5): 599-610.
[9] CHEN Kaixuan, LI Zongxuan, WANG Zidong, Demange Gilles, CHEN Xiaohua, ZHANG Jiawei, WU Xuehua, Zapolsky Helena. Morphological Evolution of Fe-Rich Precipitates in a Cu-2.0Fe Alloy During Isothermal Treatment[J]. 金属学报, 2023, 59(12): 1665-1674.
[10] SU Zhenqi, ZHANG Congjiang, YUAN Xiaotan, HU Xingjin, LU Keke, REN Weili, DING Biao, ZHENG Tianxiang, SHEN Zhe, ZHONG Yunbo, WANG Hui, WANG Qiuliang. Formation and Evolution of Stray Grains on Remelted Interface in the Seed Crystal During the Directional Solidification of Single-Crystal Superalloys Assisted by Vertical Static Magnetic Field[J]. 金属学报, 2023, 59(12): 1568-1580.
[11] WANG Chongyang, HAN Shiwei, XIE Feng, HU Long, DENG Dean. Influence of Solid-State Phase Transformation and Softening Effect on Welding Residual Stress of Ultra-High Strength Steel[J]. 金属学报, 2023, 59(12): 1613-1623.
[12] ZHANG Kaiyuan, DONG Wenchao, ZHAO Dong, LI Shijian, LU Shanping. Effect of Solid-State Phase Transformation on Stress and Distortion for Fe-Co-Ni Ultra-High Strength Steel Components During Welding and Vacuum Gas Quenching Processes[J]. 金属学报, 2023, 59(12): 1633-1643.
[13] ZHOU Xiaobin, ZHAO Zhanshan, WANG Wanxing, XU Jianguo, YUE Qiang. Physical and Mathematical Simulation on the Bubble Entrainment Behavior at Slag-Metal Interface[J]. 金属学报, 2023, 59(11): 1523-1532.
[14] QI Xiaoyong, LIU Wenbo, HE Zongbei, WANG Yifan, YUN Di. Phase-Field Simulation of the Densification Process During Sintering of UN Nuclear Fuel[J]. 金属学报, 2023, 59(11): 1513-1522.
[15] LI Sai, YANG Zenan, ZHANG Chi, YANG Zhigang. Phase Field Study of the Diffusional Paths in Pearlite-Austenite Transformation[J]. 金属学报, 2023, 59(10): 1376-1388.
No Suggested Reading articles found!