Please wait a minute...
Acta Metall Sin  1998, Vol. 34 Issue (1): 1-6    DOI:
论文 Current Issue | Archive | Adv Search |
NUMERICAL SIMULATION OF THE INTERLAMELLAR SPACING OF Al-CuAl_2 EUTECTIC
ZHANG Weiqiang;YANG Yuansheng; HU Zhuangqi (State Key Lab of RSA; Institute of Metal Research; The Chinese Academy of Sciences; Shenyang 110015)
Cite this article: 

ZHANG Weiqiang;YANG Yuansheng; HU Zhuangqi (State Key Lab of RSA; Institute of Metal Research; The Chinese Academy of Sciences; Shenyang 110015). NUMERICAL SIMULATION OF THE INTERLAMELLAR SPACING OF Al-CuAl_2 EUTECTIC. Acta Metall Sin, 1998, 34(1): 1-6.

Download:  PDF(431KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  

In this paper, a time-dependent model of directionally solidified Al-CuAl2 eutectic system is numerically calculated according to the theory of lamellar eutectic growth. The computed minimal and maxiamal interlamellar spacings correspond well to the experimental results,the lamellar spacing increases due to melt flow in solidification, and such structure is unstable as the spacing exceeds the maximum. Moreover, the lower the growing rate, the greater the effect of fluid flow.

Key words:  eutectic      lamellar spacing      fluid flow      stability     
Received:  18 January 1998     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1998/V34/I1/1

1 Jackson A.Hunt J D,Trans Metall Soc AIME;1966; 236:1129
2 Trivedi R,Magnin P,Kurz W、Acta Metall Mater. 1987; 35: 971
3 Fisher Jt Kurz W. Acta Metall; 1980; 28: 777
4 Qunenisset M,Nalslain R, J Crystal Growth,1981;54:465
5 Magnin P,Trivedi R.Acta Metall Mater.1991:39:453
6 Jordan M,Hunt J D Metall Tarns, 1971; 2:453
7 Ourdjini A,Liu J, Elliott R.Mater,Set Technol,1994;10:312
8 Clark J N, Elliott R. Metall Trons,1976;7A:1197
9 Liu J,Elliott R.Acta Metall Mater,1995;43:3301
10 Zhang Weiqang,Liu Qingmin,Zhu Yuefeng,Yang Yuansheng,Hu Zhuangqi.Acta Metall Sin(Engl Lett),1997;10:461
[1] WANG Lei, LIU Mengya, LIU Yang, SONG Xiu, MENG Fanqiang. Research Progress on Surface Impact Strengthening Mechanisms and Application of Nickel-Based Superalloys[J]. 金属学报, 2023, 59(9): 1173-1189.
[2] LU Nannan, GUO Yimo, YANG Shulin, LIANG Jingjing, ZHOU Yizhou, SUN Xiaofeng, LI Jinguo. Formation Mechanisms of Hot Cracks in Laser Additive Repairing Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1243-1252.
[3] YUAN Jianghuai, WANG Zhenyu, MA Guanshui, ZHOU Guangxue, CHENG Xiaoying, WANG Aiying. Effect of Phase-Structure Evolution on Mechanical Properties of Cr2AlC Coating[J]. 金属学报, 2023, 59(7): 961-968.
[4] FENG Aihan, CHEN Qiang, WANG Jian, WANG Hao, QU Shoujiang, CHEN Daolun. Thermal Stability of Microstructures in Low-Density Ti2AlNb-Based Alloy Hot Rolled Plate[J]. 金属学报, 2023, 59(6): 777-786.
[5] WU Xinqiang, RONG Lijian, TAN Jibo, CHEN Shenghu, HU Xiaofeng, ZHANG Yangpeng, ZHANG Ziyu. Research Advance on Liquid Lead-Bismuth Eutectic Corrosion Resistant Si Enhanced Ferritic/Martensitic and Austenitic Stainless Steels[J]. 金属学报, 2023, 59(4): 502-512.
[6] MIAO Junwei, WANG Mingliang, ZHANG Aijun, LU Yiping, WANG Tongmin, LI Tingju. Tribological Properties and Wear Mechanism of AlCr1.3TiNi2 Eutectic High-Entropy Alloy at Elevated Temperature[J]. 金属学报, 2023, 59(2): 267-276.
[7] HU Wenbin, ZHANG Xiaowen, SONG Longfei, LIAO Bokai, WAN Shan, KANG Lei, GUO Xingpeng. Corrosion Behavior of AlCoCrFeNi2.1 Eutectic High-Entropy Alloy in Sulfuric Acid Solution[J]. 金属学报, 2023, 59(12): 1644-1654.
[8] ZHANG Lili, JI Zongwei, ZHAO Jiuzhou, HE Jie, JIANG Hongxiang. Key Factors Influencing Eutectic Si Modification in Al-Si Hypoeutectic Alloy by Trace La[J]. 金属学报, 2023, 59(11): 1541-1546.
[9] FENG Di, ZHU Tian, ZANG Qianhao, LEE Yunsoo, FAN Xi, ZHANG Hao. Solution Behavior of Spray-Formed Hypereutectic AlSiCuMg Alloy[J]. 金属学报, 2022, 58(9): 1129-1140.
[10] WEN Donghui, JIANG Beibei, WANG Qing, LI Xiangwei, ZHANG Peng, ZHANG Shuyan. Microstructure Evolution at Elevated Temperature and Mechanical Properties of MoNb-Modified FeCrAl Stainless Steel[J]. 金属学报, 2022, 58(7): 883-894.
[11] HUANGFU Hao, WANG Zilong, LIU Yongli, MENG Fanshun, SONG Jiupeng, QI Yang. A First Principles Investigation of W1 - x Ir x Alloys: Structural, Electronic, Mechanical, and Thermal Properties[J]. 金属学报, 2022, 58(2): 231-240.
[12] SHEN Guohui, HU Bin, YANG Zhanbing, LUO Haiwen. Influence of Tempering Temperature on Mechanical Properties and Microstructures of High-Al-Contained Medium Mn Steel Having δ-Ferrite[J]. 金属学报, 2022, 58(2): 165-174.
[13] NIE Jinfeng, WU Yuli, XIE Kewei, LIU Xiangfa. Microstructure and Thermal Stability of Heterostructured Al-AlN Nanocomposite[J]. 金属学报, 2022, 58(11): 1497-1508.
[14] MAO Fei, LU Hao, TANG Fawei, GUO Kai, LIU Dong, SONG Xiaoyan. First-Principle Calculation on the Effect of Mn and In on the Structural Stability and Magnetic Moment of SmCo7 Alloys[J]. 金属学报, 2021, 57(7): 948-958.
[15] WANG Yihan, YUAN Yuan, YU Jiabin, WU Honghui, WU Yuan, JIANG Suihe, LIU Xiongjun, WANG Hui, LU Zhaoping. Design for Thermal Stability of Nanocrystalline Alloys Based on High-Entropy Effects[J]. 金属学报, 2021, 57(4): 403-412.
No Suggested Reading articles found!