| RELATION BETWEEN DEBYE TEMPERATURE AND PARTICLE SIZE OF NANOMETER-SIZED SILVER PARTICLES |
| ZHANG Wei;CHEN Li;ZHANG Lide(Institute of Solid State Physics; Chinese Academy of Sciences; Hefei 230031) |
|
Cite this article:
ZHANG Wei;CHEN Li;ZHANG Lide(Institute of Solid State Physics; Chinese Academy of Sciences; Hefei 230031). RELATION BETWEEN DEBYE TEMPERATURE AND PARTICLE SIZE OF NANOMETER-SIZED SILVER PARTICLES. Acta Metall Sin, 1997, 33(9): 987-990.
|
|
|
Abstract Debye temperature of nanometer-sized silver(n-Ag) particles was studied by the method of the double temperature X-ray diffraction. It was found that values of most specimens were higher than that of the bulk-Ag. And there existed a critical size.When the particle size was smaller than the critical value, the smaller the particle size was, the lower its became. To the specimen with larger particle size than the crucial size, its became smaller than that of the specimen with the crucial size.It was also deduced that the relation between and d of n-Ag particles could be given as:which explains the experiment result reasonably.
|
|
Received: 18 September 1997
|
1张立德,牟季美.纳米材料学.沈阳:辽宁科学技术出版社,1994:30 2程本培,虞炳西.物理测试,1991;5:6 3陆学善,梁敬魁.物理学报,1981;10:1366 4Stauuik Z M,Griestiach P,Dehe G,Gutlich P,Stroink G.Phys Rev B 1987;35:6588 5张立德,牟秀美纳米材料学.沈阳:辽宁科学技术出版社,1994:28 6黄昆,韩汝琦.固体物理学.北京:高等教育出版社,1988:83 7冯端,丘第荣.金属物理学(第一卷).北京:科学出版社,1987:31 |