PREPARATION OF HOMOGENEITY IMMISCIBLE ALLOY BY MARANGONI CONVECTION
XIAN Aiping; ZHANG Xiumu; LI Zhongyu; LIU Qingquan; CHEN Jizhi;LI Yiyi(International Center for Materials Physics; Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110015)(Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110015)(Manuscript received 1995-06-06; in revised form 1995-11-07)
Cite this article: 

XIAN Aiping; ZHANG Xiumu; LI Zhongyu; LIU Qingquan; CHEN Jizhi;LI Yiyi(International Center for Materials Physics; Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110015)(Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110015)(Manuscript received 1995-06-06; in revised form 1995-11-07). PREPARATION OF HOMOGENEITY IMMISCIBLE ALLOY BY MARANGONI CONVECTION. Acta Metall Sin, 1996, 32(2): 113-119.

Download:  PDF(544KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  A new control casting technique was designed for making homogeneity immiscible alloy in earth gravity field by Marangoni migration of the secondary phase drops in the melting alloy under a temperature gradient. In the technique, the droplet of the secondary phase ahead the solid-liquid interface of the melt of the immiscible alloy will make Stokes movement in gravity field and Marangoni movement in the opposite direction of gravity field in temperature gradient field. As a result, the net velocity of the droplets in the melt will be dependent on the size of the droplets. When the size of the droplets is very small,Marangoni movement of the droplets will dominate, otherwise Stokes movement will dominate. When the net velocity is zero, there will be a critical size of the droplet. By controlling the stability of the solidification process, an ingot with uniform distribution of the dropletscan be obtained. The critical size of the secondary phase droplets was estimated by the following equation Solidification test on Al-Bi and Al-Pb alloy showed that the size of the Bi or Pb particles in Al matrix is roughly the same order of magnitude as that obtained by above equation.Finally, a new conception, precipitation incubation period, was suggested in the discussion.(Correspondent. XIAN Aiping. professor, Institute of Metal Research, Chinese Academy of Scienoes, Shenyang110015)
Key words:  immiscible alloy      casting      solidification      segregation      fluid physics     
Received:  18 February 1996     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1996/V32/I2/113

1PredelB,RatkeL,FredrikssonH.FluidScienceandMaterialsScienceinSpace,In:WalterHUed,Berlin: Springer,1978:5172RegerJL.MaterialsProcessinginspace.Washington: EarlyExperimentsNASA,19803GellesSH,MarkworthJ.MicrogravityStudiesintheliquidphaseImmiscibleSystemAl-In,15thAJAAConf,losAngeles,1977:774WalterHU.WorkshoponEffectofGravityonSolidificationofImmisciblealloys,Stockholm,ESASP-219,1984;475WalterHU.MicrogravityNewsfromEsa,1994;7:26ZhangXM,XianAP,LiZY,LiuQQ,ChenJZ,LiYY,SecondJapan-ChinaWorkshoponMicrogravityscience,TokyoInstituteofTechnology,1994:177冼爱平,张修睦等.中国专利申请No.94112581.58YoungON,GoldsteinSJ,BlockJM.JFluidMech,1959;6:3509SmithellsCJ,MetalReferenceBook.5thEd,LondonandBoston:BufferWorthsCoLtd,197610McalisterAJ.PhaseDiagramsofBinaryAlloy,ASMUSA,1986:96,14711CamelD,EustathopoulosN,DesreP.ActaMetall,1980;28:23912HultgrenR,DesaiPD,HawkinsDT,GleiserM,KelleyKK.SelectedValuesofThermodynamicpropertiesofBinaryAlloys,MetalsPark,Ohio:AmSocMetals,1973
[1] MA Dexin, ZHAO Yunxing, XU Weitai, WANG Fu. Effect of Gravity on Directionally Solidified Structure of Superalloys[J]. 金属学报, 2023, 59(9): 1279-1290.
[2] ZHANG Jian, WANG Li, XIE Guang, WANG Dong, SHEN Jian, LU Yuzhang, HUANG Yaqi, LI Yawei. Recent Progress in Research and Development of Nickel-Based Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1109-1124.
[3] CHANG Songtao, ZHANG Fang, SHA Yuhui, ZUO Liang. Recrystallization Texture Competition Mediated by Segregation Element in Body-Centered Cubic Metals[J]. 金属学报, 2023, 59(8): 1065-1074.
[4] LIU Jihao, ZHOU Jian, WU Huibin, MA Dangshen, XU Huixia, MA Zhijun. Segregation and Solidification Mechanism in Spray-Formed M3 High-Speed Steel[J]. 金属学报, 2023, 59(5): 599-610.
[5] HOU Juan, DAI Binbin, MIN Shiling, LIU Hui, JIANG Menglei, YANG Fan. Influence of Size Design on Microstructure and Properties of 304L Stainless Steel by Selective Laser Melting[J]. 金属学报, 2023, 59(5): 623-635.
[6] SU Zhenqi, ZHANG Congjiang, YUAN Xiaotan, HU Xingjin, LU Keke, REN Weili, DING Biao, ZHENG Tianxiang, SHEN Zhe, ZHONG Yunbo, WANG Hui, WANG Qiuliang. Formation and Evolution of Stray Grains on Remelted Interface in the Seed Crystal During the Directional Solidification of Single-Crystal Superalloys Assisted by Vertical Static Magnetic Field[J]. 金属学报, 2023, 59(12): 1568-1580.
[7] ZHANG Limin, LI Ning, ZHU Longfei, YIN Pengfei, WANG Jianyuan, WU Hongjing. Macrosegregation Mechanism of Primary Silicon Phase in Cast Hypereutectic Al-Si Alloys Under Alternating Electropulsing[J]. 金属学报, 2023, 59(12): 1624-1632.
[8] CHEN Xueshuang, HUANG Xingmin, LIU Junjie, LV Chao, ZHANG Juan. Microstructure Regulation and Strengthening Mechanisms of a Hot-Rolled & Intercritical Annealed Medium-Mn Steel Containing Mn-Segregation Band[J]. 金属学报, 2023, 59(11): 1448-1456.
[9] DUAN Huichao, WANG Chunyang, YE Hengqiang, DU Kui. Electron Tomography Analysis on the Structure and Chemical Composition of Nanoporous Metal Surfaces[J]. 金属学报, 2023, 59(10): 1291-1298.
[10] PENG Zhiqiang, LIU Qian, GUO Dongwei, ZENG Zihang, CAO Jianghai, HOU Zibing. Independent Change Law of Mold Heat Transfer in Continuous Casting Based on Big Data Mining[J]. 金属学报, 2023, 59(10): 1389-1400.
[11] LIANG Chen, WANG Xiaojuan, WANG Haipeng. Formation Mechanism of B2 Phase and Micro-Mechanical Property of Rapidly Solidified Ti-Al-Nb Alloy[J]. 金属学报, 2022, 58(9): 1169-1178.
[12] SHEN Yingying, ZHANG Guoxing, JIA Qing, WANG Yumin, CUI Yuyou, YANG Rui. Interfacial Reaction and Thermal Stability of the SiCf/TiAl Composites[J]. 金属学报, 2022, 58(9): 1150-1158.
[13] LI Yanqiang, ZHAO Jiuzhou, JIANG Hongxiang, HE Jie. Microstructure Formation in Directionally Solidified Pb-Al Alloy[J]. 金属学报, 2022, 58(8): 1072-1082.
[14] LI Shanshan, CHEN Yun, GONG Tongzhao, CHEN Xingqiu, FU Paixian, LI Dianzhong. Effect of Cooling Rate on the Precipitation Mechanism of Primary Carbide During Solidification in High Carbon-Chromium Bearing Steel[J]. 金属学报, 2022, 58(8): 1024-1034.
[15] WANG Chunhui, YANG Guangyu, ALIMASI Aredake, LI Xiaogang, JIE Wanqi. Effect of Printing Parameters of 3DP Sand Mold on the Casting Performance of ZL205A Alloy[J]. 金属学报, 2022, 58(7): 921-931.
No Suggested Reading articles found!