| IN SITU PREPARATION OF AlN AND TiC PARTICULATES REINFORCED Al MATRIX COMPOSITE |
| CUI Chunxiang; WU Renjie (Shanghai Jiaotong University; Shanghai 200030)(Manuscript received 1995-04-11; in revised form 1995-09-05) |
|
Cite this article:
CUI Chunxiang; WU Renjie (Shanghai Jiaotong University; Shanghai 200030)(Manuscript received 1995-04-11; in revised form 1995-09-05). IN SITU PREPARATION OF AlN AND TiC PARTICULATES REINFORCED Al MATRIX COMPOSITE. Acta Metall Sin, 1996, 32(1): 101-104.
|
|
|
Abstract The better aluminum alloy composite reinforced with AIN-TiC particulates,by in situ reaction, was prepared as follows: an aluminum alloy, containing Ti and others,was melted at temperature ranged from 900 to 1200℃ , and the gaseous atomic nitrogen and carbon flow was injected by proper manner into the melting Al so that AIN (0. 2-1 .2μm) and TiC (2-5μm) formed by in situ reaction dispersed in aluminum matrix homogeneously.Correspondent: CUI Chunxiang,(Institute of Composite, Shanghai Jiaotong University, Shanghai 200030)
|
|
Received: 18 January 1996
|
| 1BaeerB.USPat4710348,19872BurkeJT,AghajanianMK,RocazellaMA.Tomorrow′sMaterialsToday,IntSAMPESympSer34,1989:24403LinY.MetallTrans,1991;22A:8594程兰征,韩世纲.物理化学.上海:上海科学技术出版社,1980:1875RoyM.MetallTrans,1992:23A:28346MurrayJL.BinaryAlloyPhaseDiagrams,Ohio:ASM,MetalsPark,1986:173f |