| PREPARATION OF La SENSOR AND DETERMINATION OF La ACTIVITY IN C-SATURATED MELTED IRON AND ITS SOLIDIFICATION PROCESS |
| WANG Ping; WANG Changzhen (Northeastern University; Shenyang 110006)(Manuscript received 1994-11-25; in revised form 1995-06-08) |
|
Cite this article:
WANG Ping; WANG Changzhen (Northeastern University; Shenyang 110006)(Manuscript received 1994-11-25; in revised form 1995-06-08). PREPARATION OF La SENSOR AND DETERMINATION OF La ACTIVITY IN C-SATURATED MELTED IRON AND ITS SOLIDIFICATION PROCESS. Acta Metall Sin, 1995, 31(21): 394-398.
|
|
|
Abstract The La sensor was composed of polycrystalline La0.95Ca0.05Fz.gs as solid electrolyte, pure La as reference electrode and Mo wire as lead wire. It can be expressed as:Mo
|
|
|
| 1肖理生,隋智通,王常珍.金属学报,1993;29:B3352邹开云,王常珍,赵乃仁,徐秀光.中国稀土学会第三届学术年会论文集,1994;4分册:152-1553McleanALuWK.MetalsMater.1974;8:4524FruehanRJ,MartonjkLJ.MetTrans,1974;5:10275江岛彬夫,铃木健一朗,原因信男,三本木贡治.铁钢,1975;61:27846WilsonWG,KAR,VahedA.JMetals,1974;26:147MazandarangFN,Rehlk2RD.JElactrochemSoc,1974;121:7118JeanninY,MannerskantzC,RkbardsonD.TransAIME1963;227:3009JacobKJ.JElectrochemsoc,1977;124:182 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|