SURFACE REACTION OF Fe_3Al WITH WATER VAPOUR OR OXYGEN
WAN Hiaojing; ZHU Jiahong; HUANG Shengbiao(Shanghai University; Shanghai200072)(Manuscript received 1994-09-05)
Cite this article: 

WAN Hiaojing; ZHU Jiahong; HUANG Shengbiao(Shanghai University; Shanghai200072)(Manuscript received 1994-09-05). SURFACE REACTION OF Fe_3Al WITH WATER VAPOUR OR OXYGEN. Acta Metall Sin, 1995, 31(16): 183-187.

Download:  PDF(363KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The kinetics of surface reaction of Fe3Al with water vapour or oxygen was investigated using AES and XPS. Both reactions are very rapid and initiate after 1.5×100-6 Pa·s exposure. The reaction of Fe3Al with water vapour saturates after an exposure of 1×10-4 Pa·s and the oxide formed is Al2O3, the reaction of Fe3Al with oxygen shows an initial saturation after an exposure of 1.5×10-5 Pa·s, followed by a further stage of reaction. These two stages were supposed to correspond to the oxidation of Al and Fe respectively. The kinetics of these reactions can be used to explain the different ductility behaviour of aluminides in various environments. (Correspondent: WAN Hiaojing , professor, Institute of Metallurgy and Materials Sciences, ShanghaiUniversity, Shanghai,200072)
Key words:  Fe3Al      surface reaction      Auger electron spectrum      hydrogen embrittlement     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1995/V31/I16/183

1LiuCT.In:LiuCTetal.eds.,OrdredIntermetallics-PhysicalMeiallurgrandMechanicalBehavior.KluwerPublishers.1992.3212LiuCT,FuCL,GeorgeEP,PainterGS.ISIJInt,1991:SpecialIssueonAdvancedHigh-TemperatureIntermetallics3WanXJetal.,JMaterSciTech.1994;10:394LiuCT,MekameyCG.In:WangSHetal.eds.,High-TemperatureAluminidesandIntermetallics.TheMineral,MetalsMaterialsSociety,1990:1335WanXJ,ZhuJH,JingKL.ScrMetallMater,1992;26:4736LiuCT,MckameyCG.LeeEH.ScrMeiall,1990;24:3857SheaM,CastagnaA,StoloffNS.MaterResSocProc,1992;213:6098SimmonsGW,PaoPS.WeiRP.MetallTrans,1978,9A:1479WeiRP,PaoPS,HartRG,WeirTW.SimmonsGW.MetallTrans.1980.11A:15110GaoSJ,SimmonsGW,WeiRP.MaterSciEng,1984;62:6511LeeEH,LiuCT,MckameyCG.ScrMetall,1989;23:87512GeorgeEP,LiuCT,PopeDP.ScrMetallMater,1994;30:3713LiuCT,KimYW,ScrMeiallMater,1992;27:5996
[1] XIAO Na, HUI Weijun, ZHANG Yongjian, ZHAO Xiaoli. Hydrogen Embrittlement Behavior of a Vacuum-Carburized Gear Steel[J]. 金属学报, 2021, 57(8): 977-988.
[2] LAN Liangyun, KONG Xiangwei, QIU Chunlin, DU Linxiu. A Review of Recent Advance on Hydrogen Embrittlement Phenomenon Based on Multiscale Mechanical Experiments[J]. 金属学报, 2021, 57(7): 845-859.
[3] LI Jinxu,WANG Wei,ZHOU Yao,LIU Shenguang,FU Hao,WANG Zheng,KAN Bo. A Review of Research Status of Hydrogen Embrittlement for Automotive Advanced High-Strength Steels[J]. 金属学报, 2020, 56(4): 444-458.
[4] LIU Zhenbao,LIANG Jianxiong,SU Jie,WANG Xiaohui,SUN Yongqing,WANG Changjun,YANG Zhiyong. Research and Application Progress in Ultra-HighStrength Stainless Steel[J]. 金属学报, 2020, 56(4): 549-557.
[5] Futao DONG,Fei XUE,Yaqiang TIAN,Liansheng CHEN,Linxiu DU,Xianghua LIU. Effect of Annealing Temperature on Microstructure, Properties and Hydrogen Embrittlement of TWIP Steel[J]. 金属学报, 2019, 55(6): 792-800.
[6] Xiaoli ZHAO, Yongjian ZHANG, Chengwei SHAO, Weijun HUI, Han DONG. Hydrogen Embrittlement of Intercritically AnnealedCold-Rolled 0.1C-5Mn Steel[J]. 金属学报, 2018, 54(7): 1031-1041.
[7] Jun SUN, Suzhi LI, Xiangdong DING, Ju LI. Hydrogenated Vacancy: Basic Properties and Its Influence on Mechanical Behaviors of Metals[J]. 金属学报, 2018, 54(11): 1683-1692.
[8] Yongwei SUN,Jizhi CHEN,Jun LIU. STUDY ON HYDROGEN EMBRITTLEMENT SUSCEPTIBILITY OF 1000 MPa GRADE 0Cr16Ni5Mo STEEL[J]. 金属学报, 2015, 51(11): 1315-1324.
[9] YAN Erhu, LI Xinzhong, TANG Ping, SU Yanqing, GUO Jingjie, FU Hengzhi. MICROSTRUCTURE AND HYDROGEN PERMEATION CHARACTERISTIC OF NEAR EUTECTIC Nb-Ti-Co HYDROGEN SEPARATION ALLOY[J]. 金属学报, 2014, 50(1): 71-78.
[10] LIU Yu, LI Yan, LI Qiang. EFFECT OF CATHODIC POLARIZATION ON HYDROGEN EMBRITTLEMENT SUSCEPTIBILITY OF X80 PIPELINE STEEL IN SIMULATED DEEP SEA ENVIRONMENT[J]. 金属学报, 2013, 49(9): 1089-1097.
[11] WANG Yanfei GONG Jianming JIANG Wenchun JIANG Yong TANG Jianqun . NUMERICAL SIMULATION OF HYDROGEN INDUCED DELAYED FRACTURE OF AISI4135 HIGH STRENGTH STEEL USING COHESIVE ZONE MODELING[J]. 金属学报, 2011, 47(5): 594-600.
[12] LI Yiyi FAN Cungan RONG Lijian YAN Desheng LI Xiuyan. HYDROGEN EMBRITTLEMENT RESISTANCE OF AUSTENITIC ALLOYS AND ALUMINIUM ALLOYS[J]. 金属学报, 2010, 46(11): 1335-1346.
[13] Jian ZHANG. EFFECTS OF GRAIN-BOUNDARY PHASES ON HYDROGEN EMBRITTLEMENT OF FE-NI-CR AUSTENITIC ALLOY BY INTERNAL FRICTION[J]. 金属学报, 2008, 44(9): 1095-1098 .
[14] ;. Microstructures and Hydrogen Permeation Characteristics of Nb-Ti-Ni Alloys[J]. 金属学报, 2008, 44(7): 781-785 .
[15] tian ye; WANG Mao-Qiu; Jinxu Li. HYDROGEN EMBRITTLEMENT SUSCEPTIBILITY OF 40CrNi3MoV STEELS WITH THE STRENGTH LEVEL OF 1500MPa[J]. 金属学报, 2008, 44(4): 403-408 .
No Suggested Reading articles found!