OBSERVATION OF CoSi PHASE TRANSFORMATION IN Co FILM
ZHANG Zaoli; XIAO Zhigang; DU Guowei (University of Science and Technology Beijing; Beijing 100083)(Manuscript received 1994-05-18; in revised form 1994-10-18)
Cite this article: 

ZHANG Zaoli; XIAO Zhigang; DU Guowei (University of Science and Technology Beijing; Beijing 100083)(Manuscript received 1994-05-18; in revised form 1994-10-18). OBSERVATION OF CoSi PHASE TRANSFORMATION IN Co FILM. Acta Metall Sin, 1995, 31(16): 179-182.

Download:  PDF(294KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  TEM observation was carried out on the phase transformation of CoSi along Co/ Si interface of the film grown on the Si substrate annealed at 250, 450 or 500℃respectively. CoSi is found to be the polycrystalline grains and no epitaxial relationship occurred between Si substrate and CoSi. The sequence of phase transformation for Co/Si interface in the annealing temperature range may be:250-450℃ 450-500℃Co2Si+ CoSi─→ CoSi─→CoSi+CoSi2(Correspondent: ZHANG Zaoli, Department of Material Physics, University of Science and TechnologyBeijing Beijing 100083)
Key words:  thin film. CoSi. TEM     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1995/V31/I16/179

1MurarkSP.SilicidesforVLSIApplicalions.NewYork.Academnic,1983:1082Bulle-LieuwmaCWT,VanOmmenAH.HornstraJ.AussemsCNAM.JApplPhys.1992:5:713VeuillenJY,DerrienJ,BodozPA,RosencherE,D'AnterrochersC.ApplPhysLett,1982;8:514D'AnterrochersC.SurSci,1985;168:515MadarR,D'AnterrochersC,Arnaudd'AvitayaF.BoursierD.ThomasO.SenateurJP.JApplPhys,1988;64:30146GibsonJM.BatstoneJL,TungRT.ApplPhysLett,1987;45:507VanGurpGJ,VanderWegWF,SigurdD.JApplPhys,1978,49:40118AppellaumA,KnoellRV.MurarkaSP.JApplPhys,1985:57:18809PirriC,PeruchettiJC,GewinnerG,DerrienJ.PhysRev,1984,B29:339110RoyerI.BullSocFrMineralCristallogr,1928;51:711PretoiusR,HarricJ,NicoletMA.SolidStateEletron,1978:21:667
No related articles found!
No Suggested Reading articles found!