| PREPARATION OF WHISKER REINFORCED Al-8.5Fe--1.3V-1.7Si COMPOSITES AND APPRAISAL OF REINFORCING BEHAVIOUR FOR VARIOUS WHISKERS |
| MA Zongyi;NING Xiaoguang (Laboratory of Atomic Imaging of Solide; Institute of Metal Research;Chinese Academy of Scicnces.Shenyang); PAN fin (Changsha Institute of Technology);LI Jihong;LU Yuxiong;BI Jing(Laboratory of Alomic Imaging of Solids; Institute of Metal Research; Chinese Academy of Sciences; Shenyang) |
|
Cite this article:
MA Zongyi;NING Xiaoguang (Laboratory of Atomic Imaging of Solide; Institute of Metal Research;Chinese Academy of Scicnces.Shenyang); PAN fin (Changsha Institute of Technology);LI Jihong;LU Yuxiong;BI Jing(Laboratory of Alomic Imaging of Solids; Institute of Metal Research; Chinese Academy of Sciences; Shenyang). PREPARATION OF WHISKER REINFORCED Al-8.5Fe--1.3V-1.7Si COMPOSITES AND APPRAISAL OF REINFORCING BEHAVIOUR FOR VARIOUS WHISKERS. Acta Metall Sin, 1994, 30(21): 420-426.
|
|
|
Abstract Various whiskers, SiC, Si_3N_4 and Al_(18)B_4O_(33),reinforced Al-8.SFe1 .3V-1 .7Si alloy composites have been prepared by the P / M technique at elevated temperature. The interfacial reaction at the Al_(18)B_4O_(33) interfaces and interfacial reaction product at the SiC or Si_3N_4 interfaces were avoided by employing the alloy matrix without Mg. The strength and modulus of the composites may be obviously improved by incorporating the whiskers in effective sequence:SiC, Si_3N_4 and Al_(18)B_4O_(33). The strength of thess compositeswill linearly drop with increasing temperature, yet their service temperature seems to be 50-100 ℃ higher than that of SiCw / 2024Al composite.
|
|
|
| 1SuganumaK,FujitaT,NiiharaK,SuzukiN.JMaterSciLett,1989;8:8082SuganumaK,FujitaT,SuzukiN,NiiharaK,JMaterSciLett,1990;7:6333潘进,宁小光,胡魁毅,叶恒强,金属学报,1993;29:B2804NingXG,PanJ,HuKY,YeHQ.MaterLett,1992;13:3775NingXG,PanJ,HuKY,YeHQ.PhilosMagA,1992;66:8116RaghunathanN,McshaneHB,DaviesC,SheppardT.JMaterSci,1990;25:49067RadmilovicV,ThomasG,DasSK.MaterSciEng,1991;A132:1718MaZY,NingXG,LuYX,LiJH,BiJ,ZhangYZ.MaterLett.accepted9周多三,王云,陈振华,蒋向阳,魏诗远,李洪湘.中南矿冶学院学报,1991;22(增刊1):89 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|