Acta Metall Sin  1994, Vol. 30 Issue (21): 427-431    DOI:
Current Issue | Archive | Adv Search |
INTERFACIAL REACTION IN K_2O·8TiO_(2(w))/ ZL109 COMPOSITE UNDER THERMAL EXPOSURE OR THERMAL CYCLING
SHEN Baoluo;LI Wei;ZHONG Yumao(Chengdu University of Science and Technology);NING Xiaoguang;LI Jihong;YE Hengqiang(Laboratory of Atomic Imaging of Solids;Institute of Metal Research; Chinese Academy of Sciences;Shenyang)
Cite this article: 

SHEN Baoluo;LI Wei;ZHONG Yumao(Chengdu University of Science and Technology);NING Xiaoguang;LI Jihong;YE Hengqiang(Laboratory of Atomic Imaging of Solids;Institute of Metal Research; Chinese Academy of Sciences;Shenyang). INTERFACIAL REACTION IN K_2O·8TiO_(2(w))/ ZL109 COMPOSITE UNDER THERMAL EXPOSURE OR THERMAL CYCLING. Acta Metall Sin, 1994, 30(21): 427-431.

Download:  PDF(347KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  A new phase, Ti_7Al_5Si_12.was found along interfaces between K_2O ·8TiO_2 whisker and ZL109 matrix of the composite under thermal exposure over 500 ℃for 100 h,and it might increase with prolonging the exposure time or thermal cycles.The tharmalexposure is more remarkable to accelerate the interfacial reaction than cycling.A transitionallayer between whiskers and matrix is observed under all conditions.
Key words:  potassium titanate whisker      Al alloy ZL109      composite      interface reaction     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1994/V30/I21/427

1福永秀春,武市通文,太田进.日本复合材料学会志,1982;8:662西田义则,今井恒道,山田守,松原弘美,白柳格,轻金属,1988;38:5153菅沼克昭,藤田辉昭,新原皓一,铃本信幸.铁钢,1989;75:15344土取功,新田明,原信彦,原田秀文.铁钢.1989;75:15265土取功,福永秀春.日本金属学会志,1992;56:3336菅沼克昭.轻金属,1992;42:52
[1] ZHANG Deyin, HAO Xu, JIA Baorui, WU Haoyang, QIN Mingli, QU Xuanhui. Effects of Y2O3 Content on Properties of Fe-Y2O3 Nanocomposite Powders Synthesized by a Combustion-Based Route[J]. 金属学报, 2023, 59(6): 757-766.
[2] MA Zongyi, XIAO Bolv, ZHANG Junfan, ZHU Shize, WANG Dong. Overview of Research and Development for Aluminum Matrix Composites Driven by Aerospace Equipment Demand[J]. 金属学报, 2023, 59(4): 457-466.
[3] MA Guonan, ZHU Shize, WANG Dong, XIAO Bolv, MA Zongyi. Aging Behaviors and Mechanical Properties of SiC/Al-Zn-Mg-Cu Composites[J]. 金属学报, 2023, 59(12): 1655-1664.
[4] JIANG Jiang, HAO Shijie, JIANG Daqiang, GUO Fangmin, REN Yang, CUI Lishan. Quasi-Linear Superelasticity Deformation in an In Situ NiTi-Nb Composite[J]. 金属学报, 2023, 59(11): 1419-1427.
[5] SHEN Yingying, ZHANG Guoxing, JIA Qing, WANG Yumin, CUI Yuyou, YANG Rui. Interfacial Reaction and Thermal Stability of the SiCf/TiAl Composites[J]. 金属学报, 2022, 58(9): 1150-1158.
[6] GU Ruicheng, ZHANG Jian, ZHANG Mingyang, LIU Yanyan, WANG Shaogang, JIAO Da, LIU Zengqian, ZHANG Zhefeng. Fabrication of Mg-Based Composites Reinforced by SiC Whisker Scaffolds with Three-Dimensional Interpenetrating-Phase Architecture and Their Mechanical Properties[J]. 金属学报, 2022, 58(7): 857-867.
[7] ZHENG Shijian, YAN Zhe, KONG Xiangfei, ZHANG Ruifeng. Interface Modifications on Strength and Plasticity of Nanolayered Metallic Composites[J]. 金属学报, 2022, 58(6): 709-725.
[8] PAN Chengcheng, ZHANG Xiang, YANG Fan, XIA Dahai, HE Chunnian, HU Wenbin. Corrosion and Cavitation Erosion Behavior of GLNN/Cu Composite in Simulated Seawater[J]. 金属学报, 2022, 58(5): 599-609.
[9] WANG Haowei, ZHAO Dechao, WANG Mingliang. A Review of the Corrosion Protection Technology on In SituTiB2/Al Composites[J]. 金属学报, 2022, 58(4): 428-443.
[10] ZHANG Lei, SHI Tao, HUANG Huogen, ZHANG Pei, ZHANG Pengguo, WU Min, FA Tao. Phase Separation and Solidification Sequence of Uranium-Based Amorphous Composites[J]. 金属学报, 2022, 58(2): 225-230.
[11] CHEN Run, WANG Shuai, AN Qi, ZHANG Rui, LIU Wenqi, HUANG Lujun, GENG Lin. Effect of Hot Extrusion and Heat Treatment on the Microstructure and Tensile Properties of Network Structured TiBw/TC18 Composites[J]. 金属学报, 2022, 58(11): 1478-1488.
[12] FAN Genlian, GUO Zhiqi, TAN Zhanqiu, LI Zhiqiang. Architecture Design Strategies and Strengthening-Toughening Mechanisms of Metal Matrix Composites[J]. 金属学报, 2022, 58(11): 1416-1426.
[13] NIE Jinfeng, WU Yuli, XIE Kewei, LIU Xiangfa. Microstructure and Thermal Stability of Heterostructured Al-AlN Nanocomposite[J]. 金属学报, 2022, 58(11): 1497-1508.
[14] WANG Shuo, WANG Junsheng. Structural Evolution and Stability of the δ′/θ′/δ′ Composite Precipitate in Al-Li Alloys: A First-Principles Study[J]. 金属学报, 2022, 58(10): 1325-1333.
[15] LI Wenya, ZHANG Zhengmao, XU Yaxin, SONG Zhiguo, YIN Shuo. Research Progress of Cold Sprayed Ni and Ni-Based Composite Coatings: A Review[J]. 金属学报, 2022, 58(1): 1-16.
No Suggested Reading articles found!