Please wait a minute...
Acta Metall Sin  1994, Vol. 30 Issue (20): 337-341    DOI:
Current Issue | Archive | Adv Search |
COMPUTER SIMULATION OF SPRAY DEPOSITION PROCESS──Ⅰ.Thoretical Model
SHEN Jun;JIANG Zuling;ZENG Songyan;CUI Chengsong; LI Qingchun(Harbin Institute of Technology)
Cite this article: 

SHEN Jun;JIANG Zuling;ZENG Songyan;CUI Chengsong; LI Qingchun(Harbin Institute of Technology). COMPUTER SIMULATION OF SPRAY DEPOSITION PROCESS──Ⅰ.Thoretical Model. Acta Metall Sin, 1994, 30(20): 337-341.

Download:  PDF(322KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The dynamics for the fluid flow and the heat transfer in a spray deposition/ rapid solidification process was thoretically analysed. The stress was placed onto modelling such parameters as powder size distribution, gas exit velocity, gas mass flow rate and metal mass flow rate, and series equations governing the heat transfer in the atomization and deposition processes.
Key words:  rapid solidification      powder metallurgy      spray deposition      thoretical model Al-Cu alloy     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1994/V30/I20/337

1LaverniaEJ,GrantNJ.ProgPowderMetall,1986;42:4572GrantPS,KimWT,CantorB.MaterSciEng,1991;Al34:11113FieiderHC,SawyerTF,KoppRW,LeathamAG.JMet,1987;8:284沈军,崔成松,蒋祖龄,曾松岩,李庆春.金属学报,1994;30:B3425GeigerGH著,俞景禄译.冶金中的传热传质现象.北京:冶金工业出版社,1981:1246林兆福.气体动力学.北京:北京航空航天大学出版社,1988:317LubansksH.JMet,1970;22:458沈军.哈尔滨工业大学博士学位论文,1993:989UpadhyayaRK,SpacilHS.SurfCoatTechnol,1989;37:37910SzekelyJ著,彭一川,徐匡迪,樊寿颐译,冶金中的流体流动现象.北京:冶金工业出版社,1985:2811Gutierrez—MiraveteE,LaverniaEJ,TrapagaGM,SzekelyJ,GrantNJ.MetallTrans,1989;20A:7112MathurP,AplianD,LawleyA,PowderMetall,1991;34:109z
[1] BAI Jiaming, LIU Jiantao, JIA Jian, ZHANG Yiwen. Creep Properties and Solute Atomic Segregation of High-W and High-Ta Type Powder Metallurgy Superalloy[J]. 金属学报, 2023, 59(9): 1230-1242.
[2] XU Lei, TIAN Xiaosheng, WU Jie, LU Zhengguan, YANG Rui. Microstructure and Mechanical Properties of Inconel 718 Powder Alloy Prepared by Hot Isostatic Pressing[J]. 金属学报, 2023, 59(5): 693-702.
[3] ZHU Yunpeng, QIN Jiayu, WANG Jinhui, MA Hongbin, JIN Peipeng, LI Peijie. Microstructure and Properties of AZ61 Ultra-Fine Grained Magnesium Alloy Prepared by Mechanical Milling and Powder Metallurgy Processing[J]. 金属学报, 2023, 59(2): 257-266.
[4] MA Guonan, ZHU Shize, WANG Dong, XIAO Bolv, MA Zongyi. Aging Behaviors and Mechanical Properties of SiC/Al-Zn-Mg-Cu Composites[J]. 金属学报, 2023, 59(12): 1655-1664.
[5] LIANG Chen, WANG Xiaojuan, WANG Haipeng. Formation Mechanism of B2 Phase and Micro-Mechanical Property of Rapidly Solidified Ti-Al-Nb Alloy[J]. 金属学报, 2022, 58(9): 1169-1178.
[6] YANG Qinzheng, YANG Xiaoguang, HUANG Weiqing, SHI Duoqi. Propagation Behaviors of Small Cracks in Powder Metallurgy Nickel-Based Superalloy FGH4096[J]. 金属学报, 2022, 58(5): 683-694.
[7] BI Sheng, LI Zechen, SUN Haixia, SONG Baoyong, LIU Zhenyu, XIAO Bolv, MA Zongyi. Microstructure and Mechanical Properties of Carbon Nanotubes-Reinforced 7055Al Composites Fabricated by High-Energy Ball Milling and Powder Metallurgy Processing[J]. 金属学报, 2021, 57(1): 71-81.
[8] HAO Zhibo, GE Changchun, LI Xinggang, TIAN Tian, JIA Chonglin. Effect of Heat Treatment on Microstructure and Mechanical Properties of Nickel-Based Powder Metallurgy Superalloy Processed by Selective Laser Melting[J]. 金属学报, 2020, 56(8): 1133-1143.
[9] ZHANG Guoqing,ZHANG Yiwen,ZHENG Liang,PENG Zichao. Research Progress in Powder Metallurgy Superalloys and Manufacturing Technologies for Aero-Engine Application[J]. 金属学报, 2019, 55(9): 1133-1144.
[10] Zhengguan LU,Jie WU,Lei XU,Xiaoxiao CUI,Rui YANG. Ring Rolling Forming and Properties of Ti2AlNb Special Shaped Ring Prepared by Powder Metallurgy[J]. 金属学报, 2019, 55(6): 729-740.
[11] QIN Jiayu, LI Xiaoqiang, JIN Peipeng, WANG Jinhui, ZHU Yunpeng. Microstructure and Mechanical Properties of Carbon Nanotubes (CNTs) Reinforced AZ91 Matrix Composite[J]. 金属学报, 2019, 55(12): 1537-1543.
[12] FENG Yefei,ZHOU Xiaoming,ZOU Jinwen,WANG Chaoyuan,TIAN Gaofeng,SONG Xiaojun,ZENG Weihu. Interface Reaction Mechanism Between SiO2 and Matrix and Its Effect on the Deformation Behavior of Inclusionsin Powder Metallurgy Superalloy[J]. 金属学报, 2019, 55(11): 1437-1447.
[13] MA Guonan, WANG Dong, LIU Zhenyu, BI Sheng, ZAN Yuning, XIAO Bolv, MA Zongyi. Effect of Hot Pressing Temperature on Microstructure and Tensile Properties of SiC/Al-Zn-Mg-Cu Composites[J]. 金属学报, 2019, 55(10): 1319-1328.
[14] Guohua WU, Yushi CHEN, Wenjiang DING. Current Research and Future Prospect on Microstructures Controlling of High Performance Magnesium Alloys During Solidification[J]. 金属学报, 2018, 54(5): 637-646.
[15] Bin ZHAI, Kai ZHOU, Peng Lü, Haipeng WANG. Rapid Solidification of Ti-6Al-4V Alloy Micro-Droplets Under Free Fall Condition[J]. 金属学报, 2018, 54(5): 824-830.
No Suggested Reading articles found!