| PREPARATION AND PROPERTIES OF FePd ALLOY ULTRAFINE PARTICLES |
| CHEN Jian;SUN Xiukui;XU Jian;YANG Mingchuan;WEI Wenduo;HU Zhuangqi Stale Key Laboratory of Rapidly Solidified and Non-Equiliberium Alloys; Institute of Metal Research; Academia Sinica; Shenyang |
|
Cite this article:
CHEN Jian;SUN Xiukui;XU Jian;YANG Mingchuan;WEI Wenduo;HU Zhuangqi Stale Key Laboratory of Rapidly Solidified and Non-Equiliberium Alloys; Institute of Metal Research; Academia Sinica; Shenyang. PREPARATION AND PROPERTIES OF FePd ALLOY ULTRAFINE PARTICLES. Acta Metall Sin, 1993, 29(9): 18-24.
|
|
|
Abstract The preparation of FePd alloy ultrafine particles (UFP) by inert gas condensa-tion technique was studied. The properties of the products were measured. The results showthat the composition of the master alloy and the activity coefficient of the components havestrong effect on the products. The single phase uniform alloy UFP can only be obtained byevaporating the alloy with the composition of N_Fe = 0.5. The stability of Fe_(50) pd (50) alloy UFPis higher than that of Fe UFP. The coercivity of Fe_(50)pd_(50), is several times higher than that ofcoarse grain powder with the same composition and can reach the value more than 4.30×10_4 A/m.
|
|
Received: 18 September 1993
|
1 Tasaki A, Tomiyana S, Ida S. Jpn J Appl Phys, 1965; 4: 707 2 Corner W D, Mundell R A. J Magn Magn Mater, 1980; 20: 148 3 Tasaki A, Takao M, Tokunaga H. Jpn J Appl Phys. 1974; 13: 271 4 Papaefthymiou V, Kostikas A, Simopoulos A, Niarchos D, Gangopadhyay S, Hadjipanayis G C, Klabunde K J, Sorensen C M. J Appl Phys, 1990; 67: 4487 5 Du Youwei, Wu Jian, Lu Huaixian, Wang Tingxiang. J Appl Phys, 1987; 61: 3314 6 吴坚,陆怀先,都有为,高学奎,王挺祥.物理学报,1988;37:2045 7 Gangopadhyay S, Hadjipanayis G C, Dale B, Sorensen C M, Klabunde K J, Papaefthymiou V, Kostikas A. Phys Rev, 1992; B45: 9778 8 Kimoto K, Kamiya Y, Nonoyama M, Uyeda R. Jpn J Appl Phys. 1963; 2: 702 9 徐坚,孙秀魁,陈文绣,范学书,魏文铎.材料科学进展,1992;6:209 10 Hultgren R, Zapffe C A. Trans Am Inst Min Metalling, 1939; 133: 58 11 Hultgren R. Selected Value of the Thermodynamic Properties of Binary Alloys. Metal Park, Ohio: ASM, 1973 12 Haneda K, Morrish A H. Nature, 1979; 282: 186 13 Kajiwara S, Ohno S, Honma K, Uda M. Philos Mag Lett, 1987; 55: 215 14 Granqvist C G, Buhrman R A. J Appl Phys, 1976; 47: 2200 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|