Please wait a minute...
Acta Metall Sin  1993, Vol. 29 Issue (3): 88-89    DOI:
Current Issue | Archive | Adv Search |
NEW TECHNIQUE-ELECTROMAGNETIC CENTRIFUGAL CASTING PROCESS
GE Yunlong;YANG Yuansheng;JIAO Yuning;HU Zhuangqi;GAO Yunyan;JIA Guanglin Institute of Metal Research; Academia Sinica; Shenyang Northeast University of Technology; Shenyang associate professor;Institute of Metal Research;Academia Sinica;Shenyang 110015
Cite this article: 

GE Yunlong;YANG Yuansheng;JIAO Yuning;HU Zhuangqi;GAO Yunyan;JIA Guanglin Institute of Metal Research; Academia Sinica; Shenyang Northeast University of Technology; Shenyang associate professor;Institute of Metal Research;Academia Sinica;Shenyang 110015. NEW TECHNIQUE-ELECTROMAGNETIC CENTRIFUGAL CASTING PROCESS. Acta Metall Sin, 1993, 29(3): 88-89.

Download:  PDF(424KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  A new technique of centrifugal casting was firstly provided withelectromagnetic field. Taking a heat resisting alloy steel 25Cr20Ni and an Al-Cu alloy as ex-amples,products, though their length,diameter and wall thickness are varied, revealed so supe-rior macrostructures that the mechanical properties are much improved in comparison withconventional centrifugal casting.
Key words:  electromagnetic field      centrifugal casting      heat resisting steel      Al-Cu alloy     
Received:  18 March 1993     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1993/V29/I3/88

[1] TANG Haiyan, LIU Jinwen, WANG Kaimin, XIAO Hong, LI Aiwu, ZHANG Jiaquan. Progress and Perspective of Functioned Continuous Casting Tundish Through Heating and Temperature Control[J]. 金属学报, 2021, 57(10): 1229-1245.
[2] REN Zhongming,LEI Zuosheng,LI Chuanjun,XUAN Weidong,ZHONG Yunbo,LI Xi. New Study and Development on Electromagnetic Field Technology in Metallurgical Processes[J]. 金属学报, 2020, 56(4): 583-600.
[3] Ran TAO, Yutao ZHAO, Gang CHEN, Xizhou KAI. Microstructure and Properties of In-Situ ZrB2 np/AA6111 Composites Synthesized Under an Electromagnetic Field[J]. 金属学报, 2019, 55(1): 160-170.
[4] Yongyong GONG, Shumin CHENG, Yuyi ZHONG, Yunhu ZHANG, Qijie ZHAI. The Solidification Technology of Pulsed Magneto Oscillation[J]. 金属学报, 2018, 54(5): 757-765.
[5] Qiang WANG, Ming HE, Xiaowei ZHU, Xianliang LI, Chunlei WU, Shulin DONG, Tie LIU. Study and Development on Numerical Simulation for Application of Electromagnetic Field Technologyin Metallurgical Processes[J]. 金属学报, 2018, 54(2): 228-246.
[6] Fei WANG,Engang WANG,Peng JIA,Tao WANG,Anyuan DENG. Effect of Electromagnetic Continuous Casting on TiN Distribution and Internal Crack of Incoloy800H Alloy Billet[J]. 金属学报, 2017, 53(1): 97-106.
[7] Fuxin WANG, Liangshun LUO, Liang WANG, Donghui ZHANG, Xinzhong LI, Yanqing SU, Jingjie GUO, Hengzhi FU. EFFECT OF ALLOY COMPOSITION AND COOLING RATE ON THE GROWTH MORPHOLOGY OF PRIMARY Al2Cu PHASE IN Al-Cu ALLOY DURING SOLIDIFICATION[J]. 金属学报, 2016, 52(3): 361-368.
[8] Cheng BI, Zhipeng GUO, E LIOTTI, Shoumei XIONG, P S GRANT. QUANTIFICATION STUDY ON DENDRITE FRAGMENTATION IN SOLIDIFICATION PROCESS OF ALLUMINUM ALLOYS[J]. 金属学报, 2015, 51(6): 677-684.
[9] GAO Zhongtang, HU Rui, WANG Jun, YANG Jieren, LI Jinshan. EFFECT OF ELECTROMAGNETIC MELT TREATMENT NEAR LIQUIDUS ON THE FORMATION OF NON-DENDRITE MICROSTRUCTURE OF SUPERALLOY[J]. 金属学报, 2014, 50(12): 1471-1477.
[10] XU Hongyu, HUANG Lujun, GENG Lin, ZHANG Jie, HUANG Yudong. EFFECTS OF Cu CONTENT ON THE WEAR PROPERTIES OF Al2O3•SiO2sf/Al-Cu COMPOSITES[J]. 金属学报, 2013, 49(9): 1131-1136.
[11] JIA Peng, WANG Engang, LU Hui, HE Jicheng. EFFECT OF ELECTROMAGNETIC FIELD ON MICRO-STRUCTURE AND MECHANICAL PROPERTY FOR INCONEL 625 SUPERALLOY[J]. 金属学报, 2013, 49(12): 1573-1580.
[12] . EFFECT OF FORCED FLOW ON THREE DIMENSIONAL DENDRITIC GROWTH OF Al-Cu ALLOYS[J]. 金属学报, 2012, 48(5): 615-620.
[13] WANG Fang LI Baokuan. ANALYSIS OF ELECTROMAGNETIC FIELD AND JOULE HEATING OF ELECTROSLAG REMELTING PROCESSES[J]. 金属学报, 2010, 46(7): 794-799.
[14] DU Huiling WANG Jianzhong QI Jingang HE Lijia CANG Daqiang . EFFECTS OF PULSED ELECTROMAGNETIC FIELD ON CoC2O4·2H2O POWDER SIZE[J]. 金属学报, 2009, 45(8): 1019-1024.
[15] XU Xiujie DENG Anyuan WANG Engang ZHANG Lintao ZHANG Xingwu ZHANG Yongjie HE Jicheng . EVOLVEMENT MECHANISM OF SURFACE OSCILLA- TION MARKS ON ROUND BILLET DURING SOFT–CONTACT ELECTROMAGNETIC CONTINUOUS CASTING[J]. 金属学报, 2009, 45(4): 464-469.
No Suggested Reading articles found!