Please wait a minute...
Acta Metall Sin  1993, Vol. 29 Issue (3): 84-87    DOI:
Current Issue | Archive | Adv Search |
NEUTRON DIFFRACTION STUDY ON R_2Fe_(17)N_χ(R=Y, Dy, Nd)
YANG Jilian;ZHANG Baisheng;DING Yongfan;YANG Yingchang;ZHANG Xiaodong;PAN Shuming China Institute of Atomic Energy; Beijing Department of Physics; Peking University; Beijing General Research Institute for Non-Ferrous Metals; Beijing associate professor; P.O. Box 275; Branch No.30; Beijing 102413
Cite this article: 

YANG Jilian;ZHANG Baisheng;DING Yongfan;YANG Yingchang;ZHANG Xiaodong;PAN Shuming China Institute of Atomic Energy; Beijing Department of Physics; Peking University; Beijing General Research Institute for Non-Ferrous Metals; Beijing associate professor; P.O. Box 275; Branch No.30; Beijing 102413. NEUTRON DIFFRACTION STUDY ON R_2Fe_(17)N_χ(R=Y, Dy, Nd). Acta Metall Sin, 1993, 29(3): 84-87.

Download:  PDF(277KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Samples of R_2Fe_(17)N_x(R=Y, Dy, Nd) were measured by neutron diffraction,and their magnetic structures and N site were determined. The effect of the site occupation ofN on magnetic properties was discussed primarily.
Key words:  neutron diffraction      Curie temperature      permanent magnet      (Y      Dy      Nd)_2Fe_(17)N_x     
Received:  18 March 1993     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1993/V29/I3/84

1 Coey J MD, Sun Hong. J Magn Magn Mater, 1990; 57: L251
2 Rietveld H M. J Appl Crystallogr, 1969; 2: 65
3 Otani Y, Hurley D P F, Sun Hong, Coey J M D. J Appl Phys, 1991; 69: 5584
4 Zhong X-P, Radwahski R J, De Boer F R, Jacobe T H, Buschow K H J. J Magn Magn Mater, 1990; 86: 333
5 Allred A L, Rochow E G. J Inorg Nucl Chem, 1958; 5: 264
6 Gschneidner K A. In: Michelsen O B ed., Analysis and Application of Rare Earth Materials, Universitets Forlaget, 1973:
[1] CHANG Songtao, ZHANG Fang, SHA Yuhui, ZUO Liang. Recrystallization Texture Competition Mediated by Segregation Element in Body-Centered Cubic Metals[J]. 金属学报, 2023, 59(8): 1065-1074.
[2] MU Yahang, ZHANG Xue, CHEN Ziming, SUN Xiaofeng, LIANG Jingjing, LI Jinguo, ZHOU Yizhou. Modeling of Crack Susceptibility of Ni-Based Superalloy for Additive Manufacturing via Thermodynamic Calculation and Machine Learning[J]. 金属学报, 2023, 59(8): 1075-1086.
[3] LI Shilei, LI Yang, WANG Youkang, WANG Shengjie, HE Lunhua, SUN Guang'ai, XIAO Tiqiao, WANG Yandong. Multiscale Residual Stress Evaluation of Engineering Materials/Components Based on Neutron and Synchrotron Radiation Technology[J]. 金属学报, 2023, 59(8): 1001-1014.
[4] LI Fulin, FU Rui, BAI Yunrui, MENG Lingchao, TAN Haibing, ZHONG Yan, TIAN Wei, DU Jinhui, TIAN Zhiling. Effects of Initial Grain Size and Strengthening Phase on Thermal Deformation and Recrystallization Behavior of GH4096 Superalloy[J]. 金属学报, 2023, 59(7): 855-870.
[5] WANG Hanyu, LI Cai, ZHAO Can, ZENG Tao, WANG Zumin, HUANG Yuan. Direct Alloying of Immiscible Tungsten and Copper Based on Nano Active Structure and Its Thermodynamic Mechanism[J]. 金属学报, 2023, 59(5): 679-692.
[6] ZHANG Zhidong. Exact Solution of Ferromagnetic Three-Dimensional (3D) Ising Model and Spontaneous Emerge of Time[J]. 金属学报, 2023, 59(4): 489-501.
[7] HAN Weizhong, LU Yan, ZHANG Yuheng. Mechanism of Ductile-to-Brittle Transition in Body-Centered-Cubic Metals:A Brief Review[J]. 金属学报, 2023, 59(3): 335-348.
[8] ZHU Yunpeng, QIN Jiayu, WANG Jinhui, MA Hongbin, JIN Peipeng, LI Peijie. Microstructure and Properties of AZ61 Ultra-Fine Grained Magnesium Alloy Prepared by Mechanical Milling and Powder Metallurgy Processing[J]. 金属学报, 2023, 59(2): 257-266.
[9] ZHANG Yuexin, WANG Jujin, YANG Wen, ZHANG Lifeng. Effect of Cooling Rate on the Evolution of Nonmetallic Inclusions in a Pipeline Steel[J]. 金属学报, 2023, 59(12): 1603-1612.
[10] LOU Feng, LIU Ke, LIU Jinxue, DONG Hanwu, LI Shubo, DU Wenbo. Microstructures and Formability of the As-Rolled Mg- xZn-0.5Er Alloy Sheets at Room Temperature[J]. 金属学报, 2023, 59(11): 1439-1447.
[11] GAO Jianbao, LI Zhicheng, LIU Jia, ZHANG Jinliang, SONG Bo, ZHANG Lijun. Current Situation and Prospect of Computationally Assisted Design in High-Performance Additive Manufactured Aluminum Alloys: A Review[J]. 金属学报, 2023, 59(1): 87-105.
[12] XIA Dahai, DENG Chengman, CHEN Ziguang, LI Tianshu, HU Wenbin. Modeling Localized Corrosion Propagation of Metallic Materials by Peridynamics: Progresses and Challenges[J]. 金属学报, 2022, 58(9): 1093-1107.
[13] WU Caihong, FENG Di, ZANG Qianhao, FAN Shichun, ZHANG Hao, LEE Yunsoo. Microstructure Evolution and Recrystallization Behavior During Hot Deformation of Spray Formed AlSiCuMg Alloy[J]. 金属学报, 2022, 58(7): 932-942.
[14] GAO Yubi, DING Yutian, LI Haifeng, DONG Hongbiao, ZHANG Ruiyao, LI Jun, LUO Quanshun. Effect of Deformation Rate on the Elastic-Plastic Deformation Behavior of GH3625 Alloy[J]. 金属学报, 2022, 58(5): 695-708.
[15] HUANGFU Hao, WANG Zilong, LIU Yongli, MENG Fanshun, SONG Jiupeng, QI Yang. A First Principles Investigation of W1 - x Ir x Alloys: Structural, Electronic, Mechanical, and Thermal Properties[J]. 金属学报, 2022, 58(2): 231-240.
No Suggested Reading articles found!