| BEHAVIOUR OF TRACE Mg IN HIGH SPEED STEEL M2 |
| MAO Weimin Beijing Polytechnic University University of Science and Technology Beijing |
|
Cite this article:
MAO Weimin Beijing Polytechnic University University of Science and Technology Beijing. BEHAVIOUR OF TRACE Mg IN HIGH SPEED STEEL M2. Acta Metall Sin, 1993, 29(11): 14-17.
|
|
|
Abstract An investigation was made of the eutectic microstructure during solidificationand the prespheroidization of eutectic carbide at elevated temperature of high speed steel M2inoculated with Mg. The traditional lamellar eutectic carbide M_2C in steel M2 may change in-to the fishbone eutectic carbide M_6C and block eutectic carbide MC if proper amount, saying0.012%, of Mg was added. The fishbone eutectic carbide prespheroidization may be retardedby Mg.
|
|
Received: 18 November 1993
|
1 Sandberg H. Scandi J of Metall, 1973; 2: 233 2 Gierek A, Marciak A, Wusatowski R. Zesz Nauk Politech Slask. 1982; 23: 5 3 #12 4 #12 5 Ghomashchi M R,Sellars C M. Met Sci, 1984; 18: 44 6 Holye G, Ineson E. Jpn Iron Steel Inst, 1959; 193: 254 7 #12 8 Lenta E J,Pesci H,Twentyman M E. Metallography, 1983; 16: 387 9 Fredriksson H, Hillert M, Nica M. Scand J Metall, 1979; 8: 115 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|