EFFECT OF Na AND K IMPURITIES AND Ce MODIFICATION ON CRACK PROPAGATION RESISTANCE FOR ALLOY 8090
MENG Liang;ZHANG Baochang;LIANG Ying;ZHANG Weizhong;TIAN Puke Northwestern Polytechnical University; Xi'an
Cite this article: 

MENG Liang;ZHANG Baochang;LIANG Ying;ZHANG Weizhong;TIAN Puke Northwestern Polytechnical University; Xi'an. EFFECT OF Na AND K IMPURITIES AND Ce MODIFICATION ON CRACK PROPAGATION RESISTANCE FOR ALLOY 8090. Acta Metall Sin, 1992, 28(3): 27-31.

Download:  PDF(1622KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The crack propagation resistance for alloy 8090 sheet decreases with the increaseof content of Na and K impurities. An improvement over the fracture toughness and crack initi-ation resistance for the alloy containing Na and K within certain limit may be made by adding0.05% Ce. This beneficial modification would not be manifested if the alloy contained moreenough Na and K. One of the reasons why Na and K injure the toughness of the alloy might bedue to that they cause the precipitation of T_1 phase along grain and subgrain boundaries andaccelerate the abnormal growth of recrystallized grains.
Key words:  alloy 8090      crack propagation resistance      Ce      fracture toughness      alkali metal     
Received:  18 March 1992     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1992/V28/I3/27

1 Webster D. Met Prog, 1984; 125(5) : 33
2 Webster D. Metall Trans, 1987; 18A: 2181
3 Webster D. In: Sanders T H Jr., Starke E A, Jr., eds., Aluminum-Lithium Alloys, Proc 5th Int Aluminum-Lithium Conf, Williamsburg, Virginia, 27--31 March, 1989, Birmingham (UK): Materials and Component Engineering Publications Ltd., 1989: 519
4 Zhang B C, Wang Z Z, Zhu W B, Li Y H, Liang Y. In: Sanders T H Jr., Starke E A Jr., eds., Aluminum-Lithium Alloys, Proc 5th Int Aluminum-Lithium Conf, Williamsburg, Virginia, 27--31 March, 1989, Birmingham (UK): Materials and Component Engineering Publications Ltd., 1989: 529
5 张匀,赵洪恩,姚大平,高国忠,陈继志,胡壮麒.航空新材料工程论文集,Vol.Ⅰ,北京,1990:129T
[1] LI Jiarong, DONG Jianmin, HAN Mei, LIU Shizhong. Effects of Sand Blasting on Surface Integrity and High Cycle Fatigue Properties of DD6 Single Crystal Superalloy[J]. 金属学报, 2023, 59(9): 1201-1208.
[2] WANG Lei, LIU Mengya, LIU Yang, SONG Xiu, MENG Fanqiang. Research Progress on Surface Impact Strengthening Mechanisms and Application of Nickel-Based Superalloys[J]. 金属学报, 2023, 59(9): 1173-1189.
[3] ZHENG Liang, ZHANG Qiang, LI Zhou, ZHANG Guoqing. Effects of Oxygen Increasing/Decreasing Processes on Surface Characteristics of Superalloy Powders and Properties of Their Bulk Alloy Counterparts: Powders Storage and Degassing[J]. 金属学报, 2023, 59(9): 1265-1278.
[4] MU Yahang, ZHANG Xue, CHEN Ziming, SUN Xiaofeng, LIANG Jingjing, LI Jinguo, ZHOU Yizhou. Modeling of Crack Susceptibility of Ni-Based Superalloy for Additive Manufacturing via Thermodynamic Calculation and Machine Learning[J]. 金属学报, 2023, 59(8): 1075-1086.
[5] CHANG Songtao, ZHANG Fang, SHA Yuhui, ZUO Liang. Recrystallization Texture Competition Mediated by Segregation Element in Body-Centered Cubic Metals[J]. 金属学报, 2023, 59(8): 1065-1074.
[6] LIU Wei, CHEN Wanqi, MA Menghan, LI Kailun. Review of Irradiation Damage Behavior of Tungsten Exposed to Plasma in Nuclear Fusion[J]. 金属学报, 2023, 59(8): 986-1000.
[7] SI Yongli, XUE Jintao, WANG Xingfu, LIANG Juhua, SHI Zimu, HAN Fusheng. Effect of Cr Addition on the Corrosion Behavior of Twinning-Induced Plasticity Steel[J]. 金属学报, 2023, 59(7): 905-914.
[8] WANG Furong, ZHANG Yongmei, BAI Guoning, GUO Qingwei, ZHAO Yuhong. First Principles Calculation of Al-Doped Mg/Mg2Sn Alloy Interface[J]. 金属学报, 2023, 59(6): 812-820.
[9] ZHANG Bin, TIAN Da, SONG Zhuman, ZHANG Guangping. Research Progress in Dwell Fatigue Service Reliability of Titanium Alloys for Pressure Shell of Deep-Sea Submersible[J]. 金属学报, 2023, 59(6): 713-726.
[10] WANG Hanyu, LI Cai, ZHAO Can, ZENG Tao, WANG Zumin, HUANG Yuan. Direct Alloying of Immiscible Tungsten and Copper Based on Nano Active Structure and Its Thermodynamic Mechanism[J]. 金属学报, 2023, 59(5): 679-692.
[11] HAN En-Hou, WANG Jianqiu. Effect of Surface State on Corrosion and Stress Corrosion for Nuclear Materials[J]. 金属学报, 2023, 59(4): 513-522.
[12] WANG Jingyang, SUN Luchao, LUO Yixiu, TIAN Zhilin, REN Xiaomin, ZHANG Jie. Rare Earth Silicate Environmental Barrier Coating Material: High-Entropy Design and Resistance to CMAS Corrosion[J]. 金属学报, 2023, 59(4): 523-536.
[13] WAN Tao, CHENG Zhao, LU Lei. Effect of Component Proportion on Mechanical Behaviors of Laminated Nanotwinned Cu[J]. 金属学报, 2023, 59(4): 567-576.
[14] XU Linjie, LIU Hui, REN Ling, YANG Ke. Effect of Cu on In-Stent Restenosis and Corrosion Resistance of Ni-Ti Alloy[J]. 金属学报, 2023, 59(4): 577-584.
[15] MA Zongyi, XIAO Bolv, ZHANG Junfan, ZHU Shize, WANG Dong. Overview of Research and Development for Aluminum Matrix Composites Driven by Aerospace Equipment Demand[J]. 金属学报, 2023, 59(4): 457-466.
No Suggested Reading articles found!