DIFFUSIVITY OF AI IN AMORPHOUS ALLOY Fe_(78)Si_9B_(13)
JIANG Honggang;DING Bingzhe;WANG Jingtang Institute of Metal Research; Academia Sinica; Shenyang
Cite this article: 

JIANG Honggang;DING Bingzhe;WANG Jingtang Institute of Metal Research; Academia Sinica; Shenyang. DIFFUSIVITY OF AI IN AMORPHOUS ALLOY Fe_(78)Si_9B_(13). Acta Metall Sin, 1992, 28(1): 77-80.

Download:  PDF(355KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  

Ion beam Sputtering Profiling in combination with SIMS technique was em-ployed to investigate the Al diffusion in Fe_(78)Si_9B_(13) amorphous alloy. Between 320℃ and 380℃,the diffusion coefficients vary from 2.43×10~(-22) to 2.01×10~(-21) m~2s~(-1), and an Arrhenius rela-tionship was established as: D_o = 2.02×10~(-12) exp (--1.17 / kT)

Key words:  amorphous alloy      atomic diffusion      SIMS     
Received:  18 January 1992     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1992/V28/I1/77

1 Johnson W L. Mater Sci Eng, 1988; 97: 1--13
2 Schultz, L. Mater Sci Eng, 1988; 97: 15
3 Luborsky F E. J Appl Phys, 1983; 54: 5732
4 Sharma S K, Banerjee S, Kuldeep, Jain A K. J Mater Res, 1989; 4: 603
5 Kijek M, Ahmadzadeh M, Cantor B, Cahn R W. Scr Metall, 1980; 14: 1337
6 De Schepper L, Knuyt G, Stals L M. J Phys Chem Solids, 1983: 44: 171--174
7 Hirvonen J, Raisanen J. J Appl Phys, 1982; 53: 3314
8 Mibe U, Methfessel S. In: Steeb S, Warlimont H eds., Rapidly Quenched Metals, Vol. 5, Proc 5th Int conf on Rapidly Quenched Metals, Germany, September 3-7, 1984, North-Holland, 1985: 775
9 Limoge Y. Acta Metall Mater, 1990; 38: 1733

[1] LIU Shuaishuai, HOU Chaonan, WANG Engang, JIA Peng. Plastic Rheological Behaviors of Zr61Cu25Al12Ti2 and Zr52.5Cu17.9Ni14.6Al10Ti5 Amorphous Alloys in the Supercooled Liquid Region[J]. 金属学报, 2022, 58(6): 807-815.
[2] LI Jinfu, LI Wei. Structure and Glass-Forming Ability of Al-Based Amorphous Alloys[J]. 金属学报, 2022, 58(4): 457-472.
[3] ZHANG Jinyong, ZHAO Congcong, WU Yijin, CHEN Changjiu, CHEN Zheng, SHEN Baolong. Structural Characteristic and Crystallization Behavior of the (Fe0.33Co0.33Ni0.33)84 -x Cr8Mn8B x High-Entropy-Amorphous Alloy Ribbons[J]. 金属学报, 2022, 58(2): 215-224.
[4] HAN Luhui, KE Haibo, ZHANG Pei, SANG Ge, HUANG Huogen. Kinetic Crystallization Behavior of Amorphous U60Fe27.5Al12.5 Alloy[J]. 金属学报, 2022, 58(10): 1316-1324.
[5] HU Xiang, GE Jiacheng, LIU Sinan, FU Shu, WU Zhenduo, FENG Tao, LIU Dong, WANG Xunli, LAN Si. Combustion Mechanism of Fe-Nb-B-Y Amorphous Alloys with an Anomalous Exothermic Phenomenon[J]. 金属学报, 2021, 57(4): 542-552.
[6] LIU Riping, MA Mingzhen, ZHANG Xinyu. New Development of Research on Casting of Bulk Amorphous Alloys[J]. 金属学报, 2021, 57(4): 515-528.
[7] ZHU Min, OUYANG Liuzhang. Kinetics Tuning and Electrochemical Performance of Mg-Based Hydrogen Storage Alloys[J]. 金属学报, 2021, 57(11): 1416-1428.
[8] HUANG Huogen, ZHANG Pengguo, ZHANG Pei, WANG Qinguo. Comparison of Glass Forming Ability Between U-Co and U-Fe Base Systems[J]. 金属学报, 2020, 56(6): 849-854.
[9] GENG Yaoxiang, WANG Yingmin. Local Structure-Property Correlation of Fe-Based Amorphous Alloys: Based on Minor Alloying Research[J]. 金属学报, 2020, 56(11): 1558-1568.
[10] XU Xiuyue, LI Yanhui, ZHANG Wei. Fabrication of Nanoporous PtRuFe by Dealloying Amorphous Fe(Pt, Ru)B Ribbons and Their Methanol Electrocatalytic Properties[J]. 金属学报, 2020, 56(10): 1393-1400.
[11] JIN Chenri, YANG Suyuan, DENG Xueyuan, WANG Yangwei, CHENG Xingwang. Effect of Nano-Crystallization on Dynamic Compressive Property of Zr-Based Amorphous Alloy[J]. 金属学报, 2019, 55(12): 1561-1568.
[12] Hongyang XU,Haibo KE,Huogen HUANG,Pei ZHANG,Pengguo ZHANG,Tianwei LIU. Nanoindentation Creep Behavior of U65Fe30Al5 Amorphous Alloy[J]. 金属学报, 2017, 53(7): 817-823.
[13] Dianguo MA,Yingmin WANG,Kunio YUBUTA,Yanhui LI,Wei ZHANG. Effect of Co Content on the Structure and Magnetic Properties of Melt-Spun Fe55-xCoxPt15B30 Alloys[J]. 金属学报, 2017, 53(5): 609-614.
[14] Huogen HUANG,Hongyang XU,Pengguo ZHANG,Yingmin WANG,Haibo KE,Pei ZHANG,Tianwei LIU. U-Cr Binary Alloys with Anomalous Glass-Forming Ability[J]. 金属学报, 2017, 53(2): 233-238.
[15] Yaoxiang GENG,Kaiming HAN,Yingmin WANG,Jianbing QIANG,Qing WANG,Chuang DONG,Guifeng ZHANG,O TEGUS,Peter HAÜSSLER. COMPOSITION DESIGN OF Fe-B-Si-Ta BULK AMORPHOUS ALLOYS BASED ON CLUSTER+ GLUE ATOM MODEL[J]. 金属学报, 2015, 51(8): 1017-1024.
No Suggested Reading articles found!