EFFECT OF Mo ON B DIFFUSION IN Ni MEASURED BY PARTICLE TRACKING AUTORADIOGRAPHY
CHU Youyi;JI Ping;KE Jun T. Ko University of Science and Technology Beijing
Cite this article: 

CHU Youyi;JI Ping;KE Jun T. Ko University of Science and Technology Beijing. EFFECT OF Mo ON B DIFFUSION IN Ni MEASURED BY PARTICLE TRACKING AUTORADIOGRAPHY. Acta Metall Sin, 1991, 27(5): 83-89.

Download:  PDF(707KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  A new technique for the measurement of B diffusivity in B bearing alloys by particle tracking autoradiography after deboronization has been established with high sensitivity, good reprocibility and fair simplicity. Experimental results show that the Mo addition up to 3% into Ni may accelerate the B diffusion in the range of 900—1250℃ and reduce both the activation energy and the frequency factor, of B diffusion but no more influential as the Mo added down to 0.5%.
Key words:  diffusion      autoradiography      B      Mo      Ni     
Received:  18 May 1991     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1991/V27/I5/83

1 Desalos Y, Maitrepierre Ph Rofes Vernis. Mem Sci Rev Metall, 1976; 73: 735
2 褚幼义,贺信莱,余宗森,欧宇光.金属学报,1980;16:380
3 Chu Youyi, He Xinlai, Ko T, Zhou Zhenxin. In; Gray J M, Ko T, Zhang Shouhua, Wu Baorong, Xie Xishan eds., HSLA Steel; Metallurgy and Applications, ASM International 1986: 351
4 Karlsson L. Ph D Thesis, Chalmers University of Technology, Goteborg, Sweden. 1986
5 褚幼义,章三红,贺信莱,柯俊.金属学报,1989;25:A275
6 Busby P E, Warga M E, Wells C. J Met, 1953; 5: 1463
7 Busby P E, Wells C. J Met, 1954; 6: 972
8 Armijo J S, Rosenbanm H S. Appl Phys, 1967; 38: 2064
9 He X L, Chu Y Y. J Phys D: Appl Phys, 1983; 16: 1145
10 Wells C, Batz W, Mehl R F, J Met, 1950; 188: 55
[1] WANG Lei, LIU Mengya, LIU Yang, SONG Xiu, MENG Fanqiang. Research Progress on Surface Impact Strengthening Mechanisms and Application of Nickel-Based Superalloys[J]. 金属学报, 2023, 59(9): 1173-1189.
[2] BAI Jiaming, LIU Jiantao, JIA Jian, ZHANG Yiwen. Creep Properties and Solute Atomic Segregation of High-W and High-Ta Type Powder Metallurgy Superalloy[J]. 金属学报, 2023, 59(9): 1230-1242.
[3] FENG Qiang, LU Song, LI Wendao, ZHANG Xiaorui, LI Longfei, ZOU Min, ZHUANG Xiaoli. Recent Progress in Alloy Design and Creep Mechanism of γ'-Strengthened Co-Based Superalloys[J]. 金属学报, 2023, 59(9): 1125-1143.
[4] BI Zhongnan, QIN Hailong, LIU Pei, SHI Songyi, XIE Jinli, ZHANG Ji. Research Progress Regarding Quantitative Characterization and Control Technology of Residual Stress in Superalloy Forgings[J]. 金属学报, 2023, 59(9): 1144-1158.
[5] ZHENG Liang, ZHANG Qiang, LI Zhou, ZHANG Guoqing. Effects of Oxygen Increasing/Decreasing Processes on Surface Characteristics of Superalloy Powders and Properties of Their Bulk Alloy Counterparts: Powders Storage and Degassing[J]. 金属学报, 2023, 59(9): 1265-1278.
[6] CHEN Jia, GUO Min, YANG Min, LIU Lin, ZHANG Jun. Effects of W Concentration on Creep Microstructure and Property of Novel Co-Based Superalloys[J]. 金属学报, 2023, 59(9): 1209-1220.
[7] JIANG He, NAI Qiliang, XU Chao, ZHAO Xiao, YAO Zhihao, DONG Jianxin. Sensitive Temperature and Reason of Rapid Fatigue Crack Propagation in Nickel-Based Superalloy[J]. 金属学报, 2023, 59(9): 1190-1200.
[8] GONG Shengkai, LIU Yuan, GENG Lilun, RU Yi, ZHAO Wenyue, PEI Yanling, LI Shusuo. Advances in the Regulation and Interfacial Behavior of Coatings/Superalloys[J]. 金属学报, 2023, 59(9): 1097-1108.
[9] ZHANG Leilei, CHEN Jingyang, TANG Xin, XIAO Chengbo, ZHANG Mingjun, YANG Qing. Evolution of Microstructures and Mechanical Properties of K439B Superalloy During Long-Term Aging at 800oC[J]. 金属学报, 2023, 59(9): 1253-1264.
[10] LU Nannan, GUO Yimo, YANG Shulin, LIANG Jingjing, ZHOU Yizhou, SUN Xiaofeng, LI Jinguo. Formation Mechanisms of Hot Cracks in Laser Additive Repairing Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1243-1252.
[11] ZHAO Peng, XIE Guang, DUAN Huichao, ZHANG Jian, DU Kui. Recrystallization During Thermo-Mechanical Fatigue of Two High-Generation Ni-Based Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1221-1229.
[12] LI Jiarong, DONG Jianmin, HAN Mei, LIU Shizhong. Effects of Sand Blasting on Surface Integrity and High Cycle Fatigue Properties of DD6 Single Crystal Superalloy[J]. 金属学报, 2023, 59(9): 1201-1208.
[13] ZHANG Jian, WANG Li, XIE Guang, WANG Dong, SHEN Jian, LU Yuzhang, HUANG Yaqi, LI Yawei. Recent Progress in Research and Development of Nickel-Based Single Crystal Superalloys[J]. 金属学报, 2023, 59(9): 1109-1124.
[14] LIU Xingjun, WEI Zhenbang, LU Yong, HAN Jiajia, SHI Rongpei, WANG Cuiping. Progress on the Diffusion Kinetics of Novel Co-based and Nb-Si-based Superalloys[J]. 金属学报, 2023, 59(8): 969-985.
[15] XU Yongsheng, ZHANG Weigang, XU Lingchao, DAN Wenjiao. Simulation of Deformation Coordination and Hardening Behavior in Ferrite-Ferrite Grain Boundary[J]. 金属学报, 2023, 59(8): 1042-1050.
No Suggested Reading articles found!